Antifriction and constructional organoplastics for elements of designs of airplanes of development Sukhoi design bureau

Kulagina G.S., Nasonov F.A., Zhelezina G.F., Demina A.S., Solovjova N.A., Morozov B.B., Shuldeshova P.M., Filatov A.A.
Kulagina G.S., Nasonov F.A., Zhelezina G.F., Demina A.S., Solovjova N.A., Morozov B.B., Shuldeshova P.M., Filatov A.A. Antifriction and constructional organoplastics for elements of designs of airplanes of development Sukhoi design bureau // Proceedings of VIAM. 2025. No. 3. DOI: 10.18577/2307-6046-2025-0-3-47-59. URL: https://www.viam-works.ru/en/journal/2025/3/5
Keywords
friction, wear resistance, prepreg, mechanization of airplanes
Abstract

Tests of details of airplanes of Sukhoi Design Bureau are executed. Details are made of prepregs of antifriction material and constructive organoplastiсs. Efficiency of antifriction material and constructional organoplastiсs for raising resistance to antifriction loss and for increasing resource of moving elements of an airplane mechanization, as well as fixed parts, which are in contact, are shown. The possibility of production of mechanization elements of an airplane by means of the co-forming prepregs of antifriction and constructive organoplastiсs has been proved.

Reference list
  1. Kablov E.N., Podzhivotov N.Yu., Lutsenko A.N. On the need to create a single information and analytical center for aviation materials in the Russian Federation. Problemy mashinostroyeniya i avtomatizatsii, 2019, no. 3, pp. 28–34.
  2. Kablov E.N., Shevchenko Yu.N., Grinevich A.V. Problems of certification of aviation materials at the present stage. 75 years. Aviation materials. Selected works of VIAM 1932–2007. Ed. E.N. Kablov. Moscow: VIAM, 2007, pp. 388–396.
  3. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  4. Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), paper no. 10. Available at: http://www.journal.viam.ru (accessed: January 26, 2024). DOI: 10.18577/2713-0193-2023-0-2-122-144.
  5. Antipov V.V., Serebrennikova N.Yu., Konovalov A.N., Nefedova Yu.N. Perspectives of application of fiber metal laminate materials based on aluminum alloys in aircraft design. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 45–53. DOI: 10.18577/2071-9140-2020-0-1-45-53.
  6. Gunyaeva A.G., Kurnosov A.O., Gulyaev I.N. High-temperature polymer composite materials developed FSUE «VIAM» for aerospace engineering: past, present and future (review). Trudy VIAM, 2021, no. 1 (95), paper no. 05. Available at: http://www.viam-works.ru (accessed: February 05, 2024). DOI: 10.18577/2307-6046-2021-0-1-43-53.
  7. Sagomonova V.A., Tselikin V.V. Vibration damping material with perforated constraining layer. Aviation materials and technologies, 2023, no. 3 (72), paper no. 10. Available at: http://www.journal.viam.ru (accessed: February 05, 2024). DOI: 10.18577/2713-0193-2023-0-3-125-133.
  8. Sidorina A.I. Woven metal-carbon reinforcing fillers for PCM. Aviation materials and technologies, 2023, no. 3 (72), paper no. 08. Available at: http://www.journal.viam.ru (accessed: March 01, 2024). DOI: 10.18577/2713-0193-2023-0-3-101-113.
  9. Marakhovskiy P.S., Barinov D.Ya., Maltseva E.Yu. The effect of reinforcing additives on the structure and thermophysical properties of ice composite materials. Aviation materials and technologies, 2023, no. 4 (73), paper no. 11. Available at: http://www.journal.viam.ru (accessed: March 01, 2024). DOI: 10.18577/2713-0193-2023-0-4-111-121.
  10. Gurtovik I.G., Sokolov V.I., Trofimov N.N., Shalgunov S.I. Radio-transparent products made of fiberglass. Moscow: Mir, 2002, 368 p.
  11. Bitkin V.E., Zhidkova O.G., Komarov V.V. Selection of materials for the manufacture of dimensionally stable load-bearing structures. Vestnik Samarskogo universiteta. Aerokosmicheskaya tekhnika, tekhnologii i mashinostroyeniye, 2018, vol. 17, no. 1, pp. 100–117. DOI: 10.18287/22541-7533-2018-17-1-100-117.
  12. Zhelezina G.F., Voynov S.I., Solovieva N.A., Kulagina G.S. Aramid organotextolites for impact-resistant aircraft structures. Zhurnal prikladnoy khimii, 2019, vol. 92, is. 3, pp. 358–364.
  13. Kulagina G.S., Zhelezina G.F., Levakova N.M. Antifriction organoplastics for high-loaded friction knots. Trudy VIAM, 2019, no. 2 (74), paper no. 09. Available at: http://www.viam-works.ru (accessed: February 14, 2024). DOI: 10.18577/2307-6046-2019-0-2-89-96.
  14. Nasonov F.A., Kulagina G.S., Demina A.S., Zhelezina G.F., Morozov B.B., Solovyova N.A., Shuldeshova P.M. Application of composites with special self-lubricating antifriction coatings in the aviation industry. XLIII All-Russian. conf. «Science and Technology»: in 2 vols. Moscow: RAS, 2023, vol. 1, pp. 21–27.
  15. Mikhailov Yu.S. Increasing the efficiency of swept wing mechanization. Scientific Bulletin of MSTU GA, 2020, vol. 23, no. 6, pp. 101–18. DOI: 10.26467/2079-0619-2020-23-6-101-120.
  16. Su-57 – Russian fifth-generation fighter. Available at: https://dzen.ru/a/YW4C16Kc_DqzBOeC (accessed: February 01, 2024).
  17. Kulagina G.S., Nasonov F.A., Zhelezina G.F., Demina A.S., Solovieva N.A., Morozov B.B., Shuldeshova P.M., Filatov A.A. Technology of flexible structural elements of aircraft developed by Sukhoi Design Bureau using prepregs of antifriction and structural organoplastics. XLIV All-Rus. Conf. «Science and Technology», dedicated to the 300th anniversary of the Russian Academy of Sciences and the 100th anniversary of Academician V.P. Makeev: in 2 vols. Moscow: RAS, 2024, vol. 1, pp. 91–99.
  18. The Best Sukhoi Aircraft: Documentary Series. Issue: Su-57 (broadcast on 04.12.2023). Zvezda TV Channel: official website. Available at: https://tvzvezda.ru/video/films-online/20241301629-lnBa9.html/20231241017-6J1p9.html (accessed: February 01, 2024).
  19. Akulin P.V. Accumulation of Damage in Composite Panels under Low-Cycle Loading. Vestnik MAI, 2023, vol. 30, no. 2, pp. 4–90. DOI: 10.34759/vst-2023-2-84-90.
  20. Soborejo A.B.O. Use of entropy principles in estimating reliability functions for creep rupture characteristics of engineering materials all high temperatures. Proc. Internat. Conf. «Strength of Metals and Alloys». Tokyo, 1967, pp. 252–256.
  21. Dudchenko A.A., Lurie S.A., Halim K. Multiscale modeling on damage mechanics of laminated composite materials. Proc. of conference «Damage in composite materials: Simulation and non-destructive testing». Stuttgart, 2006, pp. 23–26.
  22. Movchan A.A. Micromechanical approach to the problem of describing the accumulation of anisotropic scattered damage. Mekhanika tverdogo tela, 1990, no. 3, pp. 252–256.
  23. Movchan A.A. Problem of strength of thin-walled structures. Moscow: MAI Publ. House, 1989, pp. 20–24.
  24. Kablov E.N., Startsev V.O. Effect of internal stresses on the aging of polymer composite materials. Review. Mekhanika kompozitnykh materialov, 2021, vol. 57, no. 5, pp. 805–822.
  25. Kablov E.N., Laptev A.B., Prokopenko A.N., Gulyaev A.I. Relaxation of polymeric composite materials under the prolonged action of static load and climate (review). Part 1. Binders. Aviation materials and technologies, 2021, no. 4 (65), paper no. 08. Available at: http://www.journal.viam.ru (accessed: July 29, 2024). DOI: 10.18577/2713-0193-2021-0-4-70-80.
  26. Vasiliev V.V. Mechanics of structures made of composite materials. Moscow: Mashinostroyenie, 1988, 272 p.
  27. Skudra A.M., Bulavs F.Ya. Creep of reinforced plastics. Moscow: Khimiya, 1982, 214 p.