Quench sensitivity of wrought heat-treatable aluminum alloys of the Al–Mg–Si system (review)

Benarieb I., Puchkov Yu.A., Sbitneva S.V., Shorstov S.Yu., Shumeyko R.M.
Benarieb I., Puchkov Yu.A., Sbitneva S.V., Shorstov S.Yu., Shumeyko R.M. Quench sensitivity of wrought heat-treatable aluminum alloys of the Al–Mg–Si system (review) // Proceedings of VIAM. 2025. No. 2. DOI: 10.18577/2307-6046-2025-0-2-25-46. URL: https://www.viam-works.ru/en/journal/2025/2/3
Keywords
alloys of the Al–Mg–Si system, quenching, aging, solid solution stability, phase transformations, temperature –time–transformation diagrams, dispersoids, differential scanning calorimetry, mathematical modelling
Abstract

The article presents a review of the scientific literature on quenching sensitivity of wrought heat-treatable aluminum alloys of the Al–Mg–Si system (6XXX series). The analysis of the current state and the latest achievements in this field of research is carried out. The factors influencing the quenching sensitivity are considered, and some aspects of the effect of the quenching rate on aging process and properties of these alloys are described. It is revealed that an important trend in the study of phase transformations of alloys of the 6XXX series during quenching process is the use of differential scanning calorimetry and mathematical modeling.

Reference list
  1. Kolobnev N.I., Ber L.B., Tsukrov S.L. Heat treatment of deformable aluminum alloys. Ed. E.N. Kablov. Moscow: APRAL, 2020, 552 p.
  2. Ostermann F. Technology of aluminum application. Moscow: NP «APRAL», 2019, 872 p.
  3. Nechaykina T.A., Oglodkov M.S., Ivanov A.L., Kozlova O.Yu., Yakovlev S.I., Shlyapni-
  4. kov M.A. Features of hardening of wide cladding sheets from V95p.ch. aluminum alloy on a continuous heat treatment line. Trudy VIAM, 2021, no. 11 (105), paper no. 03. Available at: http://www.viam-works.ru (accessed: April 25, 2024). DOI: 10.18577/2307-6046-2021-0-11-25-33.
  5. Nefedova Yu.N., Shlyapnikova T.A., Ivanov A.L., Sedelnikov V.V. Methods for reducing residual stresses during hardening of high-strength aluminum alloys. Trudy VIAM, 2023, no. 7 (125), paper no. 03. Available at: http://www.viam-works.ru (accessed: April 25, 2024). DOI: 10.18577/2307-6046-2023-0-7-23-33.
  6. Mai Xuan D., Gnevko A.I., Puchkov Yu.A. Study of cryogenic treatment influence on residual stresses and properties of D16 aluminium alloy. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 25–31. DOI: 10.18577/2071-9140-2020-0-2-25-31.
  7. Lumley R. Fundamentals of aluminium metallurgy: recent advances. Cambridge: Woodhead Publishing, 2018, 578 р.
  8. Zakharov E.D., Davydov V.G., Egorova L.S. et al. Study of the stability of solid solutions of alloys of the Al–Mg–Si system. Tekhnologiya legkikh splavov, 1967, no. 2. pp. 12–17.
  9. Davydov V.G., Zakharov V.V., Zakharov E.D., Novikov I.I. Diagrams of isothermal decomposition of a solution in aluminum alloys: reference book. Ed. I.I. Novikov. Moscow: Metallurgiya, 1973, 152 p.
  10. Zakharov V.V. Stability of a solid solution in aluminum alloys. Tsvetnye metally, 2007, no. 11, pp. 100–107.
  11. Dons A.L., Lohne O. Quench sensitivity of AlMgSi-alloys containing Mn or Cr. MRS Online Proceedings Library, 1983, vol. 21, pp. 723–728.
  12. Staley J.T. Quench factor analysis of aluminum alloys. Materials Science and Technology, 1987, vol. 3 (11), pp. 923–935.
  13. Bratland D.H., Grong O., Shercliff H. et al. Modelling of precipitation reactions in industrial processing. Acta Materialia, 1997, vol. 45, nо. 1, pp. 1–22.
  14. Tiryakioglu M. Quench sensitivity of aluminum alloys. Conference: Quenching and Distortion Control Technology, 1999, pp. 1–11. Available at: https://www.researchgate.net/publication/
  15. 259851071_Quench_Sensitivity_of_Aluminum_Alloys (accessed: April 25, 2024).
  16. Strobel K., Easton M., Sweet L. et al. Relating quench sensitivity to microstructure in 6000 series aluminium alloys. Materials Transactions, 2011, vol. 52, no. 5, pp. 914–919.
  17. Strobel K., Easton M., Lay M. et al. Quench sensitivity in a dispersoid-containing Al–Mg–Si alloy. Metallurgical and Materials Transactions A, 2019, vol. 50, pp. 1957–1969.
  18. Kassner M.E., Geantil P., Li X. A study of the quench sensitivity of 6061‐T6 and 6069‐T6 aluminum alloys. Journal of Metallurgy, 2011, vol. 2011, no. 1, p. 747198.
  19. Shang B.C., Yin Z.M., Wang G. et al. Investigation of quench sensitivity and transformation kinetics during isothermal treatment in 6082 aluminum alloy. Materials & Design, 2011, vol. 32, no. 7, pp. 3818–3822.
  20. Li H.Y., Zeng C., Han M. et al. Time–temperature–property curves for quench sensitivity of 6063 aluminum alloy. Transactions of Nonferrous Metals Society of China, 2013, vol. 23, no. 1, pp. 38–45.
  21. Li S., Huang Z., Chen W. et al. Quench sensitivity of 6351 aluminum alloy. Transactions of Nonferrous Metals Society of China, 2013, vol. 23, no. 1, pp. 46–52.
  22. Milkereit B., Starink M.J. Quench sensitivity of Al–Mg–Si alloys: a model for linear cooling and strengthening. Materials & Design, 2015, vol. 76, pp. 117–129.
  23. Milkereit B., Starink M., Rometsch P. et al. Review of the Quench Sensitivity of Aluminium Alloys: Analysis of the Kinetics and Nature of Quench-Induced Precipitation. Materials, 2019, vol. 12, p. 4083. DOI: 10.3390/ma12244083.
  24. Vander Voort G.F. Atlas of time-temperature diagrams for nonferrous alloys. Almere: ASM International, 1991, p. 474.
  25. Birol Y. The effect of processing and Mn content on the T5 and T6 properties of AA6082 profiles. Journal of Materials Processing Technology, 2006, vol. 173, no. 1, pp. 84–91.
  26. Steele D., Evans D., Nolan P., Lloyd D.J. Quantification of grain boundary precipitation and the influence of quench rate in 6XXX aluminum alloys. Materials Characterization, 2007, vol. 58, no. 1, pp. 40–45.
  27. Svenningsen G., Larsen M., Nordlien J., Nisancioglu K. Effect of thermomechanical history on intergranular corrosion of extruded AlMgSi (Cu) model alloy. Corrosion science, 2006, vol. 48, no. 12, pp. 3969–3987.
  28. Lang P., Falahati A., Ahmadiet M.R. et al. Modeling the influence of cooling rate on the precipitate evolution in Al–Mg–Si (Cu) alloys. Materials Science and Technology. Columbus, 2011, pp. 284–291.
  29. Milkereit B., Wanderka N., Schick C., Kessler O. Continuous cooling precipitation diagrams of Al–Mg–Si alloys. Materials Science and Engineering: A, 2012, vol. 550, pp. 87–96.
  30. Giersberg L., Milkereit B., Schick C., Kessler O. In Situ Isothermal Calorimetric Measurement of Precipitation Behaviour in Al–Mg–Si Alloys. Materials Science Forum, 2014, vol. 794, pp. 939–944.
  31. Milkereit B., Giersberg L., Kessler О., Schick C. Isothermal time-temperature precipitation diagram for an aluminum alloy 6005A by in situ DSC experiments. Materials, 2014, vol. 7, pp. 2631–2649.
  32. Castany P., Diologent F., Rossol A. et al. Influence of quench rate and microstructure on bendability of AA6016 aluminum alloys. Materials Science and Engineering: A, 2013, vol. 559, pp. 558–565.
  33. Saito T., Marioara C., Royset J. et al. The effects of quench rate and pre-deformation on precipitation hardening in Al–Mg–Si alloys with different Cu amounts. Materials Science and Engineering: A, 2014, vol. 609, pp. 72–79.
  34. Strobel K., Lay M., Easton M. et al. Effects of quench rate and natural ageing on the age hardening behaviour of aluminium alloy AA6060. Materials Characterization, 2016, vol. 111, pp. 43–52.
  35. Fröck H., Milkereit B., Wiechmann P. et al. Influence of solution-annealing parameters on the continuous cooling precipitation of aluminum alloy 6082. Metals, 2018, vol. 8, no. 4, pp. 265.
  36. Fan Z., Lei X., Wang L. et al. Influence of quenching rate and aging on bendability of AA6016 sheet. Materials Science and Engineering: A, 2018, vol. 730, pp. 317–327.
  37. Milkereit B., Kessler O., Schick C. Recent Advances in Thermal Analysis and Calorimetry of Aluminum Alloys. Handbook of Thermal Analysis and Calorimetry, 2018, vol. 6,
  38. pp. 735–779.
  39. Yang Z., Mallow S., Banhart J., Kessler O. Probing precipitation in aluminium alloys during linear cooling via in-situ differential scanning calorimetry and electrical resistivity measurement. Thermochimica Acta, 2024, vol. 739, p. 179815.
  40. Kahlenberg R., Schuster R., Garcia-Arango N. et al. Revisiting High-Energy X-Ray Diffraction and Differential Scanning Calorimetry Data of En Aw-6082 with Mean Field Simulations. Available at: http://www.papers.ssrn.com/sol3/papers.cfm?abstract_id=4862542 (accessed: April 25, 2024).
  41. Zhang X., Zhou X., Nilsson J.O. Corrosion behaviour of AA6082 Al–Mg–Si alloy extrusion: The influence of quench cooling rate. Corrosion Science, 2019, vol. 150, pp. 100–109.
  42. Frodal B.H., Christiansen E., Myhr O.R. et al. The role of quench rate on the plastic flow and fracture of three aluminium alloys with different grain structure and texture. International Journal of Engineering Science, 2020, vol. 150, p. 103257.
  43. Liu S., Wang X., Pan Q. et al. Investigation of microstructure evolution and quench sensitivity of Al–Mg–Si–Mn–Cr alloy during isothermal treatment. Journal of Alloys and Compounds, 2020, vol. 826, p. 154144.
  44. Yuan B., Li G., Guo M., Zhuang L. Fast age-hardening response of Al–Mg–Si–Cu–Zn–Fe–Mn alloy via coupling control of quenching rate and pre-aging. Journal of materials research and technology, 2021, vol. 14, pp. 1518–1531.
  45. Yang Z., Jiang X., Zhang X. et al. Natural ageing clustering under different quenching conditions in an Al–Mg–Si alloy. Scripta Materialia, 2021, vol. 190, pp. 179–182.
  46. Miesenberger B., Kozeschnik E., Milkereit B. et al. Computational analysis of heterogeneous nucleation and precipitation in AA6005 Al-alloy during continuous cooling DSC experiments. Materialia, 2022, vol. 25, p. 101538.
  47. Xia C., Deng S., Ni C. et al. Study on laminar structure and process on high strength brazed aluminum alloy for heat exchangers. Vacuum, 2023, vol. 215, p. 112303.
  48. Ma Y., Liu C., Miao K. et al. Effects of cooling rate and cryogenic temperature on the mechanical properties and deformation characteristics of an Al–Mg–Si–Fe–Cr alloy. Journal of Alloys and Compounds, 2023, vol. 947, p. 169559.
  49. Yang M., Ruan Z., Lin H. et al. Quantified effect of quench rate on the microstructures and mechanical properties of an Al–Mg–Si alloy. Journal of Materials Research and Technology, 2023, vol. 24, pp. 6753–6761.
  50. Eskin D.G., Massardier V., Merle P. A study of high-temperature precipitation in Al–Mg–Si alloys with an excess of silicon. Journal of materials science, 1999, vol. 34, pp. 811–820.
  51. Sbitneva S.V., Lukina E.А., Zaytsev D.V. Investigation of the features of the decomposition of a solid solution during aging of alloys of the Al–Mg–Si–Cu system. Trudy VIAM, 2021, no. 12 (106), paper no. 02. Available at: http://www.viam-works.ru (accessed: March 18, 2024). DOI: 10.18577/2307-6046-2021-0-12-14-20.
  52. Kablov E.N., Dynin N.V., Benarieb I. et al. Promising aluminum alloys for brazed structures of aircraft equipment. Zagotovitelnye proizvodstva v mashinostroyenii, 2021, no. 4, pр. 179–192.
  53. Kutsal U., Arslan Y., Ozaydin O. et al. Heat Treatment Simulation of Aluminum Alloy Wheels and Investigation of Process Steps. International Journal of Metalcasting, 2024, vol. 18, no. 2, pp. 1556–1572.