Development of carbon and glass prepreg processed by vacuum molding with low curing temperature for the manufacture of rehabilitation equipment for the disabled

Donetskiy K.I., Karavaev R.Y., Gracheva A.D., Saburov F.A., Tkachuk A.I., Sedov E.V., Shebbo M.F.M.
Donetskiy K.I., Karavaev R.Y., Gracheva A.D., Saburov F.A., Tkachuk A.I., Sedov E.V., Shebbo M.F.M. Development of carbon and glass prepreg processed by vacuum molding with low curing temperature for the manufacture of rehabilitation equipment for the disabled // Proceedings of VIAM. 2025. No. 12. DOI: 10.18577/2307-6046-2025-0-12-74-87. URL: https://www.viam-works.ru/en/journal/2025/12/7
Keywords
polymer composite materials, prepregs, vacuum forming, binder, technological package, tooling, vacuuming, impregnation, rehabilitation equipment for the disabled
Abstract

Polymer composite materials are increasingly being used in the manufacture of rehabilitation equipment for the disabled, particularly in the production of prostheses and orthoses, including the use of prepregs processed by vacuum molding. The demand for materials in this industry is growing steadily, with imported materials primarily used, and import substitution is becoming increasingly important. NRC «Kurchatov Institute» – VIAM has developed a series of materials that can be used in this industry.

Reference list
  1. Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), pp. 122–144. Available at: http://www.journal.viam.ru (accessed: January 31, 2025). DOI: 10.18577/2713-0193-2023-0-2-122-144.
  2. Onishchenko G.G., Kablov E.N., Ivanov V.V. Scientific and technological development of Russia in the context of achieving national goals: problems and solutions. Innovatsii, 2020, no. 6 (260), pp. 3–16.
  3. Raskutin A.E. Russian polymer composite materials of new generation, their exploitation and implementation in advanced developed constructions. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 349–367. DOI: 10.18577/2071-9140-2017-0-S-349-367.
  4. Kablov E.N., Antipov V.V. The role of new generation materials in ensuring the technological sovereignty of the Russian Federation. Vestnik Rossiyskoy akademii nauk, 2023, vol. 93, no. 10, pp. 907–916.
  5. Order of the Federal Service for Environmental, Technological and Nuclear Supervision of December 15, 2020 No. 536 «On approval of federal norms and rules in the field of industrial safety «Industrial safety rules for the use of equipment operating under excess pressure». Available at: http://www.infobm.ru/upload/Правила%20промышленной%20безопасности%20при%20исполь-зовании%20оборудования.pdf (accessed: October 10, 2025).
  6. Mikhaylin Yu.A. Fibrous polymer composite materials in engineering. St. Petersburg: Scientific Foundations and Technologies, 2013, 720 p.
  7. Babaevsky P.G., Vinogradov V.M., Golovkin G.S. et al. Structural Plastics (Therapeutic Plastics). Ed. E.B. Trostyanskaya. Moscow: Khimiya, 1974, 304 p.
  8. Berring N.S., Renieri M.P., Bond G.G., Palmer D.J. Autoclave vs. Non-Autoclave: A comparison of hat-stiffened subcomponents by static and fatigue testing and related non-destructive evaluations. 2012 SAMPE International Symposium and Exhibition-Emerging Opportunities: Materials and Process Solutions. Baltimore, MD, 2012, pp. 23–25.
  9. Donetskiy K.I., Karavaev R.Yu., Bystrikova D.V., Gracheva A.D., Tkachuk A.I. Semipregs and carbon fiber reinforced plastics based on them. Trudy VIAM, 2025, no. 8 (150), paper no. 08. Available at: http://www.viam-works.ru (accessed: October 21, 2025). DOI: 10.18577/2307-6046-2025-0-8-85-99.
  10. Donetskyi K.I., Timoshkov P.N., Safronov A.M., Goncharov V.A., Mishchun M.I. Autoclave-free molding of prepregs. Konstruktsii iz kompozitsionnykh materialov, 2022, no. 1 (165), pp. 29–34.
  11. Tkachyk A.I., Kyznecova P.A., Donetskiy K.I., Karavaev R.Yu. Some technological features of manufacturing polymer composite materials by non-autoclave molding of prepregs. Trudy VIAM, 2024, no. 12 (142), paper no. 04. Available at: http://www.viam-works.ru (accessed: October 20, 2025). DOI: 10.18577/2307-6046-2024-0-12-44-55.
  12. Yakobson Ya.S., Kuzhekin A.P., Samoilov D.V., Shishkin B.V. Energy-saving lower limb prostheses. Rossiyskiy zhurnal biomekhaniki, 1999, vol. 3, no. 2, p. 129.
  13. Osipenko M.A., Nyashin Yu.I., Rudakov R.N. Mathematical modeling and optimization of the design of an elastic element of a foot prosthesis. Rossiyskiy zhurnal biomekhaniki, 1999, vol. 3, no. 2, pp. 87–88.
  14. Borisov I.M., Reznik S.V. Development of a composite structure for biomechanical purposes. Vestnik Rossiyskogo universiteta druzhby narodov. Ser.: Inzhenernyye issledovaniya, 2021, vol. 22, no. 4, pp. 348–354. DOI: 10.22363/2312-8143-2021-22-4-348-354.
  15. Tkachuk A.I., Donetsky K.I., Terekhov I.V., Karavaev R.Yu. The use of thermosetting matrices for the manufacture of polymer composite materials by the non-autoclave molding methods. Aviation materials and technology, 2021, no. 1 (62), paper no. 03. Available at: https://www.journal.viam.ru (accessed: October 20, 2025). DOI: 10.18577/2713-0193-2021-0-1-22-33.
  16. Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composites (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 48–58. DOI: 10.18577/2071-9140-2019-0-3-48-58.
  17. Mikhailin Yu.A. Thermosetting Binders of Polymeric Composites. Polimernye materialy, 2009, no. 2, pp. 40–45.
  18. Panina N.N., Chursova L.V., Babin A.N., Grebeneva T.A., Gurevich Ya.M. Main Methods of Modifying Epoxy Polymer Materials in Russia. Vse materialy. Entsiklopedicheskiy spravochnik, 2014, no. 9, pp. 10–17.
  19. Chursova L.V., Panina N.N., Grebeneva T.A., Kutergina I.Yu. Epoxy Resins, Hardeners, Modifiers, and Binders Based on Them. St. Petersburg: Profession, 2020, 550 p.
  20. Mostovoy A.S. Formulation modification of epoxy resins using new highly effective plasticizers. Sovremennye naukoyemkie tekhnologii, 2015, no. 7, pp. 66–70.
  21. Chebotareva E.G., Ogrel L.Yu. Modern trends in the modification of epoxy polymers. Fundamentalnye issledovaniya, 2008, no. 4, pp. 102–104.
  22. Bobylev V.A. Special epoxy resins for adhesives and sealants. Klei. Germetiki. Tekhnologii, 2005, vol. 5, pp. 8–12.
  23. Zagora A.G. Use of dicyandiamide in epoxy adhesives, binders and polymer composite materials based on them (review). Klei. Germetiki. Tekhnologii, 2020, no. 4, pp. 35–37.
  24. Li H., Neville K. Reference Guide to Epoxy Resins. Moscow: Energia, 1973, 108 p.
  25. Galimzyanova R.Yu. Modern Composite Materials in the Production of Medical Equipment: A Textbook. Kazan: Kazan National Research Tech. Univ., 2021, 89 p.
  26. Romo H.D. Specialized prostheses for activities: an update. Clinical Orthopaedic Related Research, 1999, vol. 361, pp. 63–70.
  27. Timoshkov P.N., Usacheva M.N., Khrulkov A.V., Grigorieva L.N. Prospects for the use of polymer composite materials in the manufacture of prostheses (review). Plasticheskie massy, 2021, no. 5-6, pp. 40–43. DOI: 10.35164/0554-2901-2021-5-6-40-43.
  28. Scholz M.-S., Blanchfield J.P., Bloom L.D. et al. The use of composite materials in modern orthopedic medicine and prosthetic devices: A review. Composites Science and Technology, 2011, vol. 71, pp. 1791–1803.
  29. Nolan L. Carbon fibre prostheses and running in amputees: a review. The Journal of Foot and Ankle Surgery, 2008, vol. 14 (3), pp. 125–129.
  30. McCarvill S. Essay: prosthetics for athletes. The Lancet, 2005, vol. 366 (1), pp. 10–11.
  31. Berry D.A. Composite material for orthotics and prosthetics. Orthotics and Prosthetics, 1987, vol. 40 (4), pp. 3543.
  32. Tryggvason H., Starker F., Lecompte Ch., Jonsdottir F. Modeling and simulation in the design process of a prosthetic foot. Proceedings of the 58th SIMS. Reykjavik, 2017, pp. 398–404.