Features of obtaining a highly heat-resistant low shrinkage material based on chemically strengthened silicon carbide

Vikulin V.V., Gvozdev S.S.
Vikulin V.V., Gvozdev S.S. Features of obtaining a highly heat-resistant low shrinkage material based on chemically strengthened silicon carbide // Proceedings of VIAM. 2025. No. 12. DOI: 10.18577/2307-6046-2025-0-12-53-62. URL: https://www.viam-works.ru/en/journal/2025/12/5
Keywords
silicon carbide, sintering, silicon organic compound, nitriding, thermodynamic calculation, gas and vibration stands
Abstract

The article presents the features and regularities of the technology of obtaining highly heat-resistant low shrinkage silicon carbide by forming zones with different thermal conductivity in the porous structure of the material, increasing the strength and resistance to oxidation at temperatures up to 1600 °C, preventing the reduction of SiO2 by silicon carbide at high temperatures.

The dependences of density, linear shrinkage and amount of binder during of pre-sintered ceramic samples on the specific surface of silicon carbide powders are presented. The effect of pre-sintered ceramic density on the strength of samples at temperatures of 20, 1400 and 1500 °C is demonstrated. Data are presented on the effect of impregnation of silicon carbide with a silicon organic compound and high-temperature treatment of ceramic samples in a nitrogen environment and in air on increasing the strength characteristics and resistance of ceramics to oxidation.

Reference list
  1. Method for producing products based on silicon nitride: pat. 2239613. Rus. Federation; appl. 02.10.03; publ. 11.10.04.
  2. Vikulin V. Production of Si3N4-Based Articles and Their Application in Aerospace Industry. Advances in Science and Technology, 2006, vol. 45, pp. 1751–1758.
  3. Bhatnagar A. World of Materials. Lightweight Ballistic Materials. Moscow: Tekhnosfera, 2000, 392 p.
  4. Molded porous ceramic article containing SiC and proses for the production there of: pat. 7648932B2 US; appl. 07.05.06; publ. 19.01.10.
  5. Method for producing an abrasive compact: pat. 2176191 B1 EP; appl. 23.07.08; publ. 21.04.10.
  6. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 1018577/ 2071-9140-2015-0-1-3-33.
  7. Ceramic oxidation-resistant composite material and products made from it: pat. 2560046 C1 Rus. Federation; appl. 10.07.14; publ. 20.08.15.
  8. Ceramic composite material and products made from it: pat. 2700428 C1 Rus. Federation; appl. 17.09.17; publ. 18.07.18.
  9. Heat-resistant low-shrinkage material based on silicon carbide: a.s. 197832 USSR; appl. 19.08.81; publ. 17.09.82.
  10. Vikulin V., Leshuk T. Material based chemically strengthened silicon carbide. Refractories and Industrial Ceramics, 1992, vol. 32, no. 9–10, pp. 510–515.
  11. Vikulin V., Leshchuk T. Materials based on chemically strengthened silicon carbide. Ogneupory i tekhnicheskaya keramika, 1991, no. 10, pp. 8–12.
  12. Method for processing products from ceramic materials based on silicon carbide and/or carbon: pat. 2276661 Rus. Federation; appl. 28.07.04; publ. 20.05.06.
  13. Vikulin V., Romashin A., Leshuk Т. Si3N4–Si composite ceramics and chemically toughened SiC for engine components. Cеramics in Energy Applications. 2nd International conference proceedings. London, 1994, pp. 21–32.
  14. Vikulin V., Kostina L., Leshchuk T., Shtarev G. Low-shrinkage silicon carbide products. Designs and technologies for producing products from non-metallic materials. Moscow: VIMI, 1988, pp. 33–34.
  15. Suvorov S., Chaykun E., Gusarov V. Multilayer oxidation-resistant materials based on silicon carbide. Oborudovanie, materialy, protsessy. Moscow: VIMI, 1989, is. 3, pp. 29–30.
  16. Protective siliconoxinitride coating for porous refractories: pat. 4187344А US; appl. 27.09.78; publ. 05.02.80.
  17. Method for protecting the surface of silicon carbide during high-temperature etching: a. s. 270080 USSR; appl. 05.03.74; publ. 12.05.75.
  18. Materials based on low-shrinkage silicon carbide: a. s. 235082 USSR; appl. 27.02.84; publ. 24.03.85.
  19. Doorbar Ph.J., Kyle-Henney S. Development of Continuosly-Rreinforced Metal Matrix Composite for Aerospace Applications. Comprehensive Composite Materials II, 2018, vol. 4, pp. 439–463. DOI: 10.1016/В 978-0-12-803581-8.09983-5.