Study of cured hot melt adhesive epoxy binders by sclero- and microhardness methods

Salakhova R.K., Veshkin E.A, Apalkova A.V., Simirgina N.D.
Salakhova R.K., Veshkin E.A, Apalkova A.V., Simirgina N.D. Study of cured hot melt adhesive epoxy binders by sclero- and microhardness methods // Proceedings of VIAM. 2025. No. 12. DOI: 10.18577/2307-6046-2025-0-12-12-24. URL: https://www.viam-works.ru/en/journal/2025/12/2
Keywords
hot melt adhesives, floor panel sheetings, microhardness, sclerometry, scratch resistance force, degree of curing, degree of conversion, volumetric anisotropy coefficient
Abstract

The results of cross-sectional microhardness measurements grade binders (compositions I–VII) are presented. Volumetric anisotropy coefficients are calculated, and the correlation between polymer matrix microhardness and the indenter scratch resistance parameter is studied. A comparative analysis of microhardness changes in the height direction of the samples and sclerograms obtained using an ST-01 laboratory scratch tester is conducted. For the low-flammability hot melt adhesive binder (composition VII), the optimal two-stage curing mode is selected, and the degree of polymer conversion is determined.

Reference list
  1. Kablov E.N. New Generation Materials – the Basis for Innovation, Technological Leadership, and National Security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
  2. Kablov E.N. Science as a Branch of the Economy. Nauka i zhizn, 2009, no. 10, pp. 6–10.
  3. Kablov E.N. Composites: Today and Tomorrow. Metally Evrazii, 2015, no. 1, pp. 36–39.
  4. Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), paper no. 10. Available at: http://www.journal.viam.ru (accessed: September 23, 2025). DOI: 10.18577/2713-0193-2023-0-2-122-144.
  5. Mishkin S.I. Application of carbon fiber plastics in constructions of pilotless devices (review). Trudy VIAM, 2022, no. 5 (111), paper no. 08. Available at: http://www.viam-works.ru (accessed: September 30, 2025). DOI: 10.18577/2307-6046-2022-0-5-87-95.
  6. Raskutin A.E. Development strategy of polymer composite materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 344–348. DOI: 10.18577/2071-9140-2017-0-S-344-348.
  7. Isaev A.Yu., Rubtsova E.V., Kotova E.V., Sutyagin M.N. Research of properties of glues and glue binding, made with use of modern domestic component base. Trudy VIAM, 2021, no. 3 (97), paper no. 05. Available at: http://www.viam-works.ru (accessed: April 09, 2025). DOI: 10.18577/2307-6046-2021-0-3-58-67.
  8. Kutsevich K.E., Dementeva L.A., Lukina N.F., Tyumeneva T.Yu. Adhesive prepregs as promising materials for parts and assemblies from polymeric composite materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 379–387. DOI: 10.18577/2071-9140-2017-0-S-379-387.
  9. Chursova L.V., Tsybin A.I., Grebeneva T.A. Binders for polymer composite and functional materials. Previous experience, current status and development prospects. Novosti materialovedeniya. Nauka i tekhnika, 2017, no. 2 (26), pp. 34–46. Available at: http://www.materialsnews.ru (accessed: April 09, 2025).
  10. Sopotov R.I., Gorbunova I.Yu., Onuchin D.V. et al. Effect of polysulfone and polyethersulfone modifiers on the thermomechanical properties of epoxyamine binder. Uspekhi v khimii i khimicheskoy tekhnologii, 2015, vol. 29, no. 10, pp. 62–64.
  11. Kablov E.N., Chursova L.V., Babin A.N. et al. Developments of FSUE VIAM in the field of melt binders for polymer composite materials. Polimernye materialy i tekhnologii, 2016, vol. 2, no. 2, pp. 37–42.
  12. Kopitsyna M.N., Bessonov I.V., Kotomin S.V. Crack resistance of epoxy binders modified with thermoplastic polysulfone and furfural acetone resin. Inzhenernyy zhurnal: nauka i innovatsii, 2016, no. 12, pp. 1–9.
  13. Khasbulatova Z.S. Aromatic polysulfones. Plasticheskiye massy, 2009, no. 4, pp. 20–23.
  14. Kostromina N.V., Olikhova Yu.V., Malakhovsky S.S., Gorbunova I.Yu. Development of epoxy binders modified with heat-resistant thermoplastics for the creation of reinforced composite materials. Plasticheskiye massy, 2022, no. 9–10, pp. 17–19.
  15. Borodulin A.S. Plasticizers for epoxy adhesives and binders. Klei. Germetiki. Tekhnologii, 2012, no. 7, pp. 31–35.
  16. Malysheva G.V., Marakhovskiy P.S., Barinov D.Ya., Nikolaev E.V. Optimization of the curing modes of fiber-glass based on epoxy binder. Aviation materials and technologies, 2023, no. 2 (71), paper no. 08. Available at: http://www.journal.viam.ru (accessed: October 06, 2025). DOI: 10.18577/2713-0193-2023-0-2-94-103.
  17. Bolshakov V.A., Antyufeeva N.V. Evaluation of the curing process model of the adhesive binder in prepreg. Aviation materials and technologies, 2023, no. 4 (73), paper no. 07. Available at: http://www.journal.viam.ru (accessed: October 08, 2025). DOI: 10.18577/2713-0193-2023-0-4-66-77.
  18. Medvedeva K.A., Cherezova E.N. Study of new aminophenolic compounds as hardeners for epoxy oligomers. Fundamentalnye issledovaniya, 2013, no. 6, part 5, pp. 1085–1088.
  19. Semenychev V.V., Salakhova R.K. Device for assessing coating properties. Zavodskaya laboratoriya. Diagnostika materialov, 2017, vol. 83, no. 2, pp. 60–65.
  20. Salakhova R.K., Kirilin S.G., Tikhoobrazov A.B., Smirnova T.B. Scratch testing of electrolytic nickel coatings on a carbon fiber substrate. Vestnik Samarskogo universiteta. Aerokosmicheskaya tekhnika, tekhnologii i mashinostroyenie, 2021, vol. 20, no. 4, pp. 100–114.
  21. Zabolotnov A.S., Gostev S.S., Maklakova I.A. et al. Influence of Crystalline Structure on a Set of Physicomechanical Characteristics of Composite Materials Based on Ultra-High Molecular Weight Polyethylene. Vysokomolekulyarnye soyedineniya. Ser.: B, 2023, vol. 65, no. 5, pp. 341–346.
  22. Matveeva L.Yu., Yastrebinskaya A.V. Relationship between Supramolecular Structure and Properties of Polymer Composite Materials Based on Thermosetting Binders. Vestnik BGTU im. V.G. Shukhova, 2017, no. 12, pp. 49–54.
  23. Veshkin E.A., Slavin A.V., Postnova M.V., Apalkova A.V. The role of temperature-time curing conditions in the formation of unidirectional and equally strong carbon fiber plastics properties. Aviation materials and technologies, 2025, no. 2 (79), paper no. 05. Available at: http://www.journal.viam.ru (accessed: October 16, 2025). DOI: 10.18577/2713-0193-2025-0-2-59-71.