Application of energy criterion to evaluate fatigue life of nickel alloy obtained by selective laser melting
UDC
669.018.44:669.245
DOI
10.18577/2307-6046-2025-0-12-149-169
Article PDF (Russian)
(1.87 MB)
How to cite
Ryzhkov P.V., Gorbovets M.A. Application of energy criterion to evaluate fatigue life of nickel alloy obtained by selective laser melting // Proceedings of VIAM. 2025. No. 12. DOI: 10.18577/2307-6046-2025-0-12-149-169. URL: https://www.viam-works.ru/en/journal/2025/12/13
Keywords
mechanical properties, fatigue characteristics, heat-resistant wrought nickel alloys, material models, fatigue crack growth rate, cyclic plasticity
Abstract
Using laboratory samples as an example, a damage development model combining the assessment of the durability of the nucleation and propagation stages was tested. The LCF criterion based on the energy criterion determines the durability of the first stage of the kinetic diagram. The choice of the initial crack length for calculating the second stage is determined by the beginning of the linear section of the kinetic diagram. To calculate the residual durability, it is necessary to have a curve of the dependence of the SIF on the crack length for the geometry of the sample, the type of loading and the shape of the crack. The durability prediction error for the proposed model was 20 %.
Reference list
- Kablov E.N., Evgenov A.G., Petrushin N.V. Next-Generation Materials and Digital Additive Technologies for the Production of Resource Parts in FGUP VIAM: IV. Development of Superalloys. Russian Metallurgy (Metally), 2023, vol. 2023, pp. 1879–1887.
- Kablov E.N., Evgenov A.G., Petrushin N.V. Next-Generation Materials and Digital Additive Technologies for the Production of Resource Parts in FGUP VIAM: III. Adaptation and Creation of Materials. Russian Metallurgy (Metally), 2023, vol. 2023, pp. 743–751.
- Kablov E.N., Evgenov A.G., Bakradze M.M. Next-Generation Materials and Digital Additive Technologies for the Production of Resource Parts in FGUP VIAM: I. Synthesis Materials and Technologies. Russian Metallurgy (Metally), 2022, vol. 2022, pp. 611–618.
- Kablov E.N., Evgenov A.G., Petrushin N.V. On the Mechanism of Formation of the Fine Structure of a Track in Selective Laser Melting. Metal Science and Heat Treatment, 2023, vol. 65, pp. 104–115.
- Beretta S. More than 25 years of extreme value statistics for defects: Fundamentals, historical developments, recent applications. International Journal of Fatigue, 2021, vol. 151, p. 106407. DOI: 10.1016/j.ijfatigue.2021.106407.
- Movenko D.A., Shurtakov S.V. Microcrack formation and controlling in nickel superalloys processed by selective laser melting (review). Aviation materials and technologies, 2022, no. 2 (67), paper no. 04. Available at: http://www.journal.viam.ru (accessed: November 11, 2024). DOI: 10.18577/2713-0193-2022-0-2-43-51.
- Rogers J., Elambasseril J., Wallbrink C. et al. The impact of surface orientation on surface roughness and fatigue life of laser-based powder bed fusion Ti-6Al-4V. Additive Manufacturing, 2024, vol. 85, p. 104149. DOI: 10.1016/j.addma.2024.104149.
- Macoretta G., Romanelli L., Santus C. et al. Modelling of the surface morphology and size effects on fatigue strength of L-PBF Inconel 718 by comparing different testing specimens. International Journal of Fatigue, 2024, vol. 181, p. 108120. DOI: 10.1016/j.ijfatigue.2023.108120.
- Rivolta B., Gerosa R., Panzeri D. Selective laser melted 316L stainless steel: Influence of surface and inner defects on fatigue behavior. International Journal of Fatigue, 2023, vol. 172, p. 107664. DOI: 10.1016/j.ijfatigue.2023.107664.
- Demina Yu.A., Beletsky E.N., Bolotnikov A.I. Influence of surface condition on the mechanical properties and fracture kinetics of 316L steel samples obtained by selective laser melting. Deformatsiya i razrushenie materialov, 2024, no. 12, pp. 26–38. DOI: 10.31044/1814-4632-2024-12-26-38.
- Kethamukkala K., Meng C., Chen J., Liu Y. Crack growth-based life prediction for additively manufactured metallic materials considering surface roughness. International Journal of Fatigue, 2023, vol. 176, p. 107914. DOI: 10.1016/j.ijfatigue.2023.107914.
- Kryzhevich G.B., Filatov A.R. Model of elastoplastic deformation of aluminum alloys and criteria for low-cycle fatigue of structures. Trudy Krylovskogo gosudarstvennogo nauchnogo tsentra, 2018, special is. no. 2, pp. 85–95. DOI: 10.24937/2542-2324-2018-2-S-I-85-95.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Evgenov A.G., Bazyleva O.A., Golovlev N.A., Zaitsev D.V. Features of structure and property of alloys on the basis of Ni3Al intermetallic compound, half-scientists method SLM. Trudy VIAM, 2018, no. 12 (72), paper no. 03. Available at: http://www.viam-works.ru (accessed: December 10, 2024). DOI: 10.18577/2307-6046-2018-0-12-25-36.
- Ospennikova O.G., Naprienko S.A., Medvedev P.N., Zaitsev D.V., Rogalev A.M. Features of the formation of the structural-phase state of the EP648 alloy during selective lase manufacture. Trudy VIAM, 2021, no. 8 (102), paper no. 01. Available at: http://www.viam-works.ru (accessed: January 21, 2025). DOI: 10.18577/2307-6046-2021-0-8-3-11.
- Erasov V.S., Oreshko E.I. Fatigue tests of metal materials (review). Part 1. Main definitions, loading parameters, representation of results of tests. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 59‒70. DOI: 10.18577/2071-9140-2020-0-4-59-70.
- Erasov V.S., Oreshko E.I. Tests for fatigue of metal materials (review). Part 2. Analysis of the Basquin–Manson–Coffin equation. Methods of testing and processing of results. Aviation materials and technology, 2021, no. 1 (62), paper no. 08. Available at: http://www.journal.viam.ru (accessed: 10.12.2024). DOI: 10.18577/2713-0193-2021-0-1-80-94.
- The electronic reference on modeling of structural mechanics. Comsol Multiphysics. Available at: https://www.comsol.com (accessed: December 01, 2024).
- Kujawski D. A deviatoric version of the SWT parameter. International Journal of Fatigue, 2014, vol. 67, pp. 95–102. DOI: 10.1016/j.ijfatigue.2013.12.002.
- Simo J.C., Hughes T.J.R. Computational Inelasticity. New York: Springer, 1998, 392 р.
- Levenberg К. A method for the solution of certain nonlinear problems in least squares. Quarterly of Applied Mathematics, 1944, vol. 2, pp. 164–168.
- Marquardt D.W. An algorithm for least-squares estimation of nonlinear parameters. Journal of the Society for Industrial and Applied Mathematics, 1963, vol. 11, pp. 431–441.