The implication of powder mixture composition and heat treatment duration on the properties of thermal diffusion aluminium-zinc coating

Sofronova D.A., Yaroshevskaya V.N., Koltsova M.А., Lonskii S.L., Knyazev A.V., Kurshev E.V.
Sofronova D.A., Yaroshevskaya V.N., Koltsova M.А., Lonskii S.L., Knyazev A.V., Kurshev E.V. The implication of powder mixture composition and heat treatment duration on the properties of thermal diffusion aluminium-zinc coating // Proceedings of VIAM. 2025. No. 12. DOI: 10.18577/2307-6046-2025-0-12-126-136. URL: https://www.viam-works.ru/en/journal/2025/12/11
Keywords
thermodiffusion coatings, zinc, aluminium, steel, corrosion, protective coatings
Abstract

The influence of the composition of the powder mixture and of the heat treatment modes upon the formation of thermodiffusional aluminium-zinc coatings has been investigated. It was found that at a temperature of 450°С the coatings have aluminium based outer layer, at a temperature of 380 °С the aluminum content in the zinc is about 10 %. The obvious influence of the composition of the mixture and of the heat treatment regime on the corrosion properties has not been established, the corrosion current is in the order of 10–6 А/cm2, and the corrosion potential is about 0,9 V in 3 % NaCl solution.

Reference list
  1. Kablov E.N. Corrosion or life. Nauka i zhizn, 2012, no. 11, pp. 16–21.
  2. Kablov E.N., Startsev O.V., Medvedev I.M. Review of international experience on corrosion and corrosion protection. Aviacionnye materialy i tehnologii, 2015, no. 2 (35), pp. 76–87. DOI: 10.18577/2071-9140-2015-0-2-76-87.
  3. Kablov E.N., Antipov V.V. The role of new generation materials in ensuring the technological sovereignty of the Russian Federation. Vestnik Rossiyskoy akademii nauk, 2023, vol. 93, no. 10, pp. 907–916.
  4. Vinogradov S.S., Nikiforov A.A., Demin S.A., Chesnokov D.V. Protection against corrosion of carbon steel. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 242–263. DOI: 10.18577/2071-9140-2017-0-S-242-263.
  5. Zakirova L.I., Laptev A.B. Properties of protective electroplating coatings for replacement of cadmium on steel fixing parts (review). Part 1. Morphology and corrosion resistance. Aviaсionnye materialy i tehnologii, 2020, no. 3 (60), pp. 37–46. DOI: 10.18577/2071-9140-2020-0-3-37-46.
  6. Laptev A.B., Zakirova L.I., Degovets M.L. Properties of protective galvanic coatings for replacement of cadmium on steel fixing parts (review). Part 2. Hydrogen embrittlement and frictional characteristics. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 35–40. DOI: 10.18577/2071-9140-2020-0-4-35-40.
  7. Kablov E.N., Nikiforov A.A., Demin S.A., Chesnokov D.V., Vinogradov S.S. Advanced Coatings for Corrosion Protection of Carbon Steels. Stal, 2016, no. 6, pp. 70–81.
  8. Proskurin E.V., Gorbunov N.S. Diffusion Zinc Coatings. Moscow: Metallurgiya, 1972, 248 p.
  9. Kablov E.N., Khmeleva K.M., Zavarzin S.V., Kozlov I.A., Lonskii S.L. The effect of heat treatment on the characteristics of aluminium-zinc coatings obtained by the cold spray method. Aviation materials and technologies, 2022, no. 1 (66), paper no. 07. Available at: http://www.journal.viam.ru (ассеssed: April 07, 2025). DOI: 10.18577/2713-0193-2022-0-1-78-91.
  10. Astalyukhina A.S., Pikalov E.S. Characteristics of modern methods of applying protective zinc coatings. Uspekhi sovremennogo estestvoznaniya, 2015, no. 11-1, pp. 11–14.
  11. Evgenov A.G., Shurtakov S.V., Prager S.M., Malinin R.Yu. On the development of a universal calculation method for assessing the degradation of recycled metal powder materials, depending on the cyclicity of use in the selective laser melting process. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 3–11. DOI: 10.18577/2071-9140-2020-0-4-3-11.
  12. Composition of powder mixture for thermal diffusion treatment of steel products, method of thermal diffusion treatment of steel products: pat. RU2685841C1 Rus. Federation; appl. 15.10.18; publ. 23.04.19.
  13. Zhigunov K.V. General patterns of diffusion saturation processes during thermochemical treatment. Mashinostroitel, 2004, no. 1, pp. 26–27.
  14. Shen T.H., Tsai C.Y., Lin C.S. Growth behavior and properties of Zn–Al pack cementation coatings on carbon steels. Surface and Coatings Technology, 2016, vol. 306, pp. 455–461.
  15. Mahdavi A. Corrosion Resistance of Boronized, Aluminized, and Chromized Thermal Diffusion-Coated Steels in Simulated High-Temperature Recovery Boiler Conditions. Coatings, 2018, vol. 8 (8), p. 257.
  16. Sun A., Xiaoming S., Li H., Wang Q. Interface microstructure and mechanical properties of zinc–aluminum thermal diffusion coating on AZ31 magnesium alloy. Materials & Design, 2015, vol. 1004–1005, pp. 154–157.
  17. Method of diffusion galvanizing of metal parts: pat. RU2593252C2 Rus. Federation; appl. 29.12.14; publ. 10.08.16.
  18. Beckert M., Klemm H. Methods of metallographic etching. Trans. from Germ. 2nd ed., rev. and add. Moscow: Metallurgiya, 1988, 268 p.
  19. Eliseev E.A., Sevalnev G.S., Doroshenko A.V., Druzhinina M.E. Influence of time-temperature parameters of long-duration exposure on transformations in structural steels (review). Aviation materials and technologies, 2021, no. 2 (63), paper no. 02. Available at: http://www.journal.viam.ru (accessed: 07.04.2025). DOI: 10.18577/2713-0193-2021-0-2-15-23.
  20. Natrup F., Graf W. Sherardizing: corrosion protection of steels by zinc diffusion coatings. Thermochemical Surface Engineering of Steels. Elsevier Ltd., 2015, pp. 737–750.
  21. Xue Q., Sun C., Yu J. et al. Microstructure evolution of a Zn-Al coating co-deposited on low-carbon steel by pack cementation. Journal of Alloys and Compounds, 2017, vol. 699, pp. 1012–1021.
  22. Kovalenko V.S. Metallographic reagents: handbook. Moscow: Metallurgiya, 1981, 120 p.
  23. Khmeleva K.M., Zavarzin S.V., Kozlov I.A., Lonskiy S.L. Effect of heat treatment on the corrosion properties of aluminum-zinc coatings obtained by the CGD method. Climate-2022: modern approaches to assessing the impact of external factors on materials and complex technical systems: Proc. VII All-Rus. sc. and tech. conf. Moscow: NRC «Kurchatov Institute» – VIAM, 2022, pp. 171–192.