The use of metal composite materials in the manufacturing of internal combustion engines in the automotive industry

Kosolapov D.V., Khodykin L.G., Nyafkin A.N., Khodykin D.L.
Kosolapov D.V., Khodykin L.G., Nyafkin A.N., Khodykin D.L. The use of metal composite materials in the manufacturing of internal combustion engines in the automotive industry // Proceedings of VIAM. 2025. No. 11. DOI: 10.18577/2307-6046-2025-0-11-86-101. URL: https://www.viam-works.ru/en/journal/2025/11/8
Keywords
piston, internal combustion engines, composite material, aluminum alloy, mechanical properties
Abstract

A brief scientific and technical literature review is presented in the field of application of metal composite materials (MMCs) in manufacturing of internal combustion engines, in particular, design and manufacturing of pistons. Methods for producing MMCs with various reinforcing components are described. The test results for MMCs and pistons made from them are shown. The results of work on manufacturing of piston blanks from MMCs at the National Research Center “Kurchatov Institute” – VIAM are presented.

Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N., Antipov V.V. The role of new generation materials in ensuring the technological sovereignty of the Russian Federation. Vestnik Rossiyskoy akademii nauk, 2023, vol. 93, no. 10, pp. 907–916. DOI: 10.31857/S0869587323100055.
  3. Antipov V.V. Prospects for development of aluminium, magnesium and titanium alloys for aerospace engineering. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 186–194. DOI: 10.18577/2071-9140-2017-0-S-186-194.
  4. Kablov E.N., Belov E.V., Trapeznikov A.V., Leonov A.A., Zaitsev D.V. Strengthening features and aging kinetics of high-strength cast aluminum alloy AL4MS based on Al–Si–Cu–Mg system. Aviation materials and technologies, 2021, no. 2 (63), paper no. 03. Available at: http://www.journal.viam.ru (accessed: August 18, 2024). DOI: 10.18577/2713-0193-2021-0-2-24-34.
  5. Khodykin L.G., Nyafkin A.N., Kosolapov D.V., Zhabin A.N. Laser welding of metal composite materials based on aluminium alloy reinforced with refractory particles SiC (review). Trudy VIAM, 2022, no. 12 (118), paper no. 06. Available at: http://www.viam-works.ru (accessed: August 18, 2024). DOI: 10.18577/2307-6046-2022-0-12-63-75.
  6. Erasov V.S., Sibayev I.G. Scheme for the development and evaluation of properties of structural aviation composite materials. Aviation materials and technologies, 2023, no. 1 (70), paper no. 05. Available at: http://www.journal.viam.ru (accessed: August 18, 2024). DOI: 10.18577/2713-0193-2023-0-1-61-81.
  7. Kosolapov D.V., Shavnev A.A., Kurbatkina E.I., Nyafkin A.N., Gololobov A.V. Study on structure and properties of dispersion hardened MMC based on aluminium alloy of Al–Mg–Si system. Trudy VIAM, 2020, no. 1, paper no. 06. Available at: http://www.viam-works.ru (accessed: August 18, 2024). DOI: 10.18577/2307-6046-2020-0-1-58-67.
  8. Shavnev A.A., Nerush S.V., Kurbatkina E.I., Kosolapov D.V., Medvedev P.N. Study of the structure of a metallic composite material of the Al–Si–Mg–SiC system obtained using mechanical alloying. Izvestiya vuzov. Poroshkovaya metallurgiya i funktsionalnye pokrytiya, 2022, no. 1, pp. 17–25. DOI: 10.17073/1997-308X-2022-1-17-25.
  9. Imametdinov E.S., Valueva M.I. Сomposites for piston engines (rеview). Aviacionnye materialy i tehnologii, 2020, no. 3 (60), pp. 19–28. DOI: 10.18577/2071-9140-2020-0-3-19-28.
  10. Abramova M.G. Full-scale accelerated tests of aluminum alloys at continental and marine type stations. Aviacionnye materialy i tehnologii, 2020, no. 3 (60), pp. 57–65. DOI: 10.18577/2071-9140-2020-0-3-57-65.
  11. Jinsheng M., Liwei S., Yongxiang H. Application of Composite Materials in Engine. Materials Science: Advanced Composite Materials, 2017, vol. 1, pp. 1–9. DOI: 10.18063/msacm.v1i1.499.
  12. Anilkumar H.C., Hebbar H.S., Ravishankar K.S. Mechanical properties Of SiC Reinforced Aluminium Alloy Composites. IJMME, 2011, vol. 6, is. 1, pp. 41–45.
  13. Falsafia J., Rosochowskaa M., Jadhava P., Tricker D. Lower cost automotive piston from 2124/SiC/25p metal-matrix composite. SAE International Journal of Engines, 2017, vol. 10, no. 4, pp. 1984–1992. DOI: 10.4271/2017-01-1048.
  14. Zhitnyuk S.V., Medvedev P.N. Investigation of microstructure and phase composition of the metallic composite material Al–Si–Mg system modified by silicon carbide particles by mechanical alloying. Part 1. Trudy VIAM, 2023, no. 1 (119), paper no. 08. Available at: http://www.viam-works.ru (accessed: August 18, 2024). DOI: 10.18577/2307-6046-2023-0-1-97-106.
  15. Dolata-Grosz A., Dyzia M., Śleziona J., Wieczorek J. Composites applied for pistons. Archives of foundry engineering, 2007, vol. 7, is. 1, pp. 37–40.
  16. Dhanesh C., Anand T., Venkatesan J. Analysis of Bronze Hybrid Composite for Spark Ignition Engine Piston. FME Transactions, 2020, vol. 48, no. 4, p. 967.
  17. Ishizuka K., Kusakai K., Imai N. Development of metal matrix composite piston. Honda R&D Technical Review F1 Special (The Third Era Activities), 2009, pp. 246–247. Available at: https://www.hondarandd.jp/summary.php?sid=23&lang=en (accessed: August 18, 2024).
  18. Jankowski A., Kowalski M. Design of a new alloy for internal combustion engines pistons. Proceedings of the 7th International Conference on Mechanics and Materials in Design. Albufeira, 2017, pp. 11–15.
  19. Haitham M.I. Al-Zuhairi, Iqbal Alshalal. Enhancement of Mechanical Properties of Aluminum Piston Alloy Using Al2O3 Material. 6th International engineering conference «Sustainable Technology and Development». Erbil, 2020, pp. 196–200. DOI: 10.1109/IEC49899.2020.9122921.
  20. Kumar M., Padmanabhan G., Kottara A.A., Shankar K.V. Analysis of aluminium metal matrix composite piston for automobile applications. AIP Conference Proceedings, 2020, vol. 2273, p. 050049. DOI: 10.1063/5.0024235.