Evaluation of the possibility of using vacuum forming technology of prepregs and semipregs for the production of rehabilitation equipment for the disabled

Donetskiy K.I., Karavaev R.Y., Gracheva A.D., Stretyachuk I.V., Shebbo M.F.M.
Donetskiy K.I., Karavaev R.Y., Gracheva A.D., Stretyachuk I.V., Shebbo M.F.M. Evaluation of the possibility of using vacuum forming technology of prepregs and semipregs for the production of rehabilitation equipment for the disabled // Proceedings of VIAM. 2025. No. 11. DOI: 10.18577/2307-6046-2025-0-11-73-85. URL: https://www.viam-works.ru/en/journal/2025/11/7
Keywords
prepreg, semipreg, vacuum forming, binder, process package, vacuum treatment, impregnation, polymer composite materials, rehabilitation equipment for the disabled
Abstract

Due to their increasing use in a wide variety of industries, primarily civil ones, polymer composite materials processed using non-autoclave molding are becoming increasingly popular due to their low cost and simple equipment. A current application of polymer composite materials is the manufacture of rehabilitation equipment for the disabled and, in particular, components of everyday and running foot modules, which are currently manufactured using imported materials.

Reference list
  1. Kablov E.N. New Generation Materials and Technologies for Their Digital Processing. Herald of the Russian Academy of Sciences, 2020, vol. 90, no. 2, pp. 225–228.
  2. Onishchenko G.G., Kablov E.N., Ivanov V.V. Scientific and technological development of Russia in the context of achieving national goals: problems and solutions. Innovatsii, 2020, no. 6 (260), pp. 3–16.
  3. Kablov E.N., Antipov V.V. The role of new generation materials in ensuring technological sovereignty of the Russian Federation. Vestnik Rossiyskoy akademii nauk, 2023, vol. 93, no. 10, pp. 907–916.
  4. Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), paper no. 10. Available at: http://www.journal.viam.ru (accessed: January 31, 2025). DOI: 10.18577/2713-0193-2023-0-2-122-144.
  5. Raskutin A.E. Russian polymer composite materials of new generation, their exploitation and implementation in advanced developed constructions. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 349–367. DOI: 10.18577/2071-9140-2017-0-S-349-367.
  6. Mikhailin Yu.A. Fibrous polymer composite materials in engineering. St. Petersburg: Nauchnye osnovy i tekhnologii, 2013, 720 p.
  7. Valueva M.I., Evdokimov A.A., Nacharkina A.V., Gubin A.M. Polymer composite materials and technologies in the automotive industry (rеview). Trudy VIAM, 2022, no. 1 (107), paper no. 06. Available at: http://www.viam-works.ru (accessed: October 05, 2025). DOI: 10.18577/2307-6046-2022-0-1-53-65.
  8. Donetskiy K.I., Karavaev R.Yu., Bystrikova D.V., Gracheva A.D., Tkachuk A.I. Semipregs and carbon fiber reinforced plastics based on them. Trudy VIAM, 2025, no. 8 (150), paper no. 08. Available at: http://www.viam-works.ru (accessed: October 02, 2025). DOI: 10.18577/2307-6046-2025-0-8-85-99.
  9. Berring N.S., Renieri M.P., Bond G.G., Palmer D.J. Autoclave vs. Non-Autoclave: A comparison of hat-stiffened subcomponents by static and fatigue testing and related non-destructive evaluations. 2012 SAMPE International Symposium and Exhibition-Emerging Opportunities: Materials and Process Solutions. Baltimore MD, 2012, рр. 23–25.
  10. Garschke C., Weimer C., Parlevliet P.P., Fox B.L. Out-of-autoclave cure cycle study of a resin film infusion process using in situ process monitoring. Composites. Part A: Applied Science and Manufacturing, 2012, vol. 43, is. 6, pp. 935–944.
  11. Levy A., Hubert P. Vacuum-bagged composite laminate forming processes: Predicting thickness deviation in complex shapes. Composites. Part A: Applied Science and Manufacturing, 2019, vol. 126, p. 105568.
  12. Ma Y., Centea T., Nutt S.R. Defect reduction strategies for the manufacture of contoured laminates using vacuum BAG-only prepregs. Polymer Composites, 2017, vol. 38, pp. 2016–2025.
  13. Tkachuk A.I., Donetsky K.I., Terekhov I.V., Karavaev R.Yu. The use of thermosetting matrices for the manufacture of polymer composite materials by the non-autoclave molding methods. Aviation materials and technology, 2021, no. 1 (62), paper no. 03. Available at: https://www.journal.viam.ru (accessed: October 01, 2025). DOI: 10.18577/2713-0193-2021-0-1-22-33.
  14. Sidorina A.I., Safronov A.M., Kutsevich K.E., Klimenko O.N. Carbon fabrics for aircraft products. Trudy VIAM, 2020, no. 12 (94), paper no. 05. Available at: http://www.viam-works.ru (accessed: October 16, 2025). DOI: 10.18577/2307-6046-2020-0-12-47-58.
  15. Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composites (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 48–58. DOI: 10.18577/2071-9140-2019-0-3-48-58.
  16. Order of the Federal Service for Environmental, Technological and Nuclear Supervision dated December 15, 2020 No. 536 «On approval of federal norms and rules in the field of industrial safety «Industrial safety rules for the use of equipment operating under excess pressure». Available at: http://www.infobm.ru/upload/Правила%20промышленной%20безопасности%20при%20ис-пользовании%20оборудования.pdf (accessed: October 10, 2025).
  17. Puzyretskiy E.A., Donetski K.I., Shabalin L.P., Karavaev R.Yu., Savinov D.V. Theoretical and experimental study of the vacuum forming of semipregs based on carbon fillers (tapes and fabric) and melting epoxy binding. Aviation materials and technologies, 2024, no. 2 (75), paper no. 08. Available at: http://www.journal.viam.ru (accessed: October 01, 2025). DOI: 10.18577/2713-0193-2024-0-2-109-121.
  18. Сentea T., Grunenfelder L.K., Nutt S.R. A review of out-of-autoclave prepregs – material properties, process phenomena and manufacturing considerations. Composites. Part A: Applied Science and Manufacturing, 2014, vol. 70, pp. 132–154.
  19. Donetskyi K.I., Timoshkov P.N., Safronov A.M., Goncharov V.A., Mishchun M.I. Autoclave-free molding of prepregs. Konstruktsii iz kompozitsionnykh materialov, 2022, no. 1 (165), pp. 29–34.
  20. Farhang L., Fernlund G. Experimental study of void evolution in partially impregnated prepregs. Journal of Composite Materials, 2019, vol. 54, pp. 1511–1523.
  21. Levy A., Kratz J., Hubert P. Air evacuation during vacuum bag only prepreg processing of honeycomb sandwich structures: In-plane air extraction prior to cure. Composites. Part A: Applied Science and Manufacturing, 2015, vol. 68, pp. 365–376.
  22. Schechter S.G.K., Grunenfelder L.K., Nutt S.R. Air evacuation and resin impregnation in semi-pregs: effects of feature dimensions. Advanced Manufacturing: Polymer & Composites Science, 2020, vol. 6, is. 2, pp. 101–114.