Investigation of the kinetics of curing of an epoxy binder in a prepreg based on an equal-strength fabric using multivariate regression methods

Skuridina N.S., Bolshakov V.A., Klimenko O.N., Barinov D.Y.
Skuridina N.S., Bolshakov V.A., Klimenko O.N., Barinov D.Y. Investigation of the kinetics of curing of an epoxy binder in a prepreg based on an equal-strength fabric using multivariate regression methods // Proceedings of VIAM. 2025. No. 11. DOI: 10.18577/2307-6046-2025-0-11-12-22. URL: https://www.viam-works.ru/en/journal/2025/11/2
Keywords
kinetics of curing, differential scanning calorimetry, correlation coefficient, reaction mechanism, conversion rate, polymer composite material, regression analysis
Abstract

The selection of the optimal kinetic model of curing of a molten epoxy binder in a prepreg based on an equal-strength carbon fabric is considered step by step. The influence of the process stages and the reaction flow pattern on the coefficient of determination of experimental and calculated dependences is shown. Using the methods of multivariate nonlinear regression, two functional dependencies between factors and response were analyzed according to the Prout–Tompkins and Avrami–Erofeev models. The kinetic parameters of the curing reaction have been refined.

Reference list
  1. Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
  2. Kablov E.N. The Role of Fundamental Research in the Creation of Next-Generation Materials. XXI Mendeleev Congress on General and Applied Chemistry: in 6 vols. St. Petersburg, 2019, vol. 3, p. 24.
  3. Kablov E.N. Materials – the Foundation of Any Business. Delovaya slava Rossii, 2013, no. 2 (40), рp. 4–9.
  4. Amirova L.M., Andrianova K.A., Amirov R.R. Epoxy Resins and Composites Based on Them: textbook. Kazan: KNITU–KAI, 2021, 216 p.
  5. Sitnikova V.E., Ponomareva A.A., Uspenskaya M.V. Methods of Thermal Analysis: workshop. St. Petersburg: ITMO University, 2021, 152 p.
  6. Bolshakov V.A., Antyufeeva N.V. Evaluation of the curing process model of the adhesive binder in prepreg. Aviation materials and technologies, 2023, no. 4 (73), paper no. 07. Available at: http://www.journal.viam.ru (accessed: January 28, 2025). DOI: 10.18577/2713-0193-2023-0-4-66-77.
  7. Terekhov I.V., Tkachuk A.I., Donetsky K.I., Karavaev R.Yu. Technological and operational characteristics of the VSE-62 low-viscosity epoxy resin with increased pot life and its application. Aviation materials and technologies, 2021, no. 2 (63), paper no. 05. Available at: http://www.journal.viam.ru (accessed: February 05, 2025). DOI: 10.18577/2713-0193-2021-0-2-43-50.
  8. Malysheva G.V., Marakhovskiy P.S., Barinov D.Ya., Nikolaev E.V. Optimization of the curing modes of fiber-glass based on epoxy binder. Aviation materials and technologies, 2023, no. 2 (71), paper no. 08. Available at: http://www.journal.viam.ru (accessed: January 28, 2025). DOI: 10.18577/2713-0193-2023-0-2-94-103.
  9. Tkachuk A.I., Donetsky K.I., Terekhov I.V., Karavaev R.Yu. The use of thermosetting matrices for the manufacture of polymer composite materials by the non-autoclave molding methods. Aviation materials and technology, 2021, no. 1 (62), paper no. 03. Available at: http://www.journal.viam.ru (accessed: February 05, 2025). DOI: 10.18577/2713-0193-2021-0-1-22-33.
  10. Kiseleva D.V., Sadykova N.O. Kinetic analysis of thermogravimetric data of fossil bone remains. Proceedings of the A.N. Zavaritsky Institute of Geology and Geochemistry, 2010, no. 157, pp. 336–339.
  11. Chutskova E.Yu., Aleksashin V.M., Barinov D.Ya., Dementyeva L.A. The differential scanning calorimetry application for kinetic regularities investigation of the epoxy adhesive VK-36R curing process. Trudy VIAM, 2015, no. 1, paper no. 12. Available at: http://www.viam-works.ru (accessed: February 10, 2025). DOI: 10.18577/2307-6046-2015-0-1-12-12.
  12. Khalafyan A.A. STATISTICA 6. Statistical analysis of data. 3rd ed. Moscow: Binom-Press, 2007, 512 p.
  13. Anoshkin A.N., Zuyko V.Yu., Shipunov G.S., Tretyakov A.A. Technologies and problems of mechanics of composite materials for creating a straightener blade for an aircraft engine. Vestnik PNIPU. Mekhanika, 2014, no. 4, pp. 5–44. DOI: 10.15593/perm.mech/2014.4.01.
  14. Mishkin S.I. Application of carbon fiber plastics in constructions of pilotless devices (review). Trudy VIAM, 2022, no. 5 (111), paper no. 08. Available at: http://www.viam-works.ru (accessed: February 18, 2025). DOI: 10.18577/2307-6046-2022-0-5-87-95.
  15. Gunyaev G.M., Zhelezina G.F., Krivonos V.V., Rumyantsev A.F. Polymer composite materials in aircraft structures. Aviatsionnye materialy i tekhnologii, 2002, no. S1, pp. 12–20.
  16. Amirova L.R., Khamidullin O.L., Zalyalova G.M., Amirova L.M. Assessment of kinetic parameters of the curing process of epoxyanhydride systems by DSC. Izvestiya Akademii nauk. Seriya khimicheskaya, 2017, no. 3, pp. 483–487.
  17. Abiev R.Sh., Bibik E.E., Vlasov E.A. New reference book for chemist and technologist. Electrode processes. Chemical kinetics and diffusion. Colloidal chemistry. St. Petersburg: Professional, 2004, 838 p.
  18. Young D. Kinetics of Decomposition of Solids. Moscow: Mir, 1969, 263 p.
  19. Khaskov M.A. Expansion of the Temperature–Time–Transformation Diagram Taking into Account the Thermophysical Properties of Components for Optimizing the Curing Modes of Polymer Composite Materials. Zhurnal prikladnoy khimii (Journal of Applied Chemistry), 2016, vol. 89, no. 4, pp. 510–518.
  20. Irzhak T.F., Mezhikovsky S.M., Irzhak V.I. On the Physical Meaning of the Avrami Equation in Oligomer Curing Reactions. Vysokomolekulyarnye soedineniya, Series B, 2008, vol. 50, no. 8, pp. 1563–1565.