The effect of the transition of air temperature through zero on the surface integrity of a polymer material

Part 1. Moistening
Laptev A.B., Matishov G.G., Krivushina A.A., Pavlov M.R., Nikolaev E.V.
Laptev A.B., Matishov G.G., Krivushina A.A., Pavlov M.R., Nikolaev E.V. The effect of the transition of air temperature through zero on the surface integrity of a polymer material. Part 1. Moistening // Proceedings of VIAM. 2025. No. 11. DOI: 10.18577/2307-6046-2025-0-11-147-156. URL: https://www.viam-works.ru/en/journal/2025/11/13
Keywords
polymer, hydrophilicity, wetting edge angle, moisture saturation, moisture content gradient, capillary pressure
Abstract

The article describes processes of surface moistening and moisture sorption with a polymer material using known physical dependencies. Moisture saturation depends on size of pores, surface contact angle (polymer hydrophilicity), temperature and pressure. It is shown that moisture saturation leads to the formation of a moisture content gradient and gradual destruction, cracking, aging and discoloration of the polymer from the surface due to tensile stresses in the presence of a moisture gradient between the surface and inner layers of the polymer material.

Reference list
  1. Kablov E.N., Laptev A.B., Prokopenko A.N., Gulyaev A.I. Relaxation of polymeric composite materials under the prolonged action of static load and climate (review). Part 1. Binders. Aviation materials and technologies, 2021, no. 4 (65), paper no. 08. Available at: http://www.journal.viam.ru (accessed: May 10, 2025). DOI: 10.18577/2307-6046-2021-0-4-70-80.
  2. Kablov E.N. New generation materials and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
  3. Kablov E.N., Kondrashov S.V., Melnikov A.A., Schur P.A. Application of functional and adaptive materials obtained by 3D printing (review). Trudy VIAM, 2022, no. 2 (108), paper no. 03. Available at: http://www.viam-works.ru (accessed: May 20, 2025). DOI: 10.18577/2307-6046-2022-0-2-32-51.
  4. Laptev A.B., Pavlov M.R., Novikov A.A., Slavin A.V. Current trends in the development of testing materials for resistance to climatic factors (review). Part 2. Main trends. Trudy VIAM, 2021, no. 2 (96), paper no. 11. Available at: http://www.viam-works.ru (accessed: May 20, 2025). DOI: 10.18577/2307-6046-2021-0-2-99-108.
  5. Whiteside M., Herndon J.M. Unequivocal Detection of Solar Ultraviolet Radiation 250‒300 nm (UV-C) at Earth's Surface. European Journal of Applied Sciences, 2023, vol. 11, no. 2, pp. 455–472. DOI: 10.14738/aivp.112.14429.
  6. Startsev O.V., Kychkin A.K., Lebedev M.P., Polyakov V.V. Effects of moisture on aging of polymer composite materials in a cold climate. Procedia Structure Integration, 2020, vol. 30, pp. 162–166.
  7. Startsev V.O., Startsev O.V., Zeleneva T.O., Vardanyan A.M. The influence of precipitation on the change in the mass of polymer composite material samples under open climatic conditions. Climate–2023: modern approaches to assessing the impact of external factors on materials and complex technical systems: collection of reports. VIII All-Rus. sc. and tech. conf. (September 29, 2023, Moscow). Moscow: NRC «Kurchatov Institute» – VIAM, 2023, pp. 131–153.
  8. Startsev V.O., Startsev O.V., Zeleneva T.O., Vardanyan A.M. Influence of precipitation on changes in the mass of samples of polymeric composite materials in open climatic conditions. Aviation materials and technologies, 2024, no. 1 (74), paper no. 11. Available at: http://www.journal.viam.ru (accessed: May 20, 2025). DOI: 10.18577/2713-0193-2024-0-1-136-154.
  9. Marakhovsky P.S., Vorobyov N.N., Gulyaev A.I., Tkachuk A.I. Influence of polyarylsulfone additives on the climatic resistance of epoxy-based carbon fiber. Vysokomolekulyarnye soyedineniya. Ser. A, 2022, vol. 64, no. 2, pp. 113–119. DOI: 10.31857/S2308112022020080.
  10. Gulyaev A.I., Yakovlev N.O., Oreshko E.I. Fractography features of interlaminar crack growth in carbon fibre reinforced plastic under various mode loading. Trudy VIAM, 2019, no. 12 (84), paper no. 11. Available at: http://www.viam-works.ru (accessed: May 20, 2025). DOI: 10.18577/2307-6046-2019-0-12-99-108.
  11. Gulyaev A.I., Medvedev P.N., Sbitneva S.V., Petrov A.A. Application of nanoindentation to determine the adhesion strength of fiber-matrix in carbon fiber reinforced plastics. The role of fundamental research in the implementation of Strategic directions for the development of materials and technologies for their processing for the period up to 2030: Proc. V All-Rus. sc. and tech. conf. (June 28, 2019, Moscow). Moscow: VIAM, 2019, pp. 240–253.
  12. Kablov E.N., Startsev V.O., Laptev A.B. Aging of polymer composite materials. Moscow: NRC «Kurchatov Institute» – VIAM, 2023, 520 p.
  13. Steadman R.G. Norms of apparent temperature in Australia. Australian Meteorological Magazine, 1994, vol. 43, pp. 1–16.
  14. De Gennes P.G., Brochard-Wyart F., Quéré D. Capillarity and Wetting Phenomena – Drops, Bubbles, Pearls, Waves. Ed. A. Reisinger. Springer, 2002, 430 p.
  15. Laptev A.B., Akhiyarov R.J., Lapteva A.A. et al. Distribution of chloride ions along the flight path of aircraft (Overview). Journal of Physics. Conference Series. IOP Publishing Ltd, 2022, vol. 2373, pp. 22008. DOI: 10.1088/1742-6596/2373/2/022008.
  16. Wenzel R.N. Resistance of solid surfaces to wetting by water. Industrial & Engineering Chemistry, 1936, vol. 28, pp. 988–994. DOI: 10.1021/IE50320A024.
  17. Cassie A.B.D., Baxter S. Wettability of porous surfaces. Transactions of The Faraday Society, 1944, vol. 40, pp. 546–551. DOI: 10.1039/TF9444000546.
  18. Crank J. The mathematics of diffusion. 2nd ed. Oxford, UK: Clarendon Press, 1975, 414 p.
  19. Lykov A.V. Heat and Mass Transfer: handbook. 2nd ed. Moscow: Energiya, 1978, 480 p.
  20. Weitsman Y.J. Composites in the sea: sorption, strength and fatigue. Twelfths Int. Con. on Composite Materials – ICCM'12: Extended abstracts. Paris, France: Instaprint S.A., 1999, pp. 210.
  21. Pomerantsev A.L. Methods of Nonlinear Regression Analysis for Modeling the Kinetics of Chemical and Physical Processes: thesis, Doct. of Sc. (Phys. & Math.). Moscow, 2003, 304 p.
  22. Krotov A.S. Diagnostics of Moisture Sorption and Diffusion Processes in Polymer Composite Materials: thesis, Cand. of Sc. (Phys. & Math.), Barnaul, 2002, 124 p.
  23. Malkin A.Ya., Chalykh A.E. Diffusion and viscosity of polymers. Measurement methods. Moscow: Khimia, 1979, 351 р.
  24. Lee S., Knaebel K.S. Effects of mechanical and chemical properties on transport in fluoropolymers. I. Transient sorption. Journal of applied polymer science, 1997, vol. 64, pp. 455–476.
  25. Perekhozhentsev A.G. Modeling of Temperature-Humidity Processes in Porous Building Materials. Part 3. Calculation of Water Vapor Diffusion Coefficients in Porous Materials Based on the Characteristics of Their Porous Structure. Stroitelnye materialy, 2013, no. 2. pp. 89–92.
  26. Vigdergauz V.E., Golberg G.Yu. Nanochemical Aspects of Mineral Particle Flocculation: Mineral Wettability and Its Effect on the Energy of Hydrophobic Interactions within the Extended DLVO Theory. Nanotekhnologii i okhrana zdorovya, 2011, vol. 3, no. 7, pp. 23–29.
  27. Startsev V.O., Nikolaev E.V., Vardanyan A.M., Nechaev A.A. The influence of climatic factors on residual stresses in nanomodified cyanate ester-based CFRP. Trudy VIAM, 2021, no. 8 (102), paper no. 12. Available at: http://www.viam-works.ru (accessed: May 20, 2025). DOI: 10.18577/2307-6046-2021-0-8-104-112.