Development trends in compositions and manufacturing technologies for powder compositions for aluminum and magnesium alloys

Mukhina I.Y., Duyunova V.A., Leonov A.A., Tokarev M.S., Trapeznikov A.V., Vlasova K.A.
Mukhina I.Y., Duyunova V.A., Leonov A.A., Tokarev M.S., Trapeznikov A.V., Vlasova K.A. Development trends in compositions and manufacturing technologies for powder compositions for aluminum and magnesium alloys // Proceedings of VIAM. 2025. No. 11. DOI: 10.18577/2307-6046-2025-0-11-3-11. URL: https://www.viam-works.ru/en/journal/2025/11/1
Keywords
magnesium and aluminum alloys, cold spraying, powder composition, surface defects, metal powder compositions
Abstract

This paper presents the results of scientific and technical research on the compositions and manufacturing technologies of powder compositions for cold spraying on castings of aluminum and magnesium alloys. The conducted research includes investigations by foreign and Russian scientists in the field of technologies for improving the characteristics of alloys through the application of functional coatings, as well as local repair of products. Technologies that do not adversely affect the applied surface and eliminate defects without additional heating are of particular interest.

Reference list
  1. Kablov E.N., Kondrashov S.V., Melnikov A.A., Schur P.A. Application of functional and adaptive materials obtained by 3D printing (review). Trudy VIAM, 2022, no. 2 (108), paper no. 03. Available at: http://www.viam-works.ru (accessed: August 20, 2024). DOI: 10.18577/2307-6046-2022-0-2-32-51.
  2. Kablov E.N. New generation materials and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
  3. Kablov E.N., Belov E.V., Trapeznikov A.V., Leonov A.A., Zaitsev D.V. Strengthening features and aging kinetics of high-strength cast aluminum alloy AL4MS based on Al–Si–Cu–Mg system. Aviation materials and technologies, 2021, no. 2 (63), paper no. 03. Available at: http://www.journal.viam.ru (accessed: August 20, 2024). DOI: 10.18577/2713-0193-2021-0-2-24-34.
  4. Mukhina I.Yu. Fundamentals of the technology of smelting magnesium alloys in protective environments. Liteynoe proizvodstvo, 2021, no. 1, pp. 2–8.
  5. Kablov E.N., Akinina M.V., Volkova E.F., Mostyaev I.V., Leonov A.A. The research of aspects of phase composition and fine structure of magnesium alloy ML9 in the as-cast and heat-treated conditions. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 17–24. DOI: 10.18577/2071-9140-2020-0-2-17-24.
  6. Mukhina I.Yu., Koshelev O.V., Koshelev A.O., Ustinov S.V., Bobryshev B.L., Bobryshev D.V. Development of technologies for eliminating metallurgical defects in complex-contour magnesium casting. Proc. of the All-Rus. sci. and pract. conf. «High-tech technologies and materials in foundry production». Moscow: MMZ «Avangard», 2019, pp. 195–220.
  7. Fomina M.A., Zakharov K.E., Yamshchikov E.I., Trofimov N.V. Selection and research of optimal paste formulation for local removal of corrosion products from magnesium alloys as well as the technology of it’s application. Aviation materials and technologies, 2023, no. 4 (73), paper no. 05. Available at: http://www.journal.viam.ru (accessed: February 20, 2025). DOI: 10.18577/2713-0193-2023-0-4-45-54.
  8. Spray coating method: pat. CN213288673U; appl. 21.08.20; publ. 28.05.21.
  9. Device and method for producing spherical type metallic magnesium powder: pat. СN112091330А; appl. 30.09.20; publ. 18.12.20.
  10. Method of repairing surface corrosion of magnesium alloy CGDS: pat. СN111485234А; appl. 29.04.20; publ. 04.08.20.
  11. Method of preparation for CGN and coating with high-etropy alloy: pat. СN113430513А; appl. 28.06.21; publ. 24.09.21.
  12. Method for producing zinc coating on the surface of magnesium alloy: pat. СN107675163А; appl. 14.11.17; publ. 09.02.18.
  13. Method for producing magnesium alloy: pat. СN114214614А; appl. 16.12.21; publ. 22.03.22.
  14. Preparation of aluminum composition powders: pat. СN109252154А; appl. 14.07.17; publ. 22.01.19.
  15. Method for manufacturing modified aluminum powder for CGDS: pat. СN115055677А; appl. 17.08.22; publ. 01.11.22.
  16. Method for increasing corrosion resistance: pat. СN115537799А; appl. 07.11.22; publ. 30.12.22.
  17. Method for the preparation of a powder mixture for CGDS: pat. СN110616424А; appl. 30.08.19; publ. 27.12.19.
  18. Method for the production of Cu–Al2O3 powder compositions: pat. СN115283664A; appl. 13.07.22; publ. 04.11.22.
  19. Method for obtaining and applying a corrosion-resistant coating: pat. СN113832456А; appl. 07.09.21; publ. 24.12.21.
  20. Powder composition based on alloy 2024: pat. СN114318323А; appl. 10.12.21; publ. 12.04.22.
  21. Method of manufacturing and applying coatings from aluminum alloys of series 7075, 6061, etc.: pat. US11215769В2; appl. 17.02.20; publ. 04.01.22.
  22. Method for obtaining powder for CGDS with REE: pat. СN116237527А; appl. 13.03.23; publ. 09.06.23.
  23. Method of manufacturing and composition of aluminum-based powder: pat. СN115961182А; appl. 21.12.22; publ. 14.04.23.
  24. Method of spraying tin and aluminum powder onto a magnesium substrate: pat. JP2013029177A; appl. 29.07.11; publ. 07.02.13.
  25. Powder composition using polylactic acid, alloys of grades AZ91D, AZ61A, AZ81A (8% Al – 1% Zn), powder manufacturing method: pat. JP2019123536A; appl. 18.01.18; publ. 17.05.22.