Thermal stability of polyimide carbon plastics based on various carbon fillers
Nacharkina A.V., Zelenina I.V., Kurshev E.V., Lonskii S.L. Thermal stability of polyimide carbon plastics based on various carbon fillers // Proceedings of VIAM. 2025. No. 10. DOI: 10.18577/2307-6046-2025-0-10-106-122. URL: https://www.viam-works.ru/en/journal/2025/10/9
Keywords
polymer composite materials (PCM), polyimide carbon fiber, carbon fillers, thermal aging, thermo-oxidative degradation, microstructural studies
Abstract
The article presents the study results of the effect, which laboratory-simulated exposure to elevated temperatures from 280 to 350 °C has on the structure and properties of high-temperature carbon fiber plastics based on polyimide binders and carbon fillers from bundles from various manufacturers. The strength characteristics, i.e. bending and interlayer shear, density, glass transition temperature and mass loss of carbon plastics after exposure to elevated temperatures has been determined. Microstructural studies of the carbon fiber surface have been carried out and the microphase composition of the binder has been determined.
Reference list
- Kablov E.N., Antipov V.V. The role of new generation materials in ensuring the technological sovereignty of the Russian Federation. Vestnik Rossiyskoy akademii nauk, 2023, vol. 93, no. 10, pp. 907–916.
- Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), paper no. 10. Available at: http://www.journal.viam.ru (accessed: January 31, 2025). DOI: 10.18577/2713-0193-2023-0-2-122-144.
- Gunyaeva A.G., Kurnosov A.O., Slavin A.V. Experience in the use of polymer composite materials developed by NRC «Kurchatov Institute» – VIAM in engines for civil aircraft. Aviation materials and technologies, 2024, no. 4 (77), paper no. 06. Available at: http://www.journal.viam.ru (accessed: January 31, 2025). DOI: 10.18577/2713-0193-2024-0-4-82-94.
- Kablov E.N. New generation materials and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
- Novikov A.S., Karimbaev T.D. Working blades of high-bypass fans for advanced turbofan engines. Dvigatel, 2015, no. 5, pp. 6–11.
- Valueva M.I., Zelenina I.V., Nacharkina A.V., Sidorina A.I., Slavin A.V. High-temperature carbon fiber reinforced plastics based on polyimide binders. Trudy VIAM, 2024, no. 11 (141), paper no. 06. Available at: http://www.viam-works.ru (accessed: January 31, 2025). DOI: 10.18577/2307-6046-2024-0-11-71-88.
- Teijin developes hightly heat- and impact-resistant prepreg as carbon fiber intermediate material for aerospace applications. Available at: https://www.teijin.com/news/2019/20190304_3521.html (accessed: December 15, 2024).
- Global Polyimide Resins Market Study 2016–2032. Available at: https://www.marketresearch.com/Prismane-Consulting-Private-Limited-v4215/Global-Polyimide-Resins-Study-32057574/ (accessed: December 15, 2024).
- Global Polyimide Resin Matrix Composite Laminate SuPly, Demand and Key Producers, 2023–2029. Available at: https://www.marketresearch.com/GlobalInfoResearch-v4117/Global-Polyimide-Resin-Matrix-Composite-35273331/ (accessed: December 15, 2024).
- Mikhailin Yu.A. Heat, thermal and fire resistance of polymeric materials. St. Petersburg: Scientific foundations and technologies, 2011, 416 p.
- Kablov E.N., Startsev V.O. Measurement and forecasting of materials samples’ temperature during weathering in different climatic zones. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 47–58. DOI: 10.18577/2071-9140-2020-0-4-47-58.
- Liu Y., Xu X.-Z., Mo S. et al. Long-term Thermo-oxidative Degradation Modeling of a Carbon Fiber Reinforced Polyimide Composite: Multistep Degradation Behaviors and Kinetics. Chinese Journal of Polymer Science, 2020, no. 38, pp. 1202–1213. DOI: 10.1007/s10118-020-2425-7.
- Wang H., Wang Z., Kuang N. et al. Zhang Effect of high-temperature thermo-oxidation on the mechanical and electrical properties of phenylethynyl-terminated polyimide/carbon fiber composite. Polymer Degradation and Stability, 2023, vol. 218, p. 110544. DOI: 10.1016/j.polymdegradstab.2023.110544.
- Kubota Y., Furuta T., Aoki T. et al. Long-term thermal stability of carbon fibre-reinforced addition-type polyimide composite in terms of compressive strength. Advanced Composite Materials, 2018, vol. 28, pp. 1–19. DOI: 10.1080/09243046.2018.1446124.
- Govorov A.V., Galiguzov A.A., Tikhonov N.A. et al. Study of oxidation kinetics of carbon fibers of different types. Novye ogneupory, 2015, no. 11, p. 34.
- Back C.A. Effects of prior aging on the creep response of carbon fiber reinforced PMR-15 neat resin at 288 °C in an air environment: Thesis. Air Force Institute of Technology, 2007, 124 p.
- Sidorina A.I., Safronov A.M. Study of the resistance of carbon fibers to oxidation. Trudy VIAM, 2022, no. 7 (113), paper no. 06. Available at: http://www.viam-works.ru (accessed: January 31, 2025). DOI: 10.18577/2307-6046-2022-0-7-63-73.
- Tong Y., Wang X., Su H., Xu L. Oxidation kinetics of polyacrylonitrile-based carbon fibers in air and the effect on their tensile properties. Corrosion Science, 2011, vol. 53, pp. 2484–2488.
- Method for producing melt-blown polyimide binders of polymerization type: pat. 2666734 Rus. Federation; appl. 05.10.17; publ. 12.09.18.
- Valueva M.I., Zelenina I.V., Nacharkina A.V., Gulyaev A.I. Research of influence of thermal aging on properties high-temperature polyimide carbon fiber reinforced plastic. Trudy VIAM, 2023, no. 6 (124), paper no. 05. Available at: http://www.viam-works.ru (accessed: December 18, 2024). DOI: 10.18577/2307-6046-2023-0-6-46-62.
- Li X.С., Jin B.C., Tsotsis T.K., Nutt S. Thermo-oxidative aging and thermal cycling of PETI-340M composites. High Performance Polymers, 2022, vol. 34, pp. 33–43.
- MVK-10. RTM Polyimide. Product description. Available at: http://www.maverickcorp.com/_CE/pagecontent/Documents/MVK-10.pdf (accessed: December 20, 2024).
- Petkov V.I., Joffe R., Fernberg P. Thermal oxidative aging of satin weave and thin-ply polyimide composites. Polymer Composites, 2022, no. 43, pp. 2615–2627. DOI: 10.1002/pc.26561.
- Tandon G.P., Ragland W.R., Shoeppner G.A. Using Optical Microscopy to Monitor Anisotropic Oxidation Growth in High-Temperature Polymer Matrix Composites. Journal of Composite Materials, 2009, vol. 43, no. 5. Р. 583–603.
- Liu L., Du M., Liu F. Recent advances in interface microscopic characterization of carbon fiber-reinforced polymer composites. Frontiers in Materials, 2023, vol. 10, pp. 1–18.
- Ripberger E.R., Tandon G.P., Shoeppner G.A. Experimental techniques for characterizing thermo-oxidative behavior in high-temperature polyimide composite. Proceedings of the 2005 SEM Annual Conference and Exposition on Experimental and Applied Mechanics, 2005, pp. 1–9. Available at: https://www.researchgate.net/publication/267819653 (accessed: December 18, 2024).
- Kurshev E.V., Lonskiy S.L., Egorov Yu.A., Zelenina I.V. Study of changes in the microstructure and chemical composition of polyimide carbon fiber reinforced plastic after exposure to simulated operational factors. Voprosy materialovedeniya, 2024, no. 4, pp. 88–102.
- Deev I.S., Kurshev E.V., Lonskiy S.L. Effect of long-term climatic aging on the surface microstructure of epoxy carbon fiber reinforced plastics. Voprosy materialovedeniya, 2018, no. 3, pp. 157–169.