Peculiarities of the technology of production of aircraft engine parts from granules of heat-resistant nickel alloys by the method of plasma melting and centrifugal spraying of a cast rotating blank

Vostrikov A.V., Yashin M.S., Kapitanenko D.V.
Vostrikov A.V., Yashin M.S., Kapitanenko D.V. Peculiarities of the technology of production of aircraft engine parts from granules of heat-resistant nickel alloys by the method of plasma melting and centrifugal spraying of a cast rotating blank // Proceedings of VIAM. 2025. No. 10. DOI: 10.18577/2307-6046-2025-0-10-16-26. URL: https://www.viam-works.ru/en/journal/2025/10/2
Keywords
granules, heat-resistant nickel alloys, pressure treatment, hot isostatic pressing, gas turbine engines, granule metallurgy, plasma melting
Abstract

The review analyzes the current state of production of HNA (Heat-resistant nickel alloy) granules by the method of plasma melting and centrifugal spraying of a cast rotating blank (PREP method). The main theoretical and practical features of the production of HNA granules by this method are shown. Based on the analysis of a number of works in a similar direction, the corresponding calculations are made, allowing to form a list of requirements for the production of granules using the method of plasma melting and centrifugal spraying of a cast rotating blank.

Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Aerospace Materials Science. Vse materialy. Entsiklopedicheskiy spravochnik, 2008, no. 3, pp. 2–14.
  3. Kablov E.N. Materials Quality Control – a Guarantee of Aviation Equipment Operation Safety. Aviacionnye materialy i tehnologii, 2001, no. 1, pp. 3–8.
  4. Kablov E.N. Science as a Branch of the Economy. Nauka i zhizn, 2009, no. 10, pp. 7–8.
  5. Letnikov M.N., Lomberg B.S., Ospennikova O.G., Bakradze M.M. The influence of quench rate on microstructure and mechanical properties of nickel-based wrought superalloy VZh175-ID. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 21–30. DOI: 10.18577/2071-9140-2019-0-2-21-30.
  6. Lomberg B.S., Shestakova A.A., Bakradze M.M., Karachevtsev F.N. The investigation of the stability of γ-phase with size below 100 nm in Ni-base superalloy VZh175-ID. Aviacionnye materialy i tehnologii, 2018, no. 4 (53), pp. 3–10. DOI: 10.18577/2071-9140-2018-0-4-3-10.
  7. Echin A.B., Bondarenko Yu.A., Kolodyazhny M.Yu., Surova V.A. Review of perspective high-temperature superalloys based on refractory non-metallic materials for production of gas turbine engines. Aviation materials and technologies, 2023, no. 3 (72), paper no. 03. Available at: http://www.journal.viam.ru (accessed: December 10, 2024). DOI: 10.18577/2713-0193-2023-0-3-30-41.
  8. Min P.G., Vadeev V.E. The development and introduction into serial production of the new superalloy VZhL125 for the advanced aviation engines vanes. Aviation materials and technologies, 2023, no. 1 (70), paper no. 01. Available at: http://www.journal.viam.ru (accessed: December 10, 2024). DOI: 10.18577/2713-0193-2023-0-1-3-16.
  9. Narsky A.R., Deynega G.I., Kuzmina I.G. Obtaining a fine-grained structure of castings from nickel superalloys using a cobalt aluminate modifier. Aviation materials and technologies, 2023, no. 3 (72), paper no. 01. Available at: http://www.journal.viam.ru (accessed: December 10, 2024). DOI: 10.18577/2713-0193-2023-0-3-3-14.
  10. Kolyadov E.V., Visik E.M., Gerasimov V.V., Bityutskaya O.N. Features of the morphology of the structure of nickel superalloy depending on the values of the axial and radial temperature gradients at the crystallization front. Aviation materials and technologies, 2024, no. 2 (75), paper no. 02. Available at: http://www.journal.viam.ru (accessed: December 10, 2024). DOI: 10.18577/2713-0193-2024-0-2-15-24.
  11. Vostrikov A.V., Volkov A.M., Bakradze M.M. Development and study of a new granulated disk alloy VZh178P for promising aircraft gas turbine engines. Tsvetnye metally, 2018, no. 8, pp. 80–84.
  12. Eskin G.I. On the conditions for the formation of a non-dendritic structure in ingots and granules of light and heat-resistant nickel alloys. Tekhnologiya legkikh splavov, 2013, no. 4, pp. 147–159.
  13. Garibov G.S., Grits N.M. V.I. Dobatkin and metallurgy of granules of heat-resistant nickel alloys. Tekhnologiya legkikh splavov, 2015, no. 2, pp. 34–39.
  14. Vostrikov A.V., Sukhov D.I. The production of powders by PREP method for addictive manufacturing – current situation and development prospects. Trudy VIAM, 2016, no. 8, paper no. 3. Available at: http://www.viam-works.ru (accessed: December 10, 2024). DOI: 10.18577/2307-6046-2016-0-8-3-3.
  15. Method for producing granules of heat-resistant nickel alloys: pat. 2468891 С1 Rus. Federation; appl. 18.11.11; publ. 10.12.12.
  16. Volkov A.M., Shestakova A.A., Bakradze M.M. The comparison of powder produced by gas atomization and by plasma rotate electrode process in the point of production disk billets from Ni-base superalloys. Trudy VIAM, 2018, no. 11 (71), paper no. 02. Available at: http://www.viam-works.ru (accessed: December 10, 2024). DOI: 10.18577/2307-6046-2018-0-11-12-19.
  17. Vostrikov A.V., Garibov G.S., Ber L.B., Shlyapin S.D. Study of physical and mechanical properties and structure of granules from a new high-strength nickel alloy produced by the PREP method. Tekhnologiya legkikh splavov, 2013, no. 2, pp. 69–75.
  18. Musienko V.T. Some results of the development of the technology for the production of granules of heat-resistant nickel alloys for the manufacture of aerospace products. Tekhnologiya legkikh splavov, 2000, no. 6, pp. 72–78.
  19. Dobatkin V.I. The role of kinetic and thermodynamic factors in the crystallization of granules. Metallurgiya granul, 1983, is. 1, pp. 23–33.
  20. Dobatkin V.I. Regularities of rapid crystallization as a basis for selecting the compositions of granulated alloys. Metallurgiya granul, 1988, is. 4, pp. 11–23.
  21. Garibov G.S. Crystallization theory and technology of granulated heat-resistant nickel alloys. Tekhnologiya legkikh splavov, 2016, no. 1, pp. 107–118.
  22. Belov A.F., Anoshkin N.F., Fatkullin O.Kh. et al. Features of alloying heat-resistant alloys obtained by granule metallurgy. Heat-resistant and heat-resistant steels and nickel-based alloys. Moscow: Nauka, 1984, pp. 31–40.
  23. Bakradze М.М., Volkov А.М., Shestakova А.А., Letnikov M.N., Bubnov M.V. The features of the grains size changing in the p/m Ni-base superalloy for disks application produced via different technologies. Trudy VIAM, 2018, no. 2 (62), paper no. 01. Available at: http://www.viam-works.ru (accessed: December 10, 2024). DOI: 10.18577/2307-6046-2018-0-2-1-1.
  24. Garibov G.S. Development of the ideas of academician A.F. Belov on a radical increase in the operational characteristics of promising gas turbine engine disks. Promising technologies of light and special alloys: on the 100th anniversary of the birth of academician A.F. Belov. Moscow: Fizmatlit, 2006, pp. 107–117.
  25. Koshelev V.Ya., Garibov G.S., Sukhov D.I. Basic patterns of the process of producing heat-resistant alloy granules by plasma spraying of a rotating workpiece. Tekhnologiya legkikh splavov, 2015, no. 3, pp. 97–103.
  26. Koshelev V.Ya., Egorov D.A. Influence of storage atmosphere on the adsorption capacity of heat-resistant nickel alloy granules. Tekhnologiya legkikh splavov, 2010, no. 4, pp. 41–45.
  27. Shestakov A.V., Karashaev M.M., Dmitriev N.S. Technological ways to create composite materials based on heat-resistant refractory compounds (review). Trudy VIAM, 2021, no. 8 (102), paper no. 03. Available at: http://www.viam-works.ru (accessed: December 10, 2024). DOI: 10.18577/2307-6046-2021-0-8-12-20.
  28. Volkov A.M., Vostrikov A.V. Low-cycle fatigue resistance of PM Ni-base superalloys (review). Aviacionnye materialy i tehnologii, 2016, no. S1, pp. 74–79. DOI: 10.18577/2071-9140-2016-0-S1-74-79.