Fluorine-containing polymers for protective and decorative coatings for industrial use
UDC
669.715:669.018.62
DOI
10.18577/2307-6046-2025-0-10-123-132
Article PDF (Russian)
(610.34 KB)
How to cite
Serdcelyubova A.S., Oshmarina T.Ya., Zverevich Yu.K. Fluorine-containing polymers for protective and decorative coatings for industrial use // Proceedings of VIAM. 2025. No. 10. DOI: 10.18577/2307-6046-2025-0-10-123-132. URL: https://www.viam-works.ru/en/journal/2025/10/10
Keywords
protective coatings, fluoropolymers, aviation coatings, film-forming systems, high molecular weight compounds, paint and varnishes
Abstract
The article considers fluorine-containing polymer film-forming agents used in protective coatings and other industrial sectors. The paper provides the results of an analysis of the fluoropolymer market in Russia and abroad, as well as an assessment of the development of these polymers in our country. The features of the chemical structure of fluorine-containing copolymers and their modifications are described. The main advantages of fluorinated film-forming agents and the areas of their application are identified.
Reference list
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Buznik V.M., Kablov E.N. State and Prospects of Arctic Materials Science. Herald of the Russian Academy of Sciences, 2017, vol. 87, no. 9, pp. 827–839.
- Kablov E.N. Modern Materials – the Basis for Innovative Modernization of Russia. Metally Evrazii, 2012, no. 3, pp. 10–15.
- Kablov E.N., Semenova L.V., Eskov A.A., Lebedeva T.A. Complex Systems of Paint and Varnish Coatings for the Protection of Metal Polymer Composite Materials, as Well as Their Contact Joints from the Impact of Aggressive Factors. Lakokrasochnye materialy i ikh primenenie, 2016, no. 6, pp. 32–35.
- Abramova M.G., Lutsenko A.N., Varchenko E.A. Concerning the aspects of validation of climate resistance of airborne materials at all life cycle stages (review). Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 86–94. DOI: 10.18577/2071-9140-2020-0-1-86-94.
- Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), paper no. 10. Available at: http://www.journal.viam.ru (accessed: January 14, 2025). DOI: 10.18577/2713-0193-2023-0-2-122-144.
- Kuznetsova V.A., Marchenko S.A., Emelyanov V.V., Zheleznyak V.G. Study of the influence of molecular mass of epoxy oligomers and hardeners on the operational properties of paint coatings. Aviation materials and technology, 2021, no. 1 (62), paper no. 07. Available at: http://www.journal.viam.ru (accessed: December 17, 2024). DOI: 10.18577/2071-9140-2021-0-1-71-79.
- Kozlova A.A., Kondrateva O.V., Kuznetsova V.A. The main problems of using domestically produced moisture-proof electrical insulating materials for automated selective application on printed assemblies (review). Aviation materials and technologies, 2022, no. 4 (69), paper no. 07. Available at: http://www.journal.viam.ru (accessed: January 20, 2025). DOI: 10.18577/2713-0193-2022-0-4-72-83.
- Serdtselyubova A.S., Krechetov D.D. Ways to improve the weather resistance of paints and varnishes used for painting the outer surface of aviation equipment. Lakokrasochnye materialy i ikh primenenie, 2021, no. 9, pp. 31–38.
- Drinberg A.S. Painting of composite materials. Lakokrasochnye materialy i ikh primenenie, 2017, no. 3, pp. 22–31.
- Nikalin D.M., Merkulova Yu.I., Zheleznyak V.G. Fluorine-containing polymer paints and varnishes in aviation equipment. Review. Rossiyskiy khimicheskiy zhurnal, 2019, vol. LXIII, no. 1, pp. 86–93.
- Drinberg A.S., Kozlova S.P., Karpov V.A. Protective coatings based on fluorinated polymers. Khimicheskaya promyshlennost, 2019, no. 4, pp. 185–192.
- Drinberg A.S., Karpov V.A., Okhrimenko A.G. Protective coatings based on fluorinated polymers. Lakokrasochnye materialy i ikh primenenie, 2017, no. 7–8, pp. 39–43.
- Drinberg A.A., Babkin O.E., Drinberg A.S. et al. Promising areas of research and development in the technology of creating new antifouling materials. Lakokrasochnye materialy i ikh primenenie, 2022, no. 12, pp. 18–23.
- Drinberg A.S., Babkin O.E., Litosov G.E. et al. Development of technology for the production of antifriction chemically resistant fluororethane coatings for equipment of underwater hydrocarbon production systems. Lakokrasochnye materialy i ikh primenenie, 2023, no. 3 (552), pp. 22–28.
- Buznik V.M. The state of domestic chemistry of fluoropolymers and possible development prospects. Rossiyskiy khimicheskiy zhurnal, 2008, vol. LII, no. 3, pp. 7–12.
- Buznik V.M. Modern Materials Science Using Fluoropolymers as an Example. Tomsk: TSU, 2012, is. 1, 42 p. (Academic Readings at Tomsk State University).
- Ignatyeva L.N., Buznik V.M. Quantum-Chemical Calculations of Spectroscopic and Topological Parameters of Fluorocarbon Oligomers. Zhurnal fizicheskoy khimii, 2005, vol. 79, no. 9, pp. 1631−1638.
- Loginov B.A., Willemson A.L., Buznik V.M. Russian Fluoropolymers: History, Technologies, Prospects. Moscow, 2013, 320 p.
- Usmanov Kh.U., Yulchibaev A.A. Vinyl Fluoride and Its Polymers. Moscow: Khimiya, 1978, 227 p.
- Panshin Yu.A., Malkevich S.G., Dunaevskaya Ts.S. Fluoroplastics. Leningrad: Khimiya, 1978, 232 p.
- Bader E.Ya., Donskoy A.A., Zhelezina G.F. et al. Experience in the use of fluoropolymer materials in aviation technology. Rossiyskiy khimicheskiy zhurnal, 2008, vol. LII, no. 3. pp. 30–44.
- Ignatieva L.N., Buznik V.M. Quantum chemical calculation of IR absorption spectra of modified forms of polytetrafluoroethylene. Zhurnal fizicheskoy khimii, 2006, vol. 80, no. 12, pp. 2178−2187.
- Huang X., Tepylo N., Pommier-Budinger V. et al. A survey of acephobic coatings and their potential use in a hybrid coating/active ice protection system for aerospace applications. Progress in Aerospace Sciences, 2019, vol. 105, pp. 74–97.
- Fluorine-containing polymers: catalogue. Cherkassy: ONIITEKHIM, 1985, 20 p.
- Glazer E.A., Mulin Yu.A. Achievements in production, processing and application of powder polymeric materials. Ed. A.D. Yakovlev. Leningrad: LDNTP, 1980, 88 p.
- Wrigth T. Clear skies ahead or more turbulence. Coating World, 2009, no. 8, pp. 26–28.
- Rytikov G.O., Doronin F.A., Evdokimov A.G. et al. The effect of the surface morphological inhomogeneitieson the polymer films mycological resistance. Protection of metals and physical chemistry of surfaces, 2021, vol. 57, pp. 329–338. DOI: 10.1134/S2070205121020088.
- Hydrophobic polymer coating: pat. RU 2676644 C1 Rus. Federation; appl. 11.04.18; publ. 09.01.19.
- Fluoropolymers. Ed. L. Wall; trans. from Engl. Moscow: Khimiya, 1975, 450 p.