Structure and properties of high-nitrogen corrosion-resistant bearing steel samples obtained by selective laser melting
UDC
669.15:621.9.048.7
DOI
10.18577/2307-6046-2025-0-10-3-15
Article PDF (Russian)
(1.02 MB)
How to cite
Sevalnev G.S., Druzhnov M.A., Leonov A.V., Novikov A.S., Lavrik E.G. Structure and properties of high-nitrogen corrosion-resistant bearing steel samples obtained by selective laser melting // Proceedings of VIAM. 2025. No. 10. DOI: 10.18577/2307-6046-2025-0-10-3-15. URL: https://www.viam-works.ru/en/journal/2025/10/1
Keywords
bearing steel, high nitrogen steel, additive technologies, selective laser melting, microstructure, mechanical and tribotechnical properties
Abstract
Change in nitrogen concentration, formation of the structure and properties of the metal-powder composition and 3D-printed samples of high-nitrogen corrosion-resistant bearing steel was studied. It is established that providing a super-equilibrium nitrogen concentration in the chemical composition of steel is possible both at the stage of obtaining an ingot and during the production of a metal-powder composition and 3D-printing of samples. The formed segregations of carbonitrides in the obtained samples contribute to a decrease in mechanical and tribotechnical characteristics.
Reference list
- Sevalnev G.S. Beryllium-containing steels – perspective material with a high level of physical and mechanical properties. Aviation materials and technologies, 2023, no. 3 (72), paper no. 02. Available at: http://www.journal.viam.ru (accessed: October 24, 2024). DOI: 10.18577/2713-0193-2023-0-3-15-29.
- Kablov E.N., Bakradze M.M., Gromov V.I., Voznesenskaya N.M., Yakusheva N.A. New high strength structural and corrosion-resistant steels for aerospace equipment developed by FSUE «VIAM» (review). Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 3–11. DOI: 10.18577/2071-9140-2020-0-1-3-11.
- Korobova E.N., Sevalnev G.S., Gromov V.I., Leonov A.V. Steels for the manufacture of roller bearings for special purposes (review). Trudy VIAM, 2021, no. 11 (105), paper no. 01. Available at: http://www.viam-works.ru (accessed: October 24, 2024). DOI: 10.18577/2307-6046-2021-0-11-3-11.
- Spektor A.G., Zelbet B.M., Kiseleva S.A. Structure and properties bearing staly. Мoscow: Metallurgist, 1980, 264 p.
- Sprishevsky A.I. Swing bearings. Мoscow: Mashinostroenie, 1968, 632 p.
- Pinegin S.V. Swing support in machines. Мoscow: Academy of Sciences of the USSR, 1961, 150 p.
- Degtyarev S.A., Leontev M.K., Popov V.V. To pliability definition «squirrel wheel» in support of rotors of aviation gasturbine engines. The messenger of the Samara state space university of academician S.P. Koroleva (national research university), 2014, no. 4 (46), pp. 52–60.
- Belousov A.I., Balyakin V.B., Novikov D.K. Theory and design of hydrodynamic dampers of support of rotors. Samara, 2002, 335 p.
- Heat-resistant bearing steel: pat. 2447183 Rus. Federation; appl. 05.04.11; publ. 10.04.12.
- High-strength corrosion-resistant steel: pat. 2724766 Rus. Federation; appl. 23.05.19; publ. 25.06.20.
- Rabitsch R., Koch F., Würzinger P. M50 (AMS 6191) and M50NiL (AMS 6278) High-Performance VIM-VAR Melted Bearing Steels for the Aviation Industry. Proceedings of the 2005 International Symposium on Liquid Metal Processing and Casting. Sata Fe (New Mexico): ASTM International, 2005, vol. 5, pp. 57–64.
- Ooi S., Bhadeshia H.K.D.H. Duplex Hardening of steels for Aeroengine Bearings. ISIJ International, 2012, vol. 52, no. 11, pp. 1927–1934.
- Bakradze M.M., Voznesenskaya N.M., Leonov A.V., Krylov S.A., Tonysheva S.A. Development and research of high-strength corrosion-resistant steel for details of bearings. Metallurgist, 2019, no. 11, pp. 39–44.
- Cronidur 30 Stainless Steel. Available at: https://www.progressivealloy.com/cronidur-30-stainless-steel (accessed: October 24, 2024).
- Trojahn W., Streit E., Chin H.A., Ehlert D. Progress in bearing performance of advanced nitrogen alloys stainless steel, Cronidur 30. Materialwissenschaft und Werkstofftechnik, 1999, vol. 30, pp. 605–611.
- Berns H., Ebert F.-J., Zoch H.-W. The new low nitrogen steel LNS – a material for advanced aircraft engine and aerospace bearing applications. Bearing steels: into the 21-st century. Eds. J.J.C Hoo, W.B. Green. American Society for Testing Material, 1998, 440 р.
- Svyazhin A.G., Kaputkina L.M. Nitrogenous and high-nitrogen became. Industrial technologies and properties. Izvestiya. Ferrous Metallurgy, 2019, no. 62 (3), pp. 173–187. DOI: 10.17073/0368-0797-2019-3-173-187.
- Svyazhin A.G., Kaputkina L.M. The steels, alloyed by nitrogen. Izvestiya. Ferrous Metallurgy, 2005, no. 10, pp. 36–46.
- Rashev Ts.V. High nitrogen steels. Metallurgy under pressure. Sofia: prof. Marin Drinov, 1995, 272 p.
- Berns H., Escher C., Streich W.D. Martensitic high nitrogen steel for applications at elevated temperature. Materials science forum. Trans. Tech. Publications Ltd, 1999, vol. 318, pp. 443–448.
- Lukin E.I., Ashmarin A.A., Bannykh I.O. et al. Effect of the Reduction during Cold Rolling on the Phase Composition, Texture, and Residual Stresses in 20Kh15AN3MD2 Steel. Russian Metallurgy (Metally), 2023, vol. 2023, no. 11, pp. 1598–1605.
- Berns H., Ehrhardt R. Carbon or nitrogen alloyed quenched and tempered stainless steel – comparative study. Steel research, 1996, vol. 67, no. 8, pp. 343–349.
- Liverani E., Toschi S., Ceschini L., Fortunato A. Effect of selective laser melting (SLM) process parameters on microstructure and mechanical properties of 316L austenitic stainless steel. Journal of Materials Processing Technology, 2017, vol. 249, pp. 255–263.
- Bogachev I.A., Sulyanova E.A., Sukhov D.I., Mazalov P.B. Microstructure and properties investigations of Fe–Cr–Ni stainless steel obtained by selective laser melting. Trudy VIAM, 2019, no. 3 (75), paper no. 01. Available at: http://www.viam-works.ru (accessed: November 01, 2024). DOI: 10.18577/2307-6046-2019-0-3-3-13.
- Yap C.Y., Chua C.K., Dong Z.L. et al. Review of selective laser melting: Materials and applications. Applied physics reviews, 2015, vol. 2, no. 4, p. 041101.
- Pei Y.T., de Hosson J.T.M. Functionally graded materials produced by laser cladding. Acta Materialia, 2000, vol. 48, pp. 2617−2624.
- Gavriljuk V.G., Berns H. High nitrogen steels: structure, properties, manufacture, applications. Springer Science & Business Media, 1999, 364 p.
- Siwka J., Hutny A. An universal formula for the calculation of nitrogen solubility in liquid nitrogen-alloyed steels. Metalurgija, 2009, vol. 48, no. 1, pp. 23–27.
- Sevalnev G.S., Nefedkin D.Yu., Dulnev K.V., Skorikova M.A. Study of the characteristics of maraging steel under tribotechnical loading. Trudy VIAM, 2024, no. 10 (140), paper no. 01. Available at: http://www.viam-works.ru (accessed: November 22, 2024). DOI: 10.18577/2307-6046-2024-0-10-3-12.