Forecasting modes of molding prepregs for aircraft products

Antyufeeva N.V., Bolshakov V.A.
Antyufeeva N.V., Bolshakov V.A. Forecasting modes of molding prepregs for aircraft products // Proceedings of VIAM. 2025. No. 1. DOI: 10.18577/2307-6046-2025-0-1-100-108. URL: https://www.viam-works.ru/en/journal/2025/1/9
Keywords
adhesive binder, prepreg, curing, thermal analysis, kinetic parameters, kinetics of curing
Abstract

The kinetics of curing binder in prepreg was studied by differential scanning calorimetry method. The most adequate scheme of the curing reaction was selected and the kinetic parameters of the curing reaction for each elementary stage of the process were determined. On the basis of experimental data, generalized kinetic models of the curing reaction were constructed, and then the curing modes of the binder in the prepreg were selected were selected based on both experimental and calculated data, which were tested on technological equipment. As a result, the degree of material curing was determined.

Reference list
  1. Kablov E.N., Valueva M.I., Zelenina I.V., Khmelnitskiy V.V., Aleksashin V.M. Carbon plastics based on benzoxazine oligomers – perspective materials. Trudy VIAM, 2020, no. 1, paper no. 07. Available at: http://www.viam-works.ru (accessed: May 22, 2024). DOI: 10.18577/2307-6046-2020-0-1-68-77.
  2. Kablov E.N., Kulagina G.S., Zhelezina G.F., Lonskii S.L., Kurshev E.V. Microstructure research of the unidirectional organoplastic based on Rusar-NT aramid fibers and epoxy-polysulfone binder. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 19–26. DOI: 10.18577/2071-9140-2020-0-4-19-26.
  3. Kablov E.N. New generation materials and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334. DOI: 10.31857/S0869587320040052.
  4. Kablov E.N., Shuldeshov E.M., Petrova A.P., Lapteva M.A., Sorokin A.E. Dependence of complex of sound-proof VZMK type material properties on concentration of hydrophobizing composition on the basis of organosilicon sealant. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 41–49. DOI: 10.18577/2071-9140-2020-0-2-41-49.
  5. Postnov V.I., Kachura S.M., Veshkin E.A. Modeling of the curing process of a polymer resin and changes in microhardness in its volume. Aviation materials and technologies, 2021, no. 4 (65), paper no. 07. Available at: http://www.journal.viam.ru (accessed: March 19, 2024). DOI: 10.18577/2307-6046-2021-0-4-92-99.
  6. Postnov V.I., Veshkin E.A., Makrushin K.V., Sudin Yu.I. Technological features of manufacturing polymer composite materials of main rotor blades for a light helicopter. Aviation materials and technologies, 2023, no. 1 (70), paper no. 06. Available at: http://www.journal.viam.ru (accessed: July 17, 2024). DOI: 10.18577/2713-0193-2023-0-1-82-92.
  7. Khaskov M.A., Melnikov D.A., Kotova E.V. Selection of temperature-time modes of curing epoxy binders taking into account the scale factor. Klei. Germetiki. Tekhnologii, 2017, no. 10, pp. 24–32.
  8. Malysheva G.V., Marakhovskiy P.S., Barinov D.Ya., Nikolaev E.V. Optimization of the curing modes of fiber-glass based on epoxy binder. Aviation materials and technologies, 2023, no. 2 (71), paper no. 08. Available at: http://www.journal.viam.ru (accessed: April 15, 2024). DOI: 10.18577/2713-0193-2023-0-2-94-103.
  9. Shershak P.V., Sutubalov A.I., Yakovlev N.O., Sherstyuk F.A. Standards test methods for polymer matrix composite materials. Part 2. Compression properties. Aviation materials and technologies, 2024, no. 2 (75), paper no. 12. Available at: http://www.journal.viam.ru (accessed: October 28, 2024). DOI: 10.18577/2713-0193-2024-0-2-149-166.
  10. Khaskov M.A. Expansion of the temperature-time-transformation diagram taking into account the thermophysical properties of the components for optimizing the curing modes of polymer composite materials. Zhurnal prikladnoy khimii, 2016, no. 4, pp. 510–518.
  11. Kutsevich K.E., Aleksashin V.M., Petrova A.P., Antyufeeva N.V. Study of the kinetics of curing reactions of adhesive binders. Klei. Germetiki. Tekhnologii, 2014, no. 11, pp. 27–31.
  12. Antyufeeva N.V., Starkov A.I. Influence of the content of halogen-containing oligomer in the composition of the adhesive binder VSK-14-6 on the kinetics of the curing process of prepregs on different fillers and a comparative analysis of the kinetics of curing of prepregs based on the adhesive binder VSK-14-1. Klei. Germetiki. Tekhnologii, 2022, no. 5, pp. 12–19.
  13. Zhelezina G.F., Voynov S.I., Karimbaev T.D., Chernyshev A.A. Aramid organoplastics for aircraft engine fan housings. Voprosy materialovedeniya, 2017, no. 32 (90), pp. 153–165.
  14. Grenier-Loustalot M.F., Bente M.P., Grenier Ph. Reactivite du dicyandiamide vis a vis des groupements et N-epoxide-1. Mechanism reactionnel. European Polymer Journal, 1991, vol. 27, no. 11, pp. 1201–1216.
  15. Sharova I.A., Lukina N.F., Aleksashin V.M., Antuyfeeva N.V. Effect of modification with rubber on properties and process of curing of epoxy-rubber adhesives compositions. Polymer Science. Series D, 2016, vol. 9, no. 4, pp. 437–440.