Analysis of the chemical composition of intermetallic titanium ortho-alloys by inductively coupled plasma atomic emission spectrometry

Part 2
Dvoretskov R.M., Alexeev E.B., Karachevtsev F.N., Burkovskaya N.P.
Dvoretskov R.M., Alexeev E.B., Karachevtsev F.N., Burkovskaya N.P. Analysis of the chemical composition of intermetallic titanium ortho-alloys by inductively coupled plasma atomic emission spectrometry. Part 2 // Proceedings of VIAM. 2025. No. 1. DOI: 10.18577/2307-6046-2025-0-1-74-86. URL: https://www.viam-works.ru/en/journal/2025/1/7
Keywords
analytical control, chemical analysis, titanium alloys, titanium intermetallics, ortho-alloys, atomic emission spectrometry, inductively coupled plasma
Abstract

A method for determining impurity elements Cr, Cu, Fe, Mn, Ni, Sn and Si microadditives in titanium ortho-alloys using inductively coupled plasma atomic emission spectrometry is proposed. Analytical lines of elements free from significant spectral overlaps are selected. The limits of detection and determination of elements are assessed. The metrological characteristics of the technique are assessed using model solutions. The correctness of the developed methodology with the use of model solutions are assessed using certified reference materials.

Reference list
  1. Dvoretskov R.M., Alekseev E.B., Karachevtsev F.N., Zagvozdkina T.N. Analysis of the chemical composition of intermetallic titanium ortho-alloys by inductively coupled plasma atomic emission spectrometry. Part 1. Trudy VIAM, 2023, no. 6 (124), paper no. 10. Available at: http://www.viam-works.ru (accessed: May 20, 2024). DOI: 10.18577/2307-6046-2023-0-6-115-129.
  2. Antashev V.G., Nochovnaya N.A., Padyukova N.M., Pavlova T.V. Analysis of the need of science and technology for high-resource heat-resistant titanium alloys and erosion heat-resistant coatings. Aviacionnye materialy i technologii, 2002, no. 2, pp. 32–45.
  3. Antipov V.V. Prospects for development of aluminium, magnesium and titanium alloys for aerospace engineering. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 186–194. DOI: 10.18577/2071-9140-2017-0-S-186-194.
  4. Kablov E.N. Materials and chemical technologies for aviation equipment. Vestnik Rossiyskoy akademii nauk, 2012, vol. 82, no. 6, pp. 520–530.
  5. Makushina M.A., Kochetkov A.S., Nochovnaya N.A. Cast titanium alloys for aviation equipment (review). Trudy VIAM, 2021, no. 7 (101), paper no. 05. Available at: http://www.viam-works.ru (accessed: June 10, 2024). DOI: 10.18577/2307-6046-2021-0-7-39-47.
  6. Kolobov Yu.R., Kablov E.N., Kozlov E.V., Koneva N.A. et al. Structure and properties of intermetallic materials with nanophase strengthening. Moscow: MISIS, 2008, 328 p.
  7. Nochovnaya N.A., Bazyleva O.A., Kablov D.E., Panin P.V. Intermetallic alloys based on titanium and nickel. Ed. E.N. Kablov. Moscow: VIAM, 2018, 308 p.
  8. Dzunovich D.A., Alekseyev E.B., Panin P.V., Lukina E.A., Novak A.V. Structure and properties of sheet semi-finished products from various wrought intermetallic titanium alloys. Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 17–25. DOI: 10.18577/2071-9140-2018-0-2-17-25.
  9. Alekseev I.E., Pilipenko A.A., Varfolomeev M.S. Possibility of replacing nickel heat-resistant alloys with alloys based on the intermetallic compound Ti-Al. Rapidly quenched materials and coatings: proc. XIX Int. sci.-tech. conf. Moscow, 2022, pp. 311–315.
  10. Skvortsova S.V., Umarova O.Z., Anishchuk D.S., Smirnov V.G. Formation of the structure, phase composition and mechanical properties of an alloy based on titanium aluminide Ti2AlNb during heat treatment. Titan, 2015, no. 3 (49), pp. 29–33.
  11. Polkin I.S., Egorova Yu.B., Davydenko L.V. Alloying, phase composition and mechanical properties of titanium alloys. Tekhnologiya legkikh splavov, 2022, no. 2, pp. 4–13.
  12. Novak A.V. Regularities of the influence of microadditives of rare earth elements on the structural-phase state and mechanical characteristics of an intermetallic alloy based on orthorhombic titanium aluminide: thesis, Cand. Sc. (Tech.). Moscow, 2019, 128 p.
  13. Kablov E.N., Kashapov O.S., Medvedev P.N., Pavlova T.V. Study of a α + β-titanium alloy based on a system of Ti–Al–Sn–Zr–Si–β-stabilizing alloying elements. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 30–37. DOI: 10.18577/2071-9140-2020-0-1-30-37.
  14. Borisova E.A., Bochvar G.A., Brun M.Ya. et al. Titanium alloys. Metallography of titanium alloys. Moscow: Metallurgiya, 1980, 464 p.
  15. Nochovnaya N.A., Panin P.V., Alekseev E.B., Novak A.V. Regularities of formation of structural-phase state of alloys based on titanium ortho- and gamma-aluminides during thermomechanical treatment. Vestnik RFFI, 2015, no. 1, pp. 18–26.
  16. Podkopalov I.A. Review of alloys based on titanium intermetallic compounds. Mavlyutov readings: materials of the XV All-Russian youth scientific conf.: in 7 vols. Ufa, 2021, vol. 2, pp. 311–315.
  17. Abraimov N.V., Petukhov I.G., Zarypov M.S., Lukina V.V. On the issue of heat resistance of titanium alloys operating at temperatures above 650 °C. Electrometallurgiya, 2021, no. 12, pp. 10–20.
  18. Skvortsova S.V., Umarova O.Z., Agarkova E.O., Chernyshova A.A. Effect of heat treatment on the structure and mechanical properties of an intermetallic alloy plate VTI-4. Titan, 2015, no. 4 (50), pp. 17–21.
  19. Duyunova V.A., Oglodkov M.S., Putyrskiy S.V., Kochetkov A.S., Zueva O.V. Modern technologies for melting titanium alloy ingots (review). Aviation materials and technologies, 2022, no. 1 (66), paper no. 03. Available at: http://www.journal.viam.ru (accessed: May 27, 2024). DOI: 10.18577/2713-0193-2022-0-1-30-40.
  20. Shubin I.Yu., Nikitin Ya.Yu., Puchkov Yu.A., Alekseev E.B., Davydova E.A. Study of resistance to high-temperature gas and salt corrosion of heat-resistant intermetallic titanium alloy VTI-4. Vestnik Moskovskogo gosudarstvennogo tekhnicheskogo universiteta im. N.E. Baumana. Ser.: Mashinostroyenie, 2020, no. 6 (135), pp. 83–105.
  21. Baranovskaya V.B., Medvedevskikh M.Yu., Karpov Yu.A. Actual problems of the quality of chemical analysis. Analitika i kontrol, 2021, vol. 25, no. 4, pp. 273–279.
  22. Karpov Yu.A., Baranovskaya V.B. Analytical control is an integral part of materials diagnostics. Zavodskaya laboratoriya. Diagnostika materialov, 2017, vol. 83, no. 1-I, pp. 5–12.
  23. Nadezhdina M.E. Digitalization – global trends and main challenges. Reports «Modern digital technologies: problems, solutions, prospects». Kazan, 2022, pp. 40–43.
  24. Nadezhdina M.E., Shinkevich A.I. End-to-end digital technology of big data as the basis of digital transformation of the enterprise production system. Current trends in the digital transformation of industrial enterprises: Reports All-Rus. scientific and practical conf. Kursk, 2022, pp. 201–204.
  25. Vasipov V.V., Evsyukov A.I. Social networks as a tool for popularizing chemical science. XX Mendeleev Congress on General and Applied Chemistry: reports: in 5 vols. Ekaterinburg: Ural Branch of the Russian Academy of Sciences, 2016, vol. 5, p. 79.
  26. Otto M. Modern methods of analytical chemistry: in 2 vols. Moscow: Tekhnosfera, 2003, vol. I, 416 p.
  27. Karpov Yu.A., Baranovskaya V.B. The role and possibilities of analytical control in metallurgy. Tsvetnye metally, 2016, no. 8 (884), pp. 63–67. DOI: 10.17580/tsm.2016.08.09.
  28. Vyacheslavov A.V., Malinkina Yu.Yu., Bichaev V.B. et al. Analysis of corrosion-resistant titanium alloys alloyed with ruthenium by inductively coupled plasma atomic emission spectrometry. Zavodskaya laboratoriya. Diagnostika materialov, 2018, vol. 84, no. 5, pp. 14–19.
  29. Karpov Yu.A., Baranovskaya V.B. Problems of standardization of chemical analysis methods in metallurgy. Zavodskaya laboratoriya. Diagnostika materialov, 2019, vol. 85, no. 1–2, pp. 5–14.
  30. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  31. 2