Abstract

The electrophysical properties of microneedles α-Fe (Pr, Dy)(Fe, Co)B at direct current and in the mode of recording the Q-factor of the resonator in an ultrahigh frequency (1010 Hz) magnetic field directed perpendicular to the constant field are investigated. It is established that the specific resistance of microneedles at direct current is in the range (1,5–2,5)·10‒6 Om·m. The magnetoresistance of R(H) microneedles and its magnetic hysteresis at direct current have been detected. The maximum value of the magnetoresistance is R = 1,18 %. The orientation dependence of the maximum dependence dP/dH(H) is revealed.

Reference list
  1. Kablov E.N., Kondrashov S.V., Melnikov A.A., Schur P.A. Application of functional and adaptive materials obtained by 3D printing (review). Trudy VIAM, 2022, no. 2 (108), paper no. 03. Available at: http://www.viam-works.ru (accessed: June 25, 2024). DOI: 10.18577/2307-6046-2022-0-2-32-51.
  2. Kablov E.N., Ospennikova O.G., Davydova E.A., Buzenkov A.V., Valeev R.A., Morgunov R.B., Piskorsky V.P. Effect of annealing of Pr–Dy–Fe–Co–B alloy on its phase composition and properties of sintered magnets made from it. Metally, 2018, no. 2, pp. 28–32.
  3. Peng H.-X., Qin F., Phan M.-H. Ferromagnetic microwire composites: from sensors to microwave applications. Springer, 2016, 245 p.
  4. Mandal K., Puerta S., Vázquez M., Hernando A. Giant magnetoimpedance in amorphous Co83.2Mn7.6Si5.8B3.3 microwires. Physical Review B, 2000, vol. 62, no. 10, p. 6598. DOI: 0163-1829/2000/62(10)/6598(5)/$15.00.
  5. Kollmannsberger P., Fabry B. High-force magnetic tweezers with force feedback for biological applications. Review of Scientific Instruments, 2007, vol. 78, p. 114301. DOI: 10.1063/1.2804771.
  6. Dvoretskaya E.V., Koplak O.V., Korolev D.V., Valeev R.A., Sidorov V.L., Piskorsky V.P., Morgunov R.B. Influence of mode of local laser annealing on the domain structure in microwires PrDyFeCoB. Trudy VIAM, 2022, no. 5 (111), paper no. 06. Available at: http://www.viam-works.ru (accessed: June 25, 2024). DOI: 10.18577/2307-6046-2022-0-5-64-73.
  7. Zhukova V., Ipatov M., Zhukov A. Thin magnetically soft wires for magnetic microsensors. Sensors, 2009, vol. 9, p. 9216. DOI: 10.3390/s91109216.
  8. Sampaio L.C., Sinnecker E.H.C.P., Cernicchiaro G.R.C. et al. Magnetic microwires as macrospins in a long-range dipole-dipole interaction. Physical Review B, 2000, vol. 61, p. 8976. DOI: 10.1103/PhysRevB.61.
  9. Knobel M., Sampaio L.C., Sinnecker E.H.C.P., Vargas P., Altbir D. Dipolar magnetic interactions among magnetic microwires. Journal of Magnetism and Magnetic Materials, 2002, vol. 249, pp. 60–72. DOI: 10.1016/S0304-8853(02)00504-8.
  10. Vazquez M., Chiriac H., Zhukov A. et al. On the state-of-the-art in magnetic microwires and expected trends for scientific and technological studies. Physica Status Solidi (A), 2011, vol. 208, p. 493. DOI: 10.1002/pssa.201026488.
  11. Zhukov A., Zhukovа V., Blancoc J.M. et al. Magnetostriction in glass-coated magnetic microwires. Journal of Magnetism and Magnetic Materials, 2003, vol. 151, pp. 258–259. DOI: 10.1016/S0304-8853(02)01029-6.
  12. Corte-Leon P., Zhukova V., Ipatov M. et al. Stress dependence of the magnetic properties of glass-coated amorphous microwires. Journal of Alloys and Compounds, 2019, vol. 789, p. 201. DOI: 10.1016/j.jallcom.2019.03.044.
  13. Severino A.M., Gómez-Polo C., Marín P., Vázquez M. Influence of the sample length on the switching process of magnetostrictive amorphous wire. Journal of Magnetism and Magnetic Materials, 1992, vol. 103, p. 117. DOI: 10.1016/0304-8853(92)90244-I.
  14. Ye J., del Real R.P., Infante G., Vazquez M. Local magnetization profile and geometry magnetization effects in microwires as determined by magneto-optical Kerr effect. Journal of Applied Physics, 2013, vol. 113. DOI: 10.1063/1.4776730.
  15. Vazquez M., Gomez-Poio C., Chen D.-X. Switching mechanism and domain structure of bistable amorphous wires. IEEE Transactions on Magnetics, 1992, vol. 28, p. 3147. DOI: 10.1109/20.179740.
  16. Zhukov A.P., Vazquez M., Velazquez J. et al. The remagnetization process in thin and ultra-thin Fe-rich amorphous wires. Journal of Magnetism and Magnetic Materials, 1995, vol. 151, p. 132. DOI: 10.1016/0304-8853(95)00393-2.
  17. Kurlyandskaya G.V., Bebenin N.G., Vaskovsky V.O. Giant magnetic impedance of wires with a thin magnetic coating. The Physics of Metals and Metallography, 2011, vol. 111(2), pp. 133–154. DOI: 10.1134/s0031918x11010200.
  18. Baranov A.A., Zhukova S.A., Obizhaev D.Yu. et al. Magnetoimpedance sensing element based on an amorphous ferromagnetic microwire and a thin-film coil. Nano- i mikrosistemnaya tekhnika, 2017, vol. 19, no. 10, pp. 626–632. DOI: 10.17587/nmst.19.626-632.
  19. Zhukova V., Mino J., Del Val J.J. et al. GMR and Kondo Effects in Cu‒Co Microwires. Journal of Superconductivity and Novel Magnetism, 2016, vol. 30(4), pp. 1109–1114. DOI: 10.1007/s10948-016-3767-9.
  20. Granovsky A.B., Ilyin M., Zhukov A. et al. Giant magnetoresistance of granular microwires: spin-dependent scattering in intergranular gaps. Fizika tverdogo tela, 2011, vol. 53, no. 2, pp. 299–301.
  21. Taylor G.F. A Method of Drawing Metallic Filaments and a Discussion of their Properties and Uses. Physical Review, 1924, vol. 23 (5), pp. 655–660. DOI: 10.1103/physrev.23.655.
  22. Umnov P.P., Molokanov V.M., Shalimov Yu.S. et al. Features of obtaining amorphous wire by the Ulitovsky-Taylor method using a continuous casting process variant. Perspektivnye materialy, 2010, no. 2, pp. 87–91.
  23. Dvoretskaya E.V., Korolev D.V., Piskorskii V.P., Valeev R.A., Koplak O.V., Morgunov R.B. Magnetron sputtering of the iron shell and microinclusions in microwires PrDyFeCoB. Aviation materials and technologies, 2022, no. 2 (67), paper no. 08. Available at: http://www.journal.viam.ru (accessed: July 25, 2024). DOI: 10.18577/2713-0193-2022-0-2-85-96.
  24. Korolev D.V., Piskorskii V.P., Valeev R.A., Bakradze M.M., Dvoretskaya E.V., Koplak O.V., Morgunov R.B. Rare-earth RE–TM–B micromagnets engineering (review). Aviation materials and technology, 2021, no. 1 (62), paper no. 05. Available at: http://www.journal.viam.ru (accessed: July 25, 2024). DOI: 10.18577/2713-0193-2021-0-1-44-60.
  25. Veinger A.I., Zabrodskii A.G., Tisnek T.V. Anomalous Positive Microwave Magnetoresistance of Compensated Ge:Ga near the Metal-Insulator Transition. Physica Status Solidi (B), 2002, vol. 230 (1), pp. 107–111. DOI: 10.1002/1521-3951(200203)230:1107::aid-pssb107>3.0.co;2-7.
  26. Altshuler B.L., Aronov A.G. Electron–Electron Interaction in Disordered Conductors. Modern Problems in Condensed Matter Sciences, 1985, pp. 1–153. DOI: 10.1016/b978-0-444-86916-6.50007-7.
  27. Gschneidner K.A. Jr., LeRoy Ey. Handbook on the Physics and Chemistry of Rare Earths. Amsterdam: Elsevier Science, 1999, 559 р.
  28. Lide D.R. Handbook of Chemistry and Physics. Boca Raton, Florida: CRC Press, 2003, 2616 р.