Research of the 2,2-bis(4-cyanatophenyl)propane catalytic polymerization

Lavrin M.A., Shosheva A.L., Eldjaeva G.B.
Lavrin M.A., Shosheva A.L., Eldjaeva G.B. Research of the 2,2-bis(4-cyanatophenyl)propane catalytic polymerization // Proceedings of VIAM. 2025. No. 1. DOI: 10.18577/2307-6046-2025-0-1-35-45. URL: https://www.viam-works.ru/en/journal/2025/1/4
Keywords
2, 2-bis(4-cyanatophenyl)propane, tris(acetylacetonato)cobalt (III), 4-nonylphenol, thermosetting polymer resin, cyclotrimerization
Abstract

In this article the results study of modification of the 2,2-bis(4-cyanatophenyl)propane by catalytic system in order to reduce the cure temperature are presented. The methods of synthesis and heat treatment are described. The influence of curing temperature and the concentration of tris(acetylacetonato)cobalt (III), as well as 4-nonylphenol, using as solvent, on the polymerization rate of 2,2-bis(4-cyanatophenyl)propane, degree of conversion and glass transition temperature of the cured polymer matrix is shown.

Reference list
  1. Kablov E.N. Materials for aerospace engineering. Vse materialy. Entsiklopedicheskiy spravochnik, 2007, no. 5, pp. 7–27.
  2. Kablov E.N., Chursova L.V., Babin A.N., Mukhametov R.R., Panina N.N. Developments of FSUE VIAM in the field of melt binders for polymer composite materials. Polimernye materialy i tekhnologii, 2016, vol. 2, no. 2, pp. 37–42.
  3. Kablov E.N. What to make the future of? New generation materials, technologies for their creation and processing are the basis of innovations. Krylya Rodiny, 2016, no. 5, pp. 8–18.
  4. Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composites (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 48–58. DOI: 10.18577/2071-9140-2019-0-3-48-58.
  5. Dolgova E.V., Lavrova K.S. Application of cyanate ester materials (review). Part 1. Aviation and space structures. Trudy VIAM, 2021, no. 4 (98), paper no. 04. Available at: http://www.viam-works.ru (accessed: July 23, 2024). DOI: 10.18577/2307-6046-2021-0-4-48-60.
  6. Guseva M.A. Cyanic esters are prospective thermosetting binders (review). Aviacionnye materialy i tehnologii, 2015, no. 2 (35), pp. 45–50. DOI: 10.18577/2071-9140-2015-0-2-45-50.
  7. Kablov E.N. Materials and chemical technologies for Aircraft Engineering. Herald of the Russian Academy of Sciences, 2012, vol. 82, no. 3, pp. 158‒167.
  8. Muhametov R.R., Ahmadieva K.R., Kim M.A., Babin A.N. Melt binding for perspective methods of production of PCM of new generation. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 260–265.
  9. Dolgova E.V. Application of cyanate ester materials. Part 2. Microelectronics, 3D printing, radiation protection. Trudy VIAM, 2023, no. 1 (119), paper no. 12. Available at: http://www.viam-works.ru (accessed: July 23, 2024). DOI: 10.18577/2307-6046-2023-0-1-139-156.
  10. Tkachuk A.I., Donetsky K.I., Terekhov I.V., Karavaev R.Yu. The use of thermosetting matrices for the manufacture of polymer composite materials by the non-autoclave molding methods. Aviation materials and technology, 2021, no. 1 (62), paper no. 03. Available at: http://www.journal.viam.ru (accessed: July 23, 2024). DOI: 10.18577/2713-0193-2021-0-1-22-23.
  11. Shosheva A.L., Akhmadieva K.R., Valueva M.I., Nacharkina A.V. Bismaleimide resins (review). Part 2. Trudy VIAM, 2023, no. 7 (125), paper no. 04. Available at: http://www.viam-works.ru (accessed: July 23, 2024). DOI: 10.18577/2307-6046-2023-0-7-34-55.
  12. Kablov E.N. The role of chemistry in the creation of new generation materials for complex technical systems. Reports of the XX Mendeleev Congress on General and Applied Chemistry. Ekaterinburg, 2016, pp. 25–26.
  13. Kablov E.N., Chursova L.V., Lukina N.F., Kutsevich K.E., Rubtsova E.V., Petrova A.P. A Study of Epoxide-Polysulfone Polymer Systems for High-Strength Adhesives of Aviation Purpose. Polymer Science. Ser.: D, 2017, vol. 10, no. 3, pp. 225–229.
  14. Kessler M.R. Cyanate Ester Resins. Wiley Encyclopedia of Composites. Second Ed. John Wiley & Sons, 2012, pp. 1–14.
  15. Bauer M., Bauer J. Aspects of the kinetics, modeling and simulation of network build-up during cyanate ester cure. Chemistry and Technology of Cyanate Ester Resins. Ed. I. Hamerton. Chapman & Hall, 1994, pp. 58–86.
  16. Pankratov V.A., Vinogradova S.V. Polytriazines. Uspekhi khimii, 1972, vol. XLI, no. 1, pp. 117‒149.
  17. Aristov V.F., Khalimanovich V.I., Mironovich V.V., Islentyeva T.A., Gurov D.A. Cyanate-ether binders in the aerospace industry. Catalytic properties of organometallic complexes and diazonium salts with complex anions in the curing of cyanate ether binders. Vestnik SibGAU, 2013, no. 2 (48), p. 159.
  18. Anshin V.S. Cyanate ether monomers and oligomers. Review of the current state of research and development prospects. Vysokomolekulyarnye soyedineniya. Ser.: B, 2022, vol. 64, no. 3, pp. 163–196.
  19. Muhametov R.R., Ahmadieva K.R., Chursova L.V., Kogan D.I. New polymeric binding for perspective methods of manufacturing of constructional fibrous PCM. Aviacionnye materialy i tekhnologii, 2011, no. 2, pp. 38–42.
  20. Korshak V.V. Main features of polycyclotrimerization. Vysokomolekulyarnye soyedineniya. Ser.: A., 1974, vol. XVI, no. 5, pр. 926–941.
  21. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.