Weldability of heat-resistant aluminum alloy V-1213

Panteleev M.D., Bondarenko S.V., Antipov K.V., Sviridov A.V.
Panteleev M.D., Bondarenko S.V., Antipov K.V., Sviridov A.V. Weldability of heat-resistant aluminum alloy V-1213 // Proceedings of VIAM. 2025. No. 1. DOI: 10.18577/2307-6046-2025-0-1-16-25. URL: https://www.viam-works.ru/en/journal/2025/1/2
Keywords
heat-resistant aluminum alloys, weldability, welded joints, hot cracking, testing of heat-resistant aluminum alloys, filler wire
Abstract

The article presents a retrospective and possible prospects for the application of the heat-resistant aluminum alloy V-1213 of the Al–Cu–Mg alloying system. The general problems of weldability of this alloy are indicated. The causes of hot cracks in welded joints during various types of welding are analyzed, and approaches for their elimination are considered in detail. The weldability of heat-resistant aluminum alloy V-1213 with the use of filler wire Sv-1217 has been studied. The influence of the welding-thermal cycle on the structure and microhardness of the material has been evaluated.

Reference list
  1. Kablov E.N. The role of fundamental research in the creation of new generation materials. Reports of the XXI Mendeleev Congress on General and Applied Chemistry: in 6 vols. St. Petersburg, 2019, vol. 4, p. 24.
  2. Fridlyander I.N. Modern aluminum, magnesium alloys and composite materials based on them. Metallovedenie i termicheskaya obrabotka metallov, 2002, no. 7, pp. 24–29.
  3. Kablov E.N., Lukin V.I., Ospennikova O.G. Promising aluminum alloys and technologies for their joining for aerospace products. Reports of the 2nd Int. Conf. and Exhibition «Aluminum–21. Welding and Soldering». St. Petersburg: Alusil-MViT, 2012, art. 08.
  4. Shemetev G.F. Aluminum alloys: compositions, properties, application: textbook. St. Petersburg: SPbPU, 2012, part 1, 155 p. Available at: https://elib.spbstu.ru/dl/2747.pdf/view (accessed: July 10, 2024).
  5. Antipov V.V., Panteleev M.D., Sviridov A.V., Skupov A.A., Odintsov N.S. Heat-resistant aluminum alloys 1151 and B-1213 welded fuselage panels fabrication and testing. Trudy VIAM, 2023, no. 5 (123), paper no. 03. Available at: http://www.viam-works.ru (accessed: July 10, 2024). DOI: 10.18577/2307-6046-2023-0-5-33-42.
  6. Antipov V.V., Klochkova Yu.Yu., Romanenko V.A. Modern aluminum and aluminum-lithium alloys. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 195–211. DOI: 10.18577/2071-9140-2017-0-S-195-211.
  7. Chirkov E.F. Weakening rate under heating is the evaluation criterion of heat resistance of Al‒Cu‒Mg and Al‒Cu structural alloys. Aviacionnye materialy i tehnologii, 2013, no. S2, pp. 11–19.
  8. Yakushin B.F., Makarov E.L. Theory of weldability of steels and alloys. Moscow: Publ. house of MSTU im. N.E. Bauman, 2018, 487 p.
  9. Panteleev M.D., Sviridov A.V., Skupov A.A., Odintsov N.S. Aluminum-Lithium alloy V-1469 welded fuselage constructions survivability. Aviation materials and technologies, 2022, no. 4 (69), paper no. 03. Available at: http://www.journal.viam.ru (accessed: July 10, 2024). DOI: 10.18577/2713-0193-2022-0-4-25-35.
  10. Mishra R.S., Ma Z.Y. Friction stir welding and processing. Journal Material Science Engineering, 2005, vol. 50, pp. 1–78.
  11. Panteleev M.D., Sviridov A.V., Skupov A.A. Welding features of heatresistant aluminum alloys, alloy V-1213 and 1151. Trudy VIAM, 2022, no. 9 (115), paper no. 03. Available at: http://www.viam-works.ru (accessed: July 10, 2024). DOI: 10.18577/2307-6046-2022-0-9-28-38.
  12. Kablov E.N., Kutyrev A.E., Vdovin A.I., Kozlov I.A., Afanasyev-Khodykin A.N. The research of possibility of galvanic corrosion in brazed connections used in aviation engine construction. Aviation materials and technologies, 2021, no. 4 (65), paper no. 01. Available at: http://www.journal.viam.ru (accessed: July 10, 2024). DOI: 10.18577/2713-0193-2021-0-4-3-13.
  13. Kablov E.N. Aerospace Materials Science. Vse materialy. Entsiklopedicheskiy spravochnik, 2008, no. 3, pp. 2–14.
  14. Antipov V.V. Strategy of development of titanium, magnesium, beryllium and aluminum alloys. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 157–167.
  15. Antipov V.V., Senatorova O.G., Tkachenko E.A., Vahromov R.O. Aluminum deformable alloys. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 167–182.
  16. Nikulin I., Kipelova A., Gazizov M. et al. Novel Al–Cu–Mg–Ag alloy for high temperature applications. 12-th ICAA. Yokohama, 2010, pp. 2303–2308.
  17. Teleshov V.V., Andreev D.A. Influence of chemical composition on the structure, mechanical properties and crack resistance characteristics of pressed alloys of the Al–Cu–Mg–Ag–Xi system in the T1 state. Tekhnologiya legkikh splavov, 2013, no. 4, p. 20–29.
  18. Grigorev M.V., Antipov V.V., Vakhromov R.O. et al. Structure and properties of ingots from Al–Cu–Mg system alloy with silver microadditives. Aviacionnye materialy i tehnologii, 2013, no. 3, pp. 3–6.
  19. An aluminum-based alloy and a product made from it: pat. 2278179 Rus. Federation; appl. 21.12.04, publ. 20.06.06.
  20. De Geuser F., Bley F., Deschamps A. Early stage of Ω phase precipitation in Al–Cu–Mg–Ag observed in situ with and without applied stress by small angle X-ray scattering. 12-th ICAA. Yokohama, 2010, pp. 475–480.
  21. Wang S.B., Chen J.H., Yin M.J. et al. Double-atomic-wall-based dynamic precipitates of the early-stage S-phase in Al–Cu–Mg alloys. Acta Materialia, 2012, vol. 60, no. 19, pp. 6573–6580.