Fatigue life of a heat-resistant titanium alloy at various loading frequencies

Khodinev I.A., Baranova E.V.
Khodinev I.A., Baranova E.V. Fatigue life of a heat-resistant titanium alloy at various loading frequencies // Proceedings of VIAM. 2024. No. 9. DOI: 10.18577/2307-6046-2024-0-9-71-82. URL: https://www.viam-works.ru/en/journal/2024/9/7
Keywords
low-cycle fatigue, total deformation amplitude, loading frequency, titanium superalloy, high-cycle fatigue, softening curves
Abstract

The influence of loading frequency on the fatigue life characteristics of a heat-resistant titanium alloy has been studied. Low cycle fatigue (LCF) tests were performed under «severe» loading conditions at temperatures of 20 and 400 °C. High cycle fatigue tests (HCF) were performed under «mild» loading conditions at room temperature. It has been established that the effect of loading frequency on the LCF is the most significant at elevated temperatures. The main difference at a fixed level of loading of the HCF is observed in the interval from 107 cycles. With an increase in the frequency of loading, the durability increases.

Reference list
  1. Kablov E.N., Ospennikova O.G., Lomberg B.S., Sidorov V.V. Priority directions of development of technologies for production of heat-resistant materials for aircraft engine building. Problemy chernoy metallurgii i materialovedeniya, 2013, no. 3, pp. 47–54.
  2. Kablov E.N. New Generation Materials and Technologies for Their Digital Processing. Herald of the Russian Academy of Sciences, 2020, vol. 90, no. 2, pp. 225–228.
  3. Gorbovets M.A., Khodinev I.A., Ryzhkov P.V. Equipment for testing carrying out the strain-controlled low-cycle fatigue. Trudy VIAM, 2018, no. 9 (69), paper no. 06. Available at: http://www.viam-works.ru (accessed: August 03, 2023). DOI: 10.18577/2307-6046-2018-0-9-51-60.
  4. Belyaev M.S., Terentyev V.F., Bakradze M.M., Gorbovets M.A., Goldberg M.A. Low-cycle fatigue of heat-resistant alloy VZh175 under elastic-plastic deformation. Deformatsiya i razrusheniye materialov, 2014, no. 7, pp. 27–33.
  5. Nazmy M.Y. High temperature low cycle fatigue of IN 738 and application of strain range partitioning. Metallurgical Transactions A, 1983, vol. 14, pp. 449–461.
  6. Lee Y.-L., Barley M.E., Kang H.-T. Metal fatigue analysis handbook: practical problem-solving techniques for computer-aided engineering. Elsevier Inc., 2012, pp. 222–223.
  7. Inozemtsev A.A., Bashkatov I.G., Koryakovtsev A.S. Titanium alloys in products developed by Aviadvigatel JSC. Modern titanium alloys and problems of their development. Ed. E.N. Kablov. Moscow: VIAM, 2010, pp. 43–46.
  8. Prohodceva L.V., Erasov V.S., Lavrova O.Yu., Lavrov A.V. Influence of form of cycle on fatigue properties and microstructure of breaks of VT3-1 titanium alloy. Aviacionnye materialy i tehnologii, 2012, no. 2, pp. 54–58.
  9. Erasov V.S., Oreshko E.I., Lutsenko A.N. Multilevel large-scale complex research of deformation of metal materials. Aviation materials and technologies, 2022, no. 1 (66), paper no. 11. Available at: http://www.journal.viam.ru (accessed: December 21, 2023). DOI: 10.18577/2713-0193-2022-0-1-129-142.
  10. Erasov V.S., Oreshko E.I. Deformation and destruction as processes of change of volume, the areas of a surface and the linear sizes in loaded bodies. Trudy VIAM, 2016, no. 8, paper no. 11. Available at: http://www.viam-works.ru (accessed: December 21, 2023). DOI: 10.18577/2307-6046-2016-0-8-11-11.
  11. Sun C., Li Y., Huang R. et al. Crack initiation mechanism and fatigue life of titanium alloy Ti–6Al–2Sn–2Zr–3Mo-X: Effects of stress ratio and loading frequency. Materials Science and Engineering: A, 2020, vol. 798, p. 140265. DOI: 10.1016/j.msea.2020.140265.
  12. Krasovskii A.Y., Petrov Y.N., Nadezhdin G.N. Fatigue damage to a pseudo-α-titanium alloy in the 10–33-Hz frequency range. Strength of Materials, 1982, vol. 14, pp. 1320–1323. DOI: 10.1007/BF00770126.
  13. Eylon D., Bartel T.L., Rosenblum M.E. High Temperature Low Cycle Fatigue in Beta Processed Ti‒5Al‒5Sn‒2Zr‒2Mo‒0.25S. American society for metals and the metallurgical society of AIME, 1980, vol. 11A, pp. 1361–1367. DOI: 10.1007/BF02653490.
  14. Matokhnyuk L.E., Voinalovich A.V., Khlyapov A.A., Bulgakova S.G., Artyushina V.P. Fatigue limit of the titanium alloy VT23 in tests with high loading frequency. Metal Science and Heat Treatment, 1988, vol. 30, pp. 786–789.
  15. Kuzmenko V.A., Matokhnyuk L.E., Pisarenko G.G. Fatigue tests at high frequencies. Kyiv, 1979, 335 p.
  16. Erasov V.S., Oreshko E.I. Fatigue tests of metal materials (review). Part 1. Main definitions, loading parameters, representation of results of tests. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 59–70. DOI: 10.18577/2071-9140-2020-0-4-59-70.
  17. Erasov V.S., Oreshko E.I. Tests for fatigue of metal materials (review). Part 2. Analysis of the Basquin–Manson–Coffin equation. Methods of testing and processing of results. Aviation materials and technology, 2021, no. 1 (62), paper no. 08. Available at: http://www.journal.viam.ru (accessed: December 10, 2023). DOI: 10.18577/2713-0193-2021-0-1-80-94.
  18. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  19. Wang Q., Ren J.Q., Xin C. et al. Low cycle fatigue behavior of near-alpha titanium alloys used in deep-driving submersible: Ti–6Al–3Nb–2Zr–1Mo vs. Ti–6Al–4V ELI. Journal of Alloys and Compounds, 2023, vol. 934, p. 167856.
  20. Bai C., Lan L., Xin R. et al. Microstructure evolution and cyclic deformation behavior of Ti–6Al–4V alloy via electron beam melting during low cycle fatigue. International Journal of Fatigue, 2022, vol. 159, p. 106784. DOI: 10.1016/j.ijfatigue.2022.106784.
  21. Polak J. Cyclic plasticity and low cycle fatigue life of metals. Amsterdam: Elsevier, 1991. С. 123.
  22. Sharkeev Y., Eroshenko A., Mairambekova A. Features of the fracture of the Ti–45 wt.% Nb alloy in ultrafine-grained state at gigacycle fatigue. Procedia Structural Integrity, 2023, vol. 47, pp. 849–854. DOI: 10.1016/j.prostr.2023.07.034.