Possibility of using layer-by-layer deposition technology (FDM) to produce ceramic products

Turchenko M.V., Lebedeva Yu.E., Kolmogorov A.Yu., Gurov D.A., Chaynikova A.S.
Turchenko M.V., Lebedeva Yu.E., Kolmogorov A.Yu., Gurov D.A., Chaynikova A.S. Possibility of using layer-by-layer deposition technology (FDM) to produce ceramic products // Proceedings of VIAM. 2024. No. 8. DOI: 10.18577/2307-6046-2024-0-8-64-76. URL: https://www.viam-works.ru/en/journal/2024/8/6
Keywords
FDM technology, ceramic filament, ceramic additive manufacturing, aluminum oxide, zirconium dioxide
Abstract

When producing ceramic products with complex shapes, traditional methods cannot compete with additive manufacturing methods. This is due to both the complexity of manufacturing molds and injection molds, and the need for subsequent mechanical processing, which significantly complicates and increases the cost of the process of obtaining a product. This article discusses the layer-by-layer deposition technology (FDM). Its main advantages and disadvantages are given. The results of producing ceramic polymer filament and products made from it using FDM technology are presented.

Reference list
  1. Molodin V.I., Mylnikova L.N. Theory and practice of studying ancient ceramics: traditional and newest methods. Samarskiy nauchnyy vestnik, 2015, no. 3 (12), pp. 122–127.
  2. Evdokimov S.A., Shchegoleva N.E., Sorokin O.Yu. Ceramic materials aviation engineering (review). Trudy VIAM, 2018, no. 12 (72), paper no. 06. Available at: http://www.viam-works.ru (accessed: May July 02, 2024). DOI: 10.18577/2307-6046-2018-0-12-54-61.
  3. Kablov E.N. No new materials – no future. Metallurg, 2013, no. 12, pp. 4–8.
  4. Kablov E.N. Main results and directions of development of materials for advanced aviation equipment. 75 years. Aviation materials. Moscow: VIAM, 2007, pp. 20–26.
  5. Andrianov N.T., Balkevich V.L., Belyakov A.V. et al. Chemical technology of ceramics: textbook for universities. Ed. I.Ya. Guzman. Moscow: Stroymaterialy, 2012, 496 p.
  6. Semerikov I.S., Gerasimova E.S. Physical Chemistry. Construction Materials: a textbook for universities, Moscow: URAYT; Ekaterinburg: Publ. House of the Ural. Univ., 2018, 204 p.
  7. Kablov E.N., Grashchenkov D.V., Isaeva N.V., Solntsev S.S., Sevastyanov V.G. Promising high-temperature ceramic composite materials. Rossiyskiy khimicheskiy zhurnal, 2010, vol. LIV, no. 1, pp. 20–24.
  8. Kablov E.N. Trends and Guidelines for Innovative Development of Russia: collection of information materials. 3rd ed., rev. and add. Moscow: VIAM, 2015, 720 p.
  9. Gorelov V.A., Alekseev S.V. Features of mechanical processing of parts from ceramic materials. Izvestiya Moskovskogo gosudarstvennogo tekhnicheskogo universiteta MAMI, 2012, no. 2, pp. 64–67.
  10. Glazunov V.S., Cherepanova M.V. Application of additive technologies in the production of ceramic products. Vestnik Permskogo natsionalnogo issledovatelskogo politekhnicheskogo universiteta. Ser.: Khimicheskaya tekhnologiya i biotekhnologiya, 2018, no. 4, pp. 174–187.
  11. Kirillova N.K., Alekseeva A.N., Egorova A.D. Application of additive technologies in construction and in the manufacture of ceramic products. Vestnik Belgorodskogo gosudarstvennogo tekhnologicheskogo universiteta im. V.G. Shukhova, 2020, no. 2, pp. 131–141.
  12. Ilyushchenko A.F. Additive technologies and powder metallurgy. New materials and technologies: powder metallurgy, composite materials, protective coatings, welding: Proc. Int. Sci.-Tech. Conf. (September 14–16, 2022, Minsk). Minsk: Belarusian Science, 2022, рp. 17–34.
  13. Cherepanova M.V., Skovorodnikov P.V., Khazeev A.A. Application of additive technologies in the production of ceramic products of complex shapes. Nauchnyy almanakh, 2018, no. 10 (2), pp. 73–76.
  14. Lakhdar Y., Tuck C., Binner J., Terry A., Goodridge R. Additive manufacturing of advanced ceramic materials. Progress in Materials Science, 2021, vol. 116, pp. 736–742.
  15. Travitzky N., Bonet A., Dermeik B. et al. Additive manufacturing of ceramic based materials. Advanced engineering materials, 2014, vol. 16, no. 6, рp. 729–754.
  16. Krasheninnikov M.A. Features of additive technologies for product design. Traditions and innovations in construction and architecture. Construction technologies: collection of articles. Samara: Samara State arch.-tech. Univ, 2017, pp. 98–102.
  17. Istomin A.V. Study of the distribution of aluminum oxide nanopowder in a polymer solution. Aviation materials and technologies, 2024, no. 1 (74), paper no. 06. Available at: http://www.journal.viam.ru (accessed: July 01, 2024). DOI: 10.18577/2713-0193-2024-0-1-78-88.
  18. Sorokin A.E., Ivanov M.S., Sagomonova V.A. Thermoplastic polymer composite materials based on polyetheretherketones of various manufacturers. Aviation materials and technologies, 2022, no. 1 (66), paper no. 04. Available at: http://www.journal.viam.ru (accessed: July 01, 2024). DOI: 10.18577/2713-0193-2022-0-1-41-50.
  19. Sokolov A.V., Deynega G.I., Kuzmina N.A. Influence of Sc2O3 additive on sintering temperature and properties of ZrO2–Y2O3 system oxide ceramics. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 64–69. DOI: 10.18577/2071-9140-2020-0-1-64-69.
  20. Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), paper no. 10. Available at: http://www.journal.viam.ru (accessed: July 01, 2024). DOI: 10.18577/2713-0193-2023-0-2-122-144.
  21. Goncharova O.N., Berezhnoy Yu.M., Bessarabov E.N. et al. Additive technologies – a dynamically developing production. Inzhenernyy vestnik Dona, 2016, vol. 43, no. 4 (43), p. 123.
  22. Murtazina S.A. Modern production technologies and types of ceramic products. Bulletin of the Kazan Technological University, 2015, vol. 18, no. 13, pp. 135–137.
  23. Dolgin A.S., Bogdanov S.P., Makogon A.I. 3D printing with corundum pastes. Functional materials: synthesis, properties, application: collection of abstracts of the XIX All-Rus. youth scientific conf. (December 1–3, 2020, St. Petersburg). St. Petersburg: LEMA, 2020, pp. 147–148.
  24. Piterskov P.P., Pobirokhin G.S. 3D printing with ceramics. Application area. Methods. Coll. proc. of the VII Congress of young scientists (April 17–20, 2018, St. Petersburg). SPb: St. Petersburg. National University of Information Technologies, Mechanics and Optics, 2018, рp. 168–171.
  25. Smirnov A., Kuznetsova E.V., Khmyrov R.S. et al. Study of mechanical properties under tension of ceramic-polymer composites obtained by the method of layer-by-layer fusion deposition. Advanced technologies and materials: proc. Int. scientific-practical conf. (September 21–23, 2022, Sevastopol). Sevastopol: Sevastopol State Univ., 2022, pp. 199–202.
  26. Smirnov A., Kuznetsova E.V., Podrabinnik N.N. et al. Production of filament based on aluminum oxide and polylactide for 3D printing of objects with complex geometry. Priority areas of innovative activity in industry: Coll. Sci. Art. VIII Int. sci. conf. (August 30–31, 2021, Kazan). Kazan: Konvert, 2021, p. 45.
  27. Smirnov A., Kuznetsova E.V., Podrabinnik N.N. et al. Development and study of ceramic-polymer filament for 3D printing by the fused deposition method. Advanced technologies and materials: Proc. Int. Sci. And Practical Conf. (October 6–8, 2021, Sevastopol). Sevastopol: Sevastopol State Univ., 2021, pp. 228–232.
  28. Furong N., Xiaole Y., Yuanbing L. et al. Fused deposition modeling of Si3N4 ceramics: A cost-effective 3D-printing route for dense and high performance non-oxide ceramic materials. Journal of the European Ceramic Society, 2022, vol. 42, no. 15, рр. 7369–7376.
  29. Abdullah A., Noraihan T., Dasmawati M. et al. Mechanical and physical properties of highly ZrO2/β-TCP filled polyamide 12 prepared via deposition modeling (FDM) 3D printer for potential craniofacial reconstruction application. Materials Letters. 2017, vol. 189, рр. 307–309.
  30. Furrong N., Xiaole Y., Yuanbing L. et al. Fused deposition modeling of dense complex-shaped SiCp/Al composites with excellent properties. Materials Letters. 2024, vol. 364, рр. 1363–1367.
  31. He Q., Jiang J., Yang X. et al. Additive manufacturing of dense zirconia ceramics by fused deposition modeling via screw extrusion. Journal of the European Ceramic Society, 2021, vol. 41, no. 1, pp. 1033–1040.
  32. Guan Z., Yang X., Liu P. et al. Additive manufacturing of zirconia ceramic by fused filament fabrication. Ceramics International, 2023, vol. 49, no. 17, pp. 27742–27749.
  33. Garshin A.P., Bogdanov S.P., Dolgin A.S., Makagon A.I. Use of ceramic pastes based on core-shell powders for 3D printing. Powder metallurgy: surface engineering, new powder composite materials. Welding: Reports of the 12th Int. Symposium (April 7–9, 2021, Minsk): in 2 parts. Minsk: Belarusian science, 2021, part 1, pp. 370–376.
  34. Sagun A.I. Development of thermoplastic feedstock for 3D printing from aluminum oxide. Problems of mechanics: theory, experiment and new technologies: Reports. XVII All-Rus. conf. young scientists (February 26, 2023, Novosibirsk – Sheregesh). Ed. E.I. Kraus. Novosibirsk: Novosibirsk National Research State Univ., 2023, pp. 165–166.
  35. Jinsong C., Enquan B., Dazhi H. et al. Extrusion Freeforming-Based 3D Printing of Ceramic Materials. Materials Transactions, 2020, vol. 61, no. 11, pp. 2236–2240.
  36. Vozarova M., Neubauer E., Baca L. et al. Preparation of fully dense boron carbide ceramics by Fused Filament Fabrication (FFF). Journal of the European Ceramic Society, 2023, vol. 43, no. 5, pp. 1751–1761.