Research of corrosion resistance of the hybrid layered metal polymeric materials

Zhelezina G.F., Kulagina G.S., Kan A.Ch., Solovjova N.A.
Zhelezina G.F., Kulagina G.S., Kan A.Ch., Solovjova N.A. Research of corrosion resistance of the hybrid layered metal polymeric materials // Proceedings of VIAM. 2024. No. 8. DOI: .18577/2307-6046-2024-0-8-38-47. URL: https://www.viam-works.ru/en/journal/2024/8/4
Keywords
metal polymer material, organoplastic, aluminum, corrosion, anodic oxidation
Abstract

Complex research of corrosion resistance of the hybrid layered metal polymer material «aluminum–organoplastiс» has been conducted according to the techniques accepted for different classes of materials: metals, polymer composites, adhesive compounds. It is established that the hybrid material has corrosion on surface and at the ends of the samples such as a metal alloy has. An there is also a number of features which are caused by layered structure of the metal composite, the permeability of layers of organoplastic to moisture and electrolytes.

Reference list
  1. Kablov E.N., Antipov V.V., Girsh R.I., Serebrennikova N.Y., Konovalov A.N. Fiber Metal Laminates Based on Aluminum–Lithium Alloy Sheets in New-generation Aircraft. Russian Engineering Research, 2021, vol. 41, no. 3, pp. 215–221.
  2. Podzhivotov N.Y., Kablov E.N., Antipov V.V. et al. Laminated Metal-Polymeric Materials in Structural Elements of Aircraft. Inorganic Materials: Applied Research, 2017, vol. 8, no. 2, pp. 211–221.
  3. Kablov E.N., Antipov V.V., Klochkova Yu.Yu. New-generation aluminum-lithium alloys and layered aluminum-glass plastics based on them. Tsvetnye metally, 2016, no. 8 (884), pp. 86–91. DOI: 10.17580/tsm.2016.08.13.
  4. Mashinskaya G.P., Zhelezina G.F. Alor. The Great Russian Encyclopedia: in 35 vols. Moscow, 2005, vol. 1, р. 518.
  5. Antipov V.V., Serebrennikova N.Yu., Konovalov A.N., Nefedova Yu.N. Perspectives of application of fiber metal laminate materials based on aluminum alloys in aircraft design. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 45–53. DOI: 10.18577/2071-9140-2020-0-1-45-53.
  6. Mashinskaya G.P., Zhelezina G.F., Senatorova O.G. Laminated Fibrous Metal – Polymer Composites. Soviet Advanced Composites Technology Series. Eds. J.N. Fridleander, I.H. Marshall. 1995, no. 3: Metal Matrix Composites, pp. 487–570.
  7. Gunnink J.W., Vlot A., De Vries T.J., Van Der Hoeven W. Glare technology development 1997–2000. Applied Composite Materials, 2002, no. 9, pp. 201–219.
  8. Kablov E.N., Antipov V.V., Girsh R.I., Serebrennikova N.Yu., Konovalov A.N. Engineered layered materials based on sheets of aluminum-lithium alloys and fiberglass in the structures of new-generation aircraft. Vestnik mashinostroyeniya, 2020, no. 12, pp. 46–52.
  9. Zhelezina G.F., Voynov S.I., Solovieva N.A., Kulagina G.S. Aramid organo-textolites for impact-resistant aircraft structures. Zhurnal prikladnoy khimii, 2019, vol. 92, no. 3, pp. 358–364. DOI: 10.1134/S0044461819030101.
  10. Zhelezina G.F., Kolobkov A.S., Kulagina G.S., Kan A.Ch. Damping properties of hybrid layered metal-polymer materials based on aluminum, titanium alloys and organoplastics layers. Trudy VIAM, 2021, no. 2 (96), paper no. 02. Available at: http://www.viam-works.ru (accessed: March 25, 2023). DOI: 10.18577/2307-6046-2021-0-2-10-19.
  11. Akmeev A.R., Gulyaev I.N., Ilyichev A.V., Ivanov N.V. Research of mechanical behavior of metal composite (aluminum and carbon fiber-reinforced polymer) with an adaptive reinforcement scheme. Aviacionnye materialy i tehnologii, 2017, no. 3 (48), pp. 43–49. DOI: 10.18577/2071-9140-2017-0-3-43-49.
  12. Yakovlev A.L., Nochovnaya N.A., Putyrskij S.V., Krohina V.A. Titanium-polymer laminated materials. Aviacionnye materialy i tehnologii, 2016, no. S2, pp. 56–62. DOI: 10.18577/2071-9140-2016-0-S2-56-62.
  13. Arislanov A.A., Goncharova L.J., Nochovnaya N.А., Goncharov V.A. Prospects for the use of titanium alloys in laminated composite materials. Trudy VIAM, 2015, no. 10, paper no. 04. Available at: http://www.viam-works.ru (accessed: February 12, 2024). DOI: 10.18577/2307-6046-2015-0-10-4-4.
  14. Kablov E.N., Startsev V.O. Effect of Internal Stresses on Aging of Polymer Composite Materials. Review. Mekhanika kompozitnykh materialov, 2021, vol. 57, no. 5, pp. 805–822.
  15. Startsev O.V., Krotov A.S., Senatorova O.G., Anikhovskaya L.I., Antipov V.V., Grashchenkov D.V. Sorption and Diffusion of Moisture in Layered Metal-Polymer Composite Materials of the SIAL Type. Materialovedenie, 2011, no. 12, pp. 38–44.
  16. Startsev V.O., Plotnikov V.I., Antipov Yu.V. Reversible influence of moisture on the mechanical properties of PCM after weathering. Trudy VIAM, 2018, no. 5 (65), paper no. 12. Available at: http://www.viam-works.ru (accessed: February 12, 2024). DOI: 10.18577/2307-6046-2018-0-5-110-118.
  17. Aviation materials: a reference book in 13 vols. Ed. E.N. Kablov. 7th ed., add. and rev. Moscow: VIAM, 2015, vol. 13: Climatic and microbiological resistance of non-metallic materials, 270 p.
  18. Kablov E.N., Startsev V.O. Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review). Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 47–58. DOI: 10.18577/2071-9140-2018-0-2-47-58. DOI: 10.18577/2071-9140-2018-0-2-47-58.
  19. Antipov V.V., Kurs M.G., Girsh R.I., Serebrennikova N.Yu. Climatic field tests of SIAL type metal-polymer composition materials in marine climate. Aviacionnye materialy i tehnologii, 2019, no. 4 (57), pp. 56–64. DOI: 10.18577/2071-9140-2019-0-4-56-64.
  20. Kablov E.N., Startsev O.V., Medvedev I.M. Review of international experience on corrosion and corrosion protection. Aviacionnye materialy i tehnologii, 2015, no. 2 (35), pp. 76–87.
  21. Kablov E.N., Startsev O.V., Medvedev I.M., Panin S.V. Corrosive aggressiveness of the coastal atmosphere. Part 1. Influencing factors (review). Korroziya: materialy, zashchita, 2013, no. 12, pp. 6–18.
  22. Kablov E.N., Startsev O.V., Medvedev I.M. Corrosive aggressiveness of the coastal atmosphere. Part 2. New approaches to assessing the corrosivity of coastal atmospheres. Korroziya: materialy, zashchita, 2016, no. 1, pp. 1–15.
  23. Kablov E.N., Startsev V.O. Climatic aging of polymer composite materials for aviation purposes. I. Assessment of the influence of significant influencing factors. Deformatsiya i razrushenie materialov, 2019, no. 12, pp. 7–16.
  24. Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), paper no. 10. Available at: http://www.journal.viam.ru (accessed: February 10, 2024). DOI: 10.18577/2713-0193-2023-0-2-122-144.
  25. Startsev V.O. The degradation of polymer composite materials in seawater (review). Aviation materials and technologies, 2023, no. 1 (70), paper no. 12. (accessed: March 15, 2024). DOI: 10.185577/2713-0193-2023-0-1-148-170.
  26. Method for measuring parameters of freely damped oscillations of a torsional pendulum: pat. RU 2258912 Rus. Federation; appl. 14.05.03; publ. 20.08.05.
  27. Duyunova V.A., Kozlov I.A., Oglodkov M.S., Kozlova A.A. Modern trends in the anodic oxidation of aluminum-lithium and aluminum alloys (review). Trudy VIAM, 2019, no. 8 (80), paper no. 09. Available at: http://www.viam-works.ru (accessed: March 05, 2024). DOI: 10.18577/2307-6046-2019-0-8-79-89.
  28. Fomina M.A., Volkov I.A., Vdovin A.I., Yamshchikov E.I. Study of protective capacity anodic oxide coating with environmental friendly improved filling technology. Aviation materials and technologies, 2023, no. 4 (73), paper no. 10. Available at: http://www.journal.viam.ru (accessed: February 12, 2024). DOI: 10.18577/2713-0193-2023-0-4-101-110.