Effect of mutual stabilization of polyetheretherketone and thermotropic liquid crystal polymers in polymer composites based on then for 3D printing

Gurov D.A., Tsapenko A.N., Pavlukovich N.G.
Gurov D.A., Tsapenko A.N., Pavlukovich N.G. Effect of mutual stabilization of polyetheretherketone and thermotropic liquid crystal polymers in polymer composites based on then for 3D printing // Proceedings of VIAM. 2024. No. 8. DOI: 10.18577/2307-6046-2024-0-8-3-18. URL: https://www.viam-works.ru/en/journal/2024/8/1
Keywords
additive technologies, fused deposition modeling, polyetheretherketone, semi-crystalline polymer, thermotropic liquid crystal polymers, stabilization, warpage
Abstract

The effects of mutual diffusion, expressed in the nature of the temperature dependences of viscosity and other thermophysical characteristics of the melt of a filament based on polyetheretherketone (PEEK) and liquid crystal polymers (LCP), including depending on the printing speed and the content of the LC phase, are considered and substantiated. Relaxation transitions inside the fiber itself and the film obtained from it by 3D printing are characterized. It has been shown that the introduction of LCP into a thermoplastic matrix based on PEEK can stabilize the viscous behavior of the melt of a thread during its solidification.

Reference list
  1. Kablov E.N. New Generation Materials and Technologies for Their Digital Processing. Herald of the Russian Academy of Sciences, 2020, vol. 90, no. 2, pp. 225–228.
  2. Onishchenko G.G., Kablov E.N., Ivanov V.V. Scientific and technological development of Russia in the context of achieving national goals: problems and solutions. Innovatsii, 2020, no. 6 (260), pp. 3–16.
  3. Kablov E.N., Kondrashov S.V., Melnikov A.A., Pavlenko S.A., Guseva M.A., Pykhtin A.A., Larionov S.A. Investigation of the influence of the thermal regime of FDM printing on the structuring and warping of polyethylene samples. Trudy VIAM, 2021, no. 7 (101), paper no. 06. Available at: http://www.viam-works.ru (accessed: August 18, 2023). DOI: 10.18577/2307-6046-2021-0-7-48-58.
  4. Kondrashov S.V., Pykhtin A.A., Larionov S.A., Sorokin A.E. Influence of the technological FDM-modes of the press and structure of used materials on physic-mechanical characteristics of FDM-models (review). Trudy VIAM, 2019, no. 10 (82), paper no. 04. Available at: http://www.viam-works.ru (accessed: August 18, 2023). DOI: 10.18577/2307-6046-2019-0-10-34-49.
  5. Pykhtin A.A., Sorokin A.E., Larionov S.A., Lonskii S.L. Study of the influence of non-covalent modifiers on the structure and properties of polymer filaments for FDM-printing based on ABS-plastic and carbon nanoparticles. Trudy VIAM, 2021, no. 10 (104), paper no. 04. Available at: http://www.viam-works.ru (accessed: August 18, 2023). DOI: 10.18577/2307-6046-2021-0-10-36-44.
  6. Kirin B.S., Lonskii S.L., Petrova G.N., Sorokin A.E. Materials for the 3D-printing on the basis of polyetheretherketones. Trudy VIAM, 2019, no. 4 (76), paper no. 03. Available at: http://viam-works.ru (accessed: August 18, 2023). DOI: 10.18577/2307-6046-2019-0-4-21-29.
  7. Armillotta A., Bellotti M., Cavallaro M. Warpage of FDM parts: Experimental tests and analytic model. Robotics and Computer–Integrated Manufacturing, 2018, vol. 50, pp. 140–152.
  8. Alsoufi M., El-Sayed A. Warping Deformation Of Desktop 3D Printed Parts Manufactured By Open Source Fused Deposition Modeling (FDM) System. International Journal of Mechanical and Mechatronics Engineering, 2017, vol. 17, pp. 7–16.
  9. Schumacher C., Schöppner V., Fels C. A method to evaluate the process-specific warpage for different polymers in the FDM process. PROCEEDINGS OF PPS-34: The 34th International Conference of the Polymer Processing Society – Conference Papers, 2019, vol. 2065, no. 1, pp. 0300571–0300575.
  10. Deberdeev T.R., Akhmetshina A.I., Karimova L.K. et al. Heat-resistant polymeric materials based on liquid crystal compounds. Vysokomolekulyarnye soyedineniya. Ser.: S, 2020, vol. 62, no. 2, pp. 145–165. DOI: 10.31857/S230811472002003X.
  11. Lyashenko E.Yu., Yakovleva K.A., Andreeva T.I. et al. Composite materials based on polyetheretherketone. Plasticheskie massy, 2023, no. 1–2, pp. 11–13. DOI: 10.35164/0554-2901-2023-1-2-11-13.
  12. D’amore A., Kenny J.M., Nicolais L. Dynamic-Mechanical and Dielectric Characterization of PEEK Crystallization. Polymer Engineering and Science, 1990, vol. 30, no. 5, pp. 314–320.
  13. Fougnies C., Dosie`re M., Koch M.H.J., Roovers J. Cold Crystallization of Narrow Molecular Weight Fractions of PEEK. Macromolecules, 1999, vol. 32, pp. 8133–8138.
  14. Jonas A., Legras R. Relation between PEEK Semicrystalline Morphology and Its Subglass Relaxations and Glass Transition. Macromolecules, 1993, vol. 26, pp. 813–824.
  15. Williams M.L., Landel R.F., Ferry J.D. The temperature dependence of relaxation mechanisms in amorphous polymers and other glass-forming liquids. Journal of the American Chemical Society, 1955, vol. 77, pp. 3701–3705.
  16. Lannunziata E., Colucci G., Minetola P., Giubilini A. Effect of annealing treatment and infill percentage on 3D printed PEEK samples by Fused Filament Fabrication. The International Journal of Advanced Manufacturing Technology, 2024, vol. 131, pp. 5209–5222.
  17. Gardea F., Glaz B., Riddick J. et al. Thermally activated energy dissipation in semi-crystalline polymer nanocomposites. Composites Science and Technology, 2016, vol. 134, pp. 275–286.
  18. Choupin T. Mechanical perfomances of PEKK thermoplastic composites linked to their processing parameters: PhD thesis. Paris: Ecole nationale superieure d’arts et métiers, 2017, p. 16.
  19. Gotsisa A.D., Odriozola M.A. Extensional viscosity of a thermotropic liquid crystalline polymer. Journal of Rheology, 2000, vol. 44, no. 5, pp. 1205–1223.
  20. Vanaei H.R., Raissi K., Deligant M. et al. Toward the understanding of temperature effect on bonding strength, dimensions and geometry of 3D-printed parts. Journal of Materials Science, 2020, vol. 55, no. 29, pp. 14677–14689.
  21. Ma Q., Pyda M., Mao B., Cebe P. Relationship between the rigid amorphous phase and mesophase in electrospun fibers. Polymer, 2013, vol. 54, no. 10, pp. 2544–2554.
  22. Calleja G., Jourdan A., Ameduri B., Habas J.-P. Where is the glass transition temperature of poly(tetrafluoroethylene)? A new approach by dynamic rheometry and mechanical tests. European Polymer Journal, 2013, vol. 49, no. 8, pp. 2214–2222.
  23. Righetti M.C. Amorphous Fractions of Poly(lactic acid). Synthesis, Structure and Properties of Poly(lactic acid). Advances in Polymer Science, 2017, vol. 279, pp. 195–234.
  24. Sirota E.B. Polymer Crystallization:  Metastable Mesophases and Morphology. Macromolecules, 2007, vol. 40, no. 4, pp. 1043–1048.
  25. Androsch R., Di Lorenzo M.L., Schick C., Wunderlich B. Mesophases in polyethylene, polypropylene, and poly(1-butene). Polymer, 2010, vol. 51, no. 21, pp. 4639–4662.
  26. Kiss G. Anomalous Temperature Dependence of Viscosity of Thermotropic Polyesters. Journal of Rheology, 1986, vol. 30, no. 3, pp. 585–599.
  27. Shabaev A.S., Zhansitov A.A., Khakyasheva E.V., Khashirova S.Yu. Study of Thermo-Oxidative Transformations of Unstabilized and Stabilized Poly(ether ether ketone). Polymer Science, Series B, 2019, vol. 61, no. 5, pp. 582–588.
  28. Al Lafi A.G., Parker D.J., Hay J.N. The crosslinking of poly (ether ether ketone): Thermally and by irradiation. Journal of Applied Polymer Science, 2015, vol. 132, p. 41999.
  29. Tsotra P., Toma M., Pascual A. et al. Thermo-oxidative degradation of PEEK at high temperatures. ECCM18 – 18th European Conference on Composite Materials, 2018, pp. 1–8.
  30. Zhou Z., Zhang S., Mu J. et al. Effect of Antioxidants on the Stability of Poly(ether ether ketone) and the Investigation on the Effect Mechanism of the Antioxidants to Poly(ether ether ketone. Journal of Macromolecular Science, Part A: Pure and Applied Chemistry, 2012, vol. 49, pp. 571–577.
  31. Patel P., Hull T.R., McCabe R.W. et al. Mechanism of Thermal Decomposition of Poly(Ether Ether Ketone) (PEEK) from a Review of Decomposition Studies. Polymer Degradation and Stability, 2010, vol. 95, pp. 709–718.