Preservation of the properties of paint coatings after exposure to climatic factors and micromycetes-destructors

Krivushina A.A., Kogan A.M., Startsev V.O.
Krivushina A.A., Kogan A.M., Startsev V.O. Preservation of the properties of paint coatings after exposure to climatic factors and micromycetes-destructors // Proceedings of VIAM. 2024. No. 7. DOI: 10.18577/2307-6046-2024-0-7-66-76. URL: https://www.viam-works.ru/en/journal/2024/7/8
Keywords
biodeterioration, paint coatings, degrading microorganisms, microbiological resistance, microbiological damage, micromycetes, polymeric materials, enamels
Abstract

The properties of coatings EP-140 and VE-69 were studied for the stability after conducting accelerated laboratory climatic tests and fungal resistance tests. Micromycetes isolated in three climatic zones were used: temperate climate, warm temperate climate and dry subtropical climate. It is noted that the adhesive properties of coatings VE-69 and EP-140 do not change after accelerated climatic tests and exposure to micromycetes from three climatic zones. Changes in decorative properties were revealed. Changes in indicators such as gloss and color were noted.

Reference list
  1. Polyakova A.V., Krivushina A.A., Goryashnik Yu.S., Buharev G.M. Microbiological resistance tests under nature conditions in variety of climatiс zones. Trudy VIAM, 2016, no. 4, paper no. 11. Available at: http://www.viam-works.ru (accessed: April 04, 2024). DOI: 10.18577/2307-6046-2016-0-4-11-11.
  2. Buznik V.M., Kablov E.N. Materials for the development of the Arctic and cold territories. Reports XXI Mendeleev Congress on General and Applied Chemistry: in 6 vols. St. Petersburg, 2019, vol. 4, p. 21.
  3. Kablov E.N. The role of fundamental research in the creation of new generation materials. Reports XXI Mendeleev Congress on General and Applied Chemistry: in 6 vols. St. Petersburg, 2019, vol. 4, p. 24.
  4. Kablov E.N., Startsev O.V., Medvedev I.M. Corrosive aggressiveness of the coastal atmosphere. 2. New approaches to assessing the corrosivity of coastal atmospheres. Korroziya: materialy, zashchita, 2016, no. 1, pp. 1–15.
  5. Kablov E.N., Laptev A.B., Prokopenko A.N., Gulyaev A.I. Relaxation of polymeric composite materials under the prolonged action of static load and climate (review). Part 1. Binders. Aviation materials and technologies, 2021, no. 4 (65), paper no. 08. Available at: http://www.journal.viam.ru (accessed: April 04, 2024). DOI: 10.18577/2071-9140-2021-0-4-70-80.
  6. Startsev O.V., Medvedev I.M., Kurs M.G. Hardness as the indicator of corrosion of aluminum alloys in sea conditions. Aviacionnye materialy i tehnologii, 2012, no. 3, pp. 16–19.
  7. Batraev I.S., Rybin D.K., Ivanyuk K.V., Ulianitsky V.Yu., Shtertser A.A. Wear resistant detonation coatings based on tungsten carbide for aviation products. Aviation materials and technologies, 2022, no. 1 (66), paper no. 08. Available at: http://www.journal.viam.ru (accessed: April 04, 2024). DOI: 10.18577/2713-0193-2022-0-1-92-109.
  8. Merkulova Yu.I., Kuznetsova V.A., Kodachenko E.N., Zheleznyak V.G. Study of the influence of the primer layer’s chemical nature on the properties of the coating system based on fluoropolyurethane enamel. Aviation materials and technologies, 2022, no. 1 (66), paper no. 09. Available at: http://www.journal.viam.ru (accessed: April 04, 2024). DOI: 10.18577/2713-0193-2022-0-1-110-119.
  9. Zheleznyak V.G., Serdcelyubova A.S., Merkulova Yu.I., Skivko P.V. Paint coating system based on polyurethane enamel for protecting heated frontal surfaces of aviation products. Aviation materials and technologies, 2022, no. 1 (66), paper no. 10. Available at: http://www.journal.viam.ru (ассеssed: April 04, 2024). DOI: 10.18577/2713-0193-2022-0-1-120-128.
  10. Merkulova Yu.I., Kurshev E.V., Vdovin A.I., Andreeva N.P. Microstructural and electrochemical studies of paint coatings under natural climate tests of tropical climate of North America. Aviation materials and technologies, 2022, no. 2 (67), paper no. 11. Available at: http://www.journal.viam.ru (accessed: April 04, 2024). DOI: 10.18577/2713-0193-2022-0-2-120-130.
  11. Rojas T.I., Aira M.J., Batista A. et al. Fungal biodeterioration in historic buildings of Havana (Cuba). Grana, 2012, vol. 51, is. 1, pp. 44–51.
  12. Popikhina E.A., Trepova E.S. Microdestructors of building materials. Reports Fourth Congress of Russian Mycologists «Modern Mycology in Russia»: in 7 vols. Moscow: National Academy of Mycology, 2017, vol. 6, pp. 424–426.
  13. Ogarkova G.R., Bukovskaya N.E., Samusenok L.V., Ogarkov B.N. Biodamage of porous building materials by associations of specific microorganisms. Reports Third Congress of Russian Mycologists «Modern Mycology in Russia»: in 3 vols. Moscow: National Academy of Mycology, 2012, vol. 3, pp. 224–225.
  14. Balyuta A.A., Vazhinskaya I.S. Resistance of modern building materials to mold damage. Reports Third Congress of Russian Mycologists «Modern Mycology in Russia»: in 3 vols. Moscow: National Academy of Mycology, 2012, vol. 3, p. 210.
  15. Kataev A.D., Kurakov A.V. Microbial colonization and destruction of biodegradable synthetic materials based on polyhydroxybutyrate and polyhydroxyvalerate in soils. Reports Third Congress of Russian Mycologists «Modern Mycology in Russia»: in 3 vols. Moscow: National Academy of Mycology, 2012, vol. 3, рр. 218–219.
  16. Goncharova I.A., Sabadakha E.N., Trigubovich A.M., Chernaya N.V. Mycological analysis of industrial materials contaminated with microscopic fungi. Trudy BGTU. Ser.: 2, 2020, no. 2, pp. 163–168.
  17. Smolyanitskaya O.L. Micromycetes as potential agents of biodamage to cultural property and a strategy for protecting against them in the State Hermitage: thesis abstracts, Cand. Sc. (Bio.). St. Petersburg, 2007, 26 p.
  18. Sevastyanov D.V., Sutubalov I.V., Daskovskij M.I., Shein E.A. Polymer biocomposites based on biodegradable binders reinforced by natural fibers (review). Aviacionnye materialy i tehnologii, 2017, no. 4 (49), pp. 42–50. DOI: 10.18577/2071-9140-2017-0-4-42-50.
  19. Goryaeva A.G., Velikova T.D., Dobrusina S.A. Mycobiota of air and paper composites with polymer coatings in the Russian National Library. Mikologiya i fitopatologiya, 2010, no. 44 (1), pp. 10–18.
  20. Antipov V.V., Krivushina A.A., Startsev V.O., Kogan A.M. Study of the paint coatings properties after impact of micromycetes in a moderate and moderate warm climate. Trudy VIAM, 2023, no. 6 (124), paper no. 11. Available at: http://www.viam-works.ru (accessed: April 04, 2024). DOI: 10.18577/2307-6046-2023-0-6-130-141.
  21. Krivushina A.A., Bobyreva T.V., Yakovenko T.V., Nikolaev E.V. Methods of microorganisms-destructors storage in FSUE «VIAM» collection (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 89–94. DOI: 10.18577 / 2071-9140-2019-0-3-89-94.
  22. Lugauskas A.Yu., Mikulskienė A.I., Shlauzhenė D.Yu. Catalog of micromycetes – biodestructors of polymer materials. Moscow: Nauka, 1987, pp. 258–259.
  23. Saparrat M.C.N., Arambarri A.M., Balatti P.A. Growth response and extracellular enzyme activity of Ulocladium botrytis LPSC 813 cultured on carboxy-methylcellulose under a pH range. Biology and Fertility of soils, 2007, vol. 44, pp. 383–386. DOI: 10.1007/s00374-007-0217-7.
  24. Lu Y., Qiu J., Wang S. et al. Species diversity and toxigenic potential of Fusarium incarnatum-equiseti species complex isolates from rice and soybean in China. Plant Disease, 2021, vol. 105, no. 9, pp. 2628–2636. DOI: 10.1094/PDIS-09-20-1907-RE.
  25. Pidoplichko N.M. Fungi-parasites of cultivated plants: Key: in 3 vols. Kyiv: Naukova Dumka, 1977, vol. 2, pp. 140–142.
  26. Manamgoda D.S., Cai L., McKenzie E.H.C. et al. A phylogenetic and taxonomic re-evaluation of the Bipolaris – Cochliobolus – Curvularia Complex. Fungal Diversity, 2012, vol. 56, pp. 131–144. DOI: 10.1007/s13225-012-0189-2.