Granulation of model compositions produced by national research center «Kurchatov Institute» – VIAM for castings on smelted models

Forostovich T.L., Narskiy A.R., Bityutskaya O.N., Mokeev N.A.
Forostovich T.L., Narskiy A.R., Bityutskaya O.N., Mokeev N.A. Granulation of model compositions produced by national research center «Kurchatov Institute» – VIAM for castings on smelted models // Proceedings of VIAM. 2024. No. 7. DOI: 10.18577/2307-6046-2024-0-7-3-11. URL: https://www.viam-works.ru/en/journal/2024/7/1
Keywords
model compositions, wax, plasticizer, petroleum polymer resin, precision casting, superalloys, granulation
Abstract

The technological issues of manufacturing modern high-quality model compositions of the VIAM type based on domestic raw materials for the production of parts by casting on smelted models are considered. The results of experimental studies conducted at the National Research Center «Kurchatov Institute» – VIAM, to study the possibility of granulating model compositions made it possible to improve the manufacturability of their production process. The resulting granules, due to their high bulk density, made it possible to simplify both the loading of pressing equipment and packaging for subsequent storage.

Reference list
  1. Ospennikova O.G., Pikulina L.V., Shunkin V.N. Model compositions for casting blades of gas turbine engines. Liteynoe proizvodstvo, 2001, no. 10, pp. 23–24.
  2. Lost wax casting. Ed. Ya.I. Shklennik, V.A. Ozerova. Ed. 3rd. Moscow: Mashinostroyenie, 1984, 408 p.
  3. Ospennikova O.G., Aslanyan I.R. Directions for the development of technology for manufacturing model compositions for blades and other gas turbine engine parts. Liteynoe proizvodstvo, 2018, no. 3, pp. 20–24.
  4. Ospennikova O.G., Kablov E.N., Shunkin V.N. Development and research of a plasticizer for model compositions based on natural waxes. Aviacionnye materialy i tehnologii, 2002, no. 3, рр. 68–70.
  5. Narsky A.R., Deynega G.I., Kuzmina I.G. Obtaining a fine-grained structure of castings from nickel superalloys using a cobalt aluminate modifier. Aviation materials and technologies, 2023, no. 3 (72), paper no. 01. Available at: http://www.journal.viam.ru (accessed: March 25, 2024). DOI: 10.18577/2713-0193-2023-0-3-3-14.
  6. Echin A.B., Bondarenko Yu.A., Kolodyazhny M.Yu., Surova V.A. Review of perspective high-temperature superalloys based on refractory non-metallic materials for production of gas turbine engines. Aviation materials and technologies, 2023, no. 3 (72), paper no. 03. Available at: http://www.journal.viam.ru (accessed: March 25, 2024). DOI: 10.18577/2713-0193-2023-0-3-30-41.
  7. Ospennikova O.G. Thermophysical and rheological characteristics of synthetic resins for model compositions. Liteynoe proizvodstvo, 2016, no. 10, pp. 26–28.
  8. Ospennikova O.G. New generation heat-resistant alloys and model compositions for investment casting. Liteynoe proizvodstvo, 2016, no. 3, pp. 17–20.
  9. Guseva M.A., Aslanyan I.R. The effect of fillers on the rheology of model composition. Trudy VIAM, 2019, no. 5 (77), paper no. 11. Available at: http://www.viam-works.ru (accessed: March 25, 2024). DOI: 10.18577/2307-6046-2019-0-5-94-102.
  10. Ospennikova O.G., Khayutin S.G. Structure of model compositions for lost wax casting. Materialovedenie, 2009, no. 10, pp. 46–51
  11. Ospennikova O.G. Influence research of fillers on properties and stability of modelling compositions, a choice of optimum structures. Aviacionnye materialy i tehnologii, 2014, no. 3, pp. 14–17. DOI: 10.18577/2071-9140-2014-0-3-14-17.
  12. Ospennikova O.G. Research and working out of parametres of technological process of manufacturing of models from modelling compositions on the basis of synthetic waxes. Aviacionnye materialy i tehnologii, 2014, no. 3, pp. 18–21. DOI: 10.18577/2071-9140-2014-0-3-18-21.
  13. Ospennikova O.G., Kablov E.N., Shunkin V.N. Model compositions based on synthetic materials for casting gas turbine engine blades. Aviacionnye materialy i tehnologii, 2002, no. 3, pp. 64–67.
  14. Echin A.B., Deynega G.I., Narsky A.R. New developments of NRC «Kurchatov Institute» – VIAM in the field of materials for casting processes of superalloys. Trudy VIAM, 2023, no. 8 (126), paper no. 02. Available at: http://www.viam-works.ru (accessed: March 25, 2024). DOI: 10.18577/2307-6046-2023-0-8-13-24.
  15. Composition for making lost wax models: pat. 2600468 C2 Rus. Federation; appl. 20.03.15; publ. 10.08.16.