Properties of sintered magnets Pr–Dy–Fe–Co–B depending on the composition and technological parameters of manufacture

Buzenkov A.V., Burkanov M.V., Valeev R.A., Piskorsky V.P.
Buzenkov A.V., Burkanov M.V., Valeev R.A., Piskorsky V.P. Properties of sintered magnets Pr–Dy–Fe–Co–B depending on the composition and technological parameters of manufacture // Proceedings of VIAM. 2024. No. 5. DOI: 10.18577/2307-6046-2024-0-5-91-100. URL: https://www.viam-works.ru/en/journal/2024/5/9
Keywords
magnetic hard materials, navigation devices, sintering temperature, rectangularity of demagnetization curve, coercive force, residual induction, chemical composition
Abstract

Magnetic hard materials (Pr1–xDyx)13,12–13,3(Fe1–yCoy)76,29–78,98B7,86–10,5 (x=0,40–0,58, y=0,20–0,24) for navigation devices are investigated depending on the composition and temperature of sintering. Measurements were carried out on a vibrating magnetometer on spherical samples at a temperature of 20±5 °C in magnetic fields up to 1800 kA/m. The demagnetization curves of sintered materials were measured by magnetization and induction with different cobalt and dysprosium contents. Special attention is paid to the rectangularity of the demagnetization curve depending on the composition and temperature of sintering.

Reference list
  1. Martynenko Yu.G. Trends in the development of modern gyroscopy. Sorosovskiy obrazovatelny zhurnal, 1997, no. 11, pp. 120–127.
  2. Сhirkin D.S., Roslovets P.V., Tatarinov F.V., Novikov L.Z. Reducing the drift of a dynamically tuned gyroscope from launch to launch. Inzhenerny zhurnal: nauka i innovatsii, 2017, no. 1, pp. 1–12. DOI: 10.18698/2308-6033-2017-01-1579.
  3. Topilskaya S.V., Borodulin D.S., Kornyukhin A.V. Experimental assessment of permissible mechanical influences on a dynamically adjustable gyroscope. Vestnik MGTU im. N.E. Baumana. Ser.: Priborostroenie, 2018, no. 4, pp. 69–79. DOI: 10.18698/0236-3933-2018-4-69-79.
  4. Peshekhonov V.G. Prospects for the development of gyroscopy. Giroskopiya i navigatsiya, 2020, vol. 28, no. 2, pp. 3–10. DOI: 10.1785/0869-7035-0028.
  5. Vershovsky A.K., Litmanovich Yu.A., Pazgalev A.S., Peshekhonov V.G. Nuclear magnetic resonance gyroscope. Giroskopiya i navigatsiya, 2018, vol. 26, no. 1, pp. 55–80. DOI: 10.17285/0869-7035.2018.26.1.055-080.
  6. Umarkhodzhaev R.M., Pavlov Yu.V., Vasilyeva A.N. History of the development of a gyroscope based on nuclear magnetic resonance in Russia in 1960–2000. Giroskopiya i navigatsiya, 2018, vol. 26, no. 1, pp. 3–27. DOI: 10.17285/0869-7035.2018.26.1.003-027.
  7. Korolev M.N. Research of technical characteristics of modern types of angular velocity sensors. Proc. 12th Int. scientific-technical conf. «Instrument Engineering-2019». Moscow, 2019, pp. 21–23.
  8. Pomerantsev N.M., Skrotsky G.V. Physical foundations of quantum gyroscopy. Uspekhi fizicheskikh nauk, 1970, vol. 100, is. 3, pp. 361–394.
  9. Popov A.G., Maikov V.G. Permanent magnets with radial texture from alloys based on rare earth metals. Symposium «Study of the problems of creating magnetic systems of new electric machines and the use of high-energy hard magnetic materials in them in order to improve parameters and designs». Moscow, 1991, pp. 147–157.
  10. Piskorskiy V.P., Valeev R.A., Korolev D.V., Stolyankov Yu.V., Morgunov R.B. Technologies of magneto-optical information recording in thin films of rare-earth magnetically soft alloys. Part II. Ultrafast all optical switching of magnetization. Trudy VIAM, 2020, no. 2 (86), paper no. 03. Available at: http://www.viam-works.ru (accessed: January 26, 2024). DOI: 10.18577/2307-6046-2020-0-2-10-21.
  11. Wang Y., Yu B., Feng M. et al. Magnetic properties оf Nd–Fe–Co–B permanent magnetic alloys. Journal of Applied Physics, 1987, vol. 61, pp. 3448–3450.
  12. Kablov E.N., Antipov V.V. The role of new generation materials in ensuring the technological sovereignty of the Russian Federation. Vestnik Rossiyskoy akademii nauk, 2023, vol. 93, no. 10, pp. 907–916.
  13. Foner S. Versatile and sensitive vibrating-sample magnetometer. The review of scientific instruments, 1959, vol. 30, no. 7, pp. 548–557.
  14. Lapteva K.A., Tolmachev I.I. Calculation of the demagnetizing factor during longitudinal magnetization in magnetic particle flaw detection. Izvestiya Tomskogo politekhnicheskogo universiteta, 2012, vol. 321, no. 2, pp. 140–144.
  15. Valeev R.A., Korolev D.V., Morgunov R.B., Piskorsky V.P. The effect of high concentrations of cobalt on the properties of magnets Pr–Dy–Fe–Co–B and Nd–Dy–Fe–Co–B. Trudy VIAM, 2022, no. 10 (116), paper no. 06. Available at: http://www.viam-works.ru (accessed: January 26, 2024). DOI: 10.18577/2307-6046-2022-0-10-66-75.
  16. Morgunov R.B., Piskorskiy V.P., Valeev R.A., Korolev D.V. The thermal stability of rare-earth magnets supported by means of the magnetocaloric effect. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 88–94. DOI: 10.18577/2071-9140-2019-0-1-88-94.
  17. Herbst J.F. R2Fe14B materials: intrinsic properties and technological properties and technological aspects. Reviews of Modern Physics, 1991, vol. 63 nо. 4, pp. 819–898.
  18. Morgunov R., Lu Y., Lavanant M. et al. Magnetic aftereffects in CoFeB/Ta/CoFeB spin valves of large area. Physical review B, 2017, vol. 96, p. 054421. DOI: 10.1103/PhysRevB.96.054421.
  19. Buzenkov A.V., Valeev R.A., Piskorsky V.P., Morgunov R.B. The effect of the content of yttrium on the properties of the sintered Magnets Nd–Dy–Y–Fe–Co–B. Trudy VIAM, 2022, no. 4 (110), paper no. 11. Available at: http://www.viam-works.ru (accessed: January 26, 2024). DOI: 10.18577/2307-6046-2022-0-4-108-117.
  20. Pedziwiatr A.T., Chen H.Y., Wallace W.E. Magnetism of the TbzFe14‒xCoxB system. Journal of Magnetism and Magnetic Materials, 1987, vol. 67, pp. 311–315.
  21. Fujii H., Wallace W.E., Boltich E.B. Concerning magnetic characteristics of
  22. (R2‒xR*x)Fe12Co2B (R=Pr and Nd, R*=Tb and Dy). Journal of Magnetism and Magnetic Materials, 1986, vol. 61, pp. 251–256.
  23. Givord D., Li H.S., Cadogan J.M. et al. Analysis of high-field magnetization measurements on R2Fe14B single crystals (R=Tb, Dy, Ho, Er and Tm). Journal of Applied Physics, 1988, vol. 63, pp. 3713–3715.
  24. Pedziviatr A.T., Wallace W.E. Spin reorientations in R2Fe14‒xCoxB systems (R=Pr, Nd and Er). Journal of Magnetism and Magnetic Materials, 1987, vol. 65, pp. 139–144.
  25. Akbar S., Ahmad Z., Awan M.S. et al. Development of Fe–Cr–Co permanents magnets by single step thermos-magnetic treatment. Key Engineering Materials, 2012, vol. 510–511, pp. 507–512.
  26. Sergeev V.V., Bulygina T.I. Hard magnetic materials. Moscow: Energiya, 1980, 224 p.
  27. Haavisto M., Tuominen S., Santa-Nokki T. et al. Magnetic behavior of sintered NdFeB magnets on a long-term timescale. Advances in Materials Science and Engineering, 2014, vol. 2024, art. ID 760584. DOI: 10.1155/2014/760584.
  28. Rakotoarison H.R., Yonnet J.P., Delinchant B. Using coulombian approach for modeling scalar potential and magnetic field of a permanent magnet with radial polarization. IEEE Transactions on Magnetics, 2007, vol. 43, no. 4, pp. 1261–1264.
  29. Tian J., Pan D., Zhou H. et al. Radial cracks and fracture mechanism of radially oriented ring 2:17 type SmCo magnets. Journal of Alloys and Compounds, 2009, vol. 476, pp. 98–101.
  30. Ido H., Wallace W.E., Suzuki T. et al. Magnetic and crystallographic properties of NdCo4M (M=B, Al, and Ga). Journal of Applied Physics, 1990, vol. 67, pp. 4635–4637.
  31. Hasaka M., Nakashima H., Oki K. Crystal structures of the RCo5 and R2Co17 types observed in polystyrene latexes. Transactions of the Japan Institute of Metals, 1984, vol. 25, nо. 2, pp. 73–79.
  32. Liu J., Corte-Real M., George C. et al. Magnetic hardening studies in sintered Sm(Co, Cu, Fe, Zr)z 2:17 high temperature magnets. Journal of Applied Physics, 2000, vol. 87, no. 9, pp. 6722–6724.