Resistance of aramid organic plastics to the effects of natural environment factors

Zhelezina G.F., Kulagina G.S., Kan A.Ch., Startsev V.O.
Zhelezina G.F., Kulagina G.S., Kan A.Ch., Startsev V.O. Resistance of aramid organic plastics to the effects of natural environment factors // Proceedings of VIAM. 2024. No. 5. DOI: 10.18577/2307-6046-2024-0-5-13-24. URL: https://www.viam-works.ru/en/journal/2024/5/2
Keywords
polymeric binding, organoplastics, polymeric composites, climatic aging, moisture absorption
Abstract

The climatic aging of aramid organic plastics in various natural environments is investigated. It is shown that the climatic stability of organic plastics is at the level of resistance of polymeric composite materials reinforced by carbon fibers and fiber glasses, despite the higher water absorption. Organic plastic Organit 10Т has 71 % of tensile strength properties after 18 years of climatic aging. Organic plastics can recover their properties after removal (drying) of the sorbed moisture. Organic plastics from new Rusar-NT fiber and epoxy melt binders have the biggest resistance to climatic aging.

Reference list
  1. Kablov E.N., Startsev O.V. The basic and applied research in the field of corrosion and ageing of materials in natural environments (review). Aviacionnye materialy i tehnologii, 2015, no. 4 (37), pp. 38–52. DOI: 10.18577/2071-9140-2015-0-4-38-52.
  2. Mashinskaya G.P., Perov B.V. Principles of developing organic fibre-reinforced plastics for aircraft engineering. Polymer Matrix Composites: Soviet Advanced Composites Technology. London: Chapman & Hall, 1995, pp. 305–425.
  3. Kablov E.N., Startsev O.V., Krotov A.S., Kirillov V.N. Climatic aging of composite materials for aviation purposes. I. Aging mechanisms. Deformation and destruction of materials, 2010, no. 11, pp. 19–27.
  4. Garanina S.D., Shul G.S., Lebedev L.B. et al. Effect of water on the properties of organic plastics. Mechanics of Composite Materials, 1985, vol. 20, pp. 454–457.
  5. Startsev O.V., Krotov A.S., Mashinskaya G.P. Climatic ageing of organic fiber reinforced plastics: water effect. International Journal of Polymeric Materials, 1997, vol. 37, pp. 161–171.
  6. Kurzemnieks A.K. Structural deformation properties of organic fibers based on para-polyamides. Mechanics of Composite Materials, 1979, vol. 15, pp. 7–10.
  7. Vijayan K. Effect of environmental exposure on the aramid fibre Kevlar. Metals Materials and Processes, 2000, vol. 12, pp. 259–268.
  8. Startseva L.T. Climatic ageing of organic fiber reinforced plastics. Mechanics of Composite Materials, 1984, vol. 29, pp. 620–626.
  9. Bulmanis V.N., Popov N.S., Starzhenetskaya T.A. et al. Effect of alternating thermocycling and humidity on the strength of wound glass-fiber and organic-fiber plastics. Mechanics of Composite Materials, 1989, vol. 24, pp. 782–789.
  10. Bulmanis V.N., Startsev O.V. Prediction of changes in the strength of polymer fiber composites as a result of climatic influences. Yakutsk, 1988, 32 p.
  11. Baker D.J. Ten-year ground exposure of composite materials used on the Bell model 206L helicopter flight service program: NASA Technical Paper 3468; ARL Technical Report 480. Hampton, VA, 1994, 54 p.
  12. Dexter H.B. Long-term environmental effects and flight service evaluation of composite materials: NASA TM-89067. Hampton, VA, 1987, 188 p.
  13. Haque A., Copeland C.W., Zadoo D.P., Jeelani S. Hygrothermal influence on the flexural properties of kevlar-graphite/epoxy hybrid composites. Journal of Reinforced Plastics and Composites, 1990, vol. 9, pp. 602–613.
  14. Ramesh C., Arumugam V., Stanley J., Kumar V. Effects of hydrolytic aging on glass/epoxy, kevlar/epoxy, and hybrid (glass/kevlar/epoxy) composites. International Journal of Engineering Research & Technology (IJERT), 2013, vol. 2, pp. 1589–1596.
  15. Zhelezina G.F., Voinov S.I., Pletin P.I., Veshkin E.A., Satdinov R.A. Development and production of structural organoplastics for aviation technology. Izvestiya Samarskogo nauchnogo tsentra RAN, 2012, vol. 14, no. 4, pp. 411–416.
  16. Zhelezina G.F., Gulyaev I.N., Soloveva N.A. Aramide organic plastics of new generation for aviation designs. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 368–378. DOI: 10.18577/2071-9140-2017-0-S-368-378.
  17. Zhelezina G.F., Tikhonov I.V., Chernykh T.E., Bova V.G., Voinov S.I. Third generation aramid fibers Rusar NT for reinforcing organotextolites for aviation purposes. Plasticheskiye massy, 2019, no. 3–4, pp. 43–47.
  18. Chaykun A.M., Venediktova M.A., Smirnov D.N., Gerasimov D.M. Features of the influence of atmospheric factors on the main technical characteristics of sealing materials of various types of aviation purposes. Trudy VIAM, 2019, no. 2 (74), paper no. 06. Available at: http://viam-works.ru (accessed: December 15, 2023). DOI: 10.18577/2307-6046-2019-0-2-58-67.
  19. Andreeva N.P., Pavlov M.R., Nikolaev E.V., Kurnosov A.O. Research of climatic factors influence of cold, temperate (moderate) and tropical climates on properties of construction fibreglass. Trudy VIAM, 2019, no. 3 (75), paper no. 12. Available at: http://www.viam-works.ru (accessed: November 15, 2023). DOI: 10.18577/2307-6046-2019-0-3-105-114.
  20. Kablov E.N., Laptev A.B., Prokopenko A.N., Gulyaev A.I. Relaxation of polymeric composite materials under the prolonged action of static load and climate (review). Part 1. Binders. Aviation materials and technologies, 2021, no. 4 (65), paper no. 08. Available at: http://www.journal.viam.ru (accessed: December 15, 2023). DOI: 10.18577/2071-9140-2021-0-4-70-80.
  21. Veligodskiy I.M., Koval T.V., Kurnosov A.O., Marakhovskiy P.S. Study of resistance of glass fiber reinforced plastic to natural weathering in different climatic conditions. Trudy VIAM, 2022, no. 11 (117), paper no. 12. Available at: http://www.viam-works.ru (accessed: November 24, 2023). DOI: 10.18577/2307-6046-2022-0-11-134-148.
  22. Kablov E.N. New generation materials – the basis of innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 14, pp. 16–21.
  23. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  24. Vasilyeva E.D., Vasilyeva A.A., Kychkin A.K. On the question of methods for studying the effects of moisture on polymer composite materials. Materialovedenie. Energetika, 2022, vol. 28, no. 1, pp. 21–31. DOI: 10.18721/JEST.28102.
  25. Zhang S., Karbhari V.M., Reynaud D. NOL-ring based evaluation of freeze and freeze-thaw exposure effects on FRP composite colomn wrap systems. Composites. Part B, 2001, vol. 32, pp. 589–598.
  26. Muralidharan M., Sathishkumar T.P., Rajini N. et al. Evaluation of tensile strength retention and service life prediction of hydrothermal aged balanced orthotropic carbon/glass and kevlar/glass fabric reinforced polymer hybrid composites. Journal of Applied Polymer Science, 2022, vol. 139, no. 6, p. 51602.
  27. Agarwal S., Pai Y., Pai D., Mahesha G.T. Assessment of ageing effect on the mechanical and damping characteristics of thin quasi-isotropic hybrid carbon-Kevlar/epoxy intraply composites. Cogent Engineering, 2023, vol. 10, art. 223511.