Influence of corrosion inhibitors on the microstructure and vulcanization kinetics of polysulfide sealant

Makushchenko I.S., Kozlov I.A., Smirnov D.N., Kurshev E.V., Lonskii S.L.
Makushchenko I.S., Kozlov I.A., Smirnov D.N., Kurshev E.V., Lonskii S.L. Influence of corrosion inhibitors on the microstructure and vulcanization kinetics of polysulfide sealant // Proceedings of VIAM. 2024. No. 4. DOI: 10.18577/2307-6046-2024-0-4-123-132. URL: https://www.viam-works.ru/en/journal/2024/4/9
Keywords
polymers, polysulfide sealant, corrosion inhibitors, microstructure, kinetics of vulcanization
Abstract

The article presents the results of studies of the effect of corrosion inhibitors of various chemical compositions on the time of crosslinking, the thermal effect and the structural formation of a polysulfide sealant in which they are included. The data on the dependence of the crosslinking rate of a polysulfide sealant with corrosion inhibitors on temperature and relative humidity are presented; the phase transitions and the change in the heat capacity of the sealant samples are determined; the microstructure of the sealant is investigated and its effect on the protective properties of the composition is described

Reference list
  1. Makushchenko I.S., Smirnov D.N., Kozlov I.A. Polysulfide anti-corrosion sealants and inhibitory compounds (literature review). Korroziya: zashchita, materialy, 2023, no. 1, рр. 20–25.
  2. Kablov E.N., Semenova L.V., Eskov A.A., Lebedeva T.A. Complex systems of paint and varnish coatings for the protection of metal polymer composite materials, as well as their contact connections from the effects of aggressive factors. Lakokrasochnye materialy i ikh primenenie, 2016, no. 6, рр. 32−35.
  3. Rakova T.M., Kozlova A.A., Nefedov N.I., Laptev A.B. The study of influence organic and inorganic corrosion inhibitors on the stress-corrosion cracking high-strength steels. Trudy VIAM, 2017, no. 6 (54), paper no. 12. Available at: http://www.viam-works.ru (accessed: November 24, 2023). DOI: 10.18577/2307-6046-2017-0-6-12-12.
  4. Rakhmankulov D.L., Bugai D.E., Gabitov A.I., Golubev M.V., Laptev A.B., Kalimullin A.A. Corrosion inhibitors: in 2 vols. Ufa: Reaktiv, 1997, vol. 1: Fundamentals of theory and practice of application, pp. 117–128.
  5. Rosenfeld I.L. Corrosion inhibitors. Moscow: Khimiya, 1977, 552 p.
  6. Makushchenko I.S., Kozlov I.A., Smirnov D.N., Vdovin A.I., Karachevtsev F.N. Study of the protective properties of polysulfide sealant containing corrosion inhibitors. Klei. Germetiki. Tekhnologii, 2023, no. 11, pp. 7–14. DOI: 10.31044/1813-7008-2023-0-11-7-14.
  7. Rosenfeld I.L., Rubinshtein F.I. Anti-corrosion primers and inhibited paint and varnish coatings. Moscow: Khimiya, 1980, pp. 95–112.
  8. Eliseev O.A., Bryk Ya.A., Smirnov D.N. Polysulfide sealants modification by corrosion inhibitors. Aviacionnye materialy i tehnologii, 2016, no. S2 (44), pp. 15–21. DOI: 10.18577/2071-9140-2016-0-S2-15-21.
  9. Sorokin O.Yu. On the issue of the mechanism of interaction between carbon materials and Si melt (review). Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 65–70. DOI: 10.18577/2071-9140-2015-0-1-65-70.
  10. Kablov E.N., Startsev O.V., Medvedev I.M. Review of international experience on corrosion and corrosion protection. Aviacionnye materialy i tehnologii, 2015, no. 2 (35), pp. 76–87. DOI: 10.18577/2071-9140-2015-0-2-76-87.
  11. Seleznev D.V., Kozhevnikova Yu.M., Belobrova I.A., Ishuzhin R.R., Tashlanov V.V. Method for determining the enthalpy of endo- and exothermic effects in compo-site phase-change materials based on DSC-research. Aviation materials and technologies, 2022, no. 1 (69), paper no. 11. Available at: http://www.journal.viam.ru (accessed: December 04, 2023). DOI: 10.18577/2713-0193-2022-0-4-123-131.
  12. Chalykh A.E. Diffusion in polymer systems. Moscow: Khimiya, 1987, 312 p.
  13. Bazyleva O.A., Arginbayeva E.G., Lutskaya S.A. Ways of increasing corrosion resistance of superalloys (review). Trudy VIAM, 2018, no. 4 (64), paper no. 01. Available at: http://www.viam-works.ru (accessed: November 24, 2023). DOI: 10.18577/2307-6046-2018-0-4-3-8.
  14. Zheleznyak V.G., Serdcelyubova A.S., Merkulova Yu.I., Skivko P.V. Paint coating system based on polyurethane enamel for protecting heated frontal surfaces of aviation products. Aviation materials and technologies, 2022, no. 1 (66), paper no. 10. Available at: http://www.journal.viam.ru (ассеssed: November 24, 2023). DOI: 10.18577/2713-0193-2022-0-1-120-128.
  15. Kablov E.N. New generation materials and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
  16. Kovrizhkina N.A., Kuznetsova V.A., Silaeva A.A., Marchenko S.A. Ways to improve the properties of paint coatings by adding different fillers (review). Aviacionnye materialy i tehnologii, 2019, no. 4 (57), pp. 41–48. DOI: 10.18577/2071-9140-2019-0-4-41-48.
  17. Serdtselyubova A.S., Merkulova Yu.I., Zagora A.G., Kurshev E.V. Research of film-forming
  18. parameters and protective properties of basecoat/clearcoat system. Aviation materials and technologies, 2023, no. 1 (70), paper no. 07. Available at: http://www.journal.viam.ru (accessed: December 04, 2023). DOI: 10.18577/2713-0193-2022-0-1-93-104.
  19. State Standard R 56755‒2015. Plastics. Differential scanning calorimetry (DSC). Part 5. Determination of characteristic temperatures and time from reaction curves, determination of enthalpy and degree of conversion. Moscow: Standartinform, 2016, 15 p.
  20. PPG Aerospase. P/S 870 Class C Corrosion Inhibitive Sealant. Available at: https://www.ppgaerospase.com/Products/Sealants/Corrosion-Inhibitive/P-S-870-Class-C-Corrosion-Inhibitive-Sealant (accessed: December 04, 2023).
  21. Sitnikova V.E., Ponomareva A.A., Uspenskaya M.V. Methods of thermal analysis: workshop. St. Petersburg: ITMO University, 2021, 152 p.
  22. Valeev R.R. Highly filled sealing compositions based on polysulfide oligomers: thesis abstract, Cand. Sc. (Tech.), Kazan, 2004, 16 p.
  23. Kayushnikov S.N., Prokopchuk N.R., Use E.P., Alfimov I.V. Study of the influence of zinc-containing technological additives on the technical properties of rubber. Vestnik tekhnologicheskogo universiteta, 2017, vol. 20, no. 6, pp. 36‒40.
  24. Fiaud C. Theory and Practice of Vapour Phase Inhibitors. A Working Party Report on Corrosion Inhibitors. London: The Institute of Materials, 1994, pp. 1–11.
  25. Kozlova A.A., Kondrateva O.V., Kuznetsova V.A. The main problems of using domestically produced moisture-proof electrical insulating materials for automated selective application on printed assemblies (review). Aviation materials and technologies, 2022, no. 4 (69), paper no. 07. Available at: http://www.journal.viam.ru (accessed: November 30, 2023). DOI: 10.18577/2713-0193-2022-0-4-72-83.