Comprehensive assessment of the impact of operational and climatic tests on the change of strength properties of polymer composite materials based on adhesive prepregs
Part 2. Glass fiber-reinforced plastic VPS-68
Starkov A.I., Isaev A.Yu., Kutsevich K.E. Comprehensive assessment of the impact of operational and climatic tests on the change of strength properties of polymer composite materials based on adhesive prepregs. Part 2. Glass fiber-reinforced plastic VPS-68 // Proceedings of VIAM. 2024. No. 4. DOI: 10.18577/2307-6046-2024-0-4-98-107. URL: https://www.viam-works.ru/en/journal/2024/4/7
Keywords
glass fiber-reinforced plastic, adhesive prepreg, adhesive joints, tensile strength, compression strength, flexural strength, interlayer shear strength, influence of external factors
Abstract
A comprehensive assessment of the retention of the strength properties of fiberglass VPS-68 for tension, compression, bending, interlayer shear was carried out at test temperatures of –60, +20, +80 and +105 °C in the initial state and after climatic influences in a tropical climate chamber for 1 and 3 months, thermal aging for 500 and 1000 hours, exposure to mycological environments and technical fluids. To confirm viability, samples of VPS-68 fiberglass were tested in tension and compression
Reference list
- Satdinov R.A., Veshkin E.A., Postnov V.I. Assessment of the impact of climatic factors on the performance properties of fiberglass VPS-42P/T-64. Trudy VIAM, 2020, no. 10 (92), paper no. 03. Available at: http://www.viam-works.ru (accessed: August 20, 2023). DOI: 10.18577/2307-6046-2020-0-10-21-29.
- Starkov A.I., Kutsevich K.E., Tyumeneva T.Yu., Petrova A.P. Low-combustibility adhesive prepregs designed for the manufacture of integral and three-layer honeycomb struc-tures aircraft technology. Trudy VIAM, 2022, no. 5 (111), paper no. 04. Available at: http://www.viam-works.ru (accessed: August 20, 2023). DOI: 10.18577/2307-6046-2022-0-4-41-52.
- Kablov E.N. New generation materials and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
- Kablov E.N., Chursova L.V., Babin A.N., Mukhametov R.R., Panina N.N. Developments of FSUE «VIAM» in the field of melt binders for polymer composite materials. Polimernye materialy i tekhnologii, 2016, vol. 2, no. 2, pp. 37–42.
- Aviation materials: reference book in 13 vols. Ed. E.N. Kablov. 7th ed., rev. and add. Moscow: VIAM, 2019, vol. 10: Adhesives, sealants, rubbers, hydraulic fluids, part 1: Adhesives, adhesive prepregs, 276 p.
- Kablov E.N., Startsev V.O. Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review).
- Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 47–58. DOI: 10.18577/2071-9140-2018-0-2-47-58.
- Vavilova M.I., Kavun N.S. The properties of glass filler for constructions of fiberglass. Aviacionnye materialy i tehnologii, 2014, no. 3, pp. 33–37. DOI: 10.18577/2071-9140-2014-0-3-33-37.
- Volnov O.I., Dudukin D.O. Fiberglass. History of development, production technology, shaping of parts and modern application. Trudy NGTU im. R.Ye. Alekseyeva, 2014, no. 5 (107),
- pp. 400–404.
- Bolshakov V.A., Antyufeeva N.V. Evaluation of the curing process model of the adhesive binder in prepreg. Aviation materials and technologies, 2023, no. 4 (73), paper no. 07. Available at: http://www.journal.viam.ru (accessed: October 20, 2023). DOI: DOI: 10.18577/2713-0193-2023-0-4-66-77.
- Petrova A.P., Malysheva G.V. Adhesives, adhesive binders and adhesive prepregs: allowance. Ed. E.N. Kablov. Moscow: VIAM, 2017, 472 p.
- Perov N.S. Design of polymeric materials on the molecular principles. II. The molecular mobility in the cross-linked complex systems. Aviacionnye materialy i tehnologii, 2017, no. 4 (49), pp. 30–36. DOI: 10.18577/2071-9140-2017-0-4-30-36.
- Laptev A.B., Barbotko S.L., Nikolaev E.V. The main research areas of the persistence properties of materials under the influence of climatic and operational factors. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 547–561. DOI: 10.18577/2071-9140-2017-0-S-547-561.
- Isaev A.Yu., Rubtsova E.V., Kotova E.V., Sutyagin M.N. Research of properties of glues and glue binding, made with use of modern domestic component base. Trudy VIAM, 2021, no. 3 (97), paper no. 05. Available at: http://www.viam-works.ru (accessed: October 18, 2023). DOI: 10.18577/2307-6046-2021-0-3-58-67.
- Lukina N.Ph., Petrova A.P., Muhametov R.R., Kogtjonkov A.S. New developments in the field of adhesive aviation materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 452–459. DOI: 10.18577/2071-9140-2017-0-S-452-459.
- Khrychev Yu.I., Shkodinova E.P., Dementieva L.A. Development of a technological process for manufacturing a radio-transparent radome from adhesive prepregs of the KMKS-2m.120 type. Collection report conf. «Adhesive materials for aviation purposes». Moscow: VIAM, 2013, pp. 43–47.