Implementation of technology for chemical vapor deposition of silicon carbide in electronics

Part 1
Sidorov D.V., Grunin А.А., Shavnev A.A.
Sidorov D.V., Grunin А.А., Shavnev A.A. Implementation of technology for chemical vapor deposition of silicon carbide in electronics. Part 1 // Proceedings of VIAM. 2024. No. 3. DOI: 10.18577/2307-6046-2024-0-3-101-116. URL: https://www.viam-works.ru/en/journal/2024/3/9
Keywords
silicon carbide, electronics, semiconductor, chemical vapor deposition, methods of growing crystals, epitaxy
Abstract

The comparative characteristics of modern semiconductor materials, the basic electrophysical properties of the applied silicon carbide polytypes, and the possibilities of using silicon carbide semiconductors in microelectronic devices are presented. The most common methods for producing silicon carbide crystals are considered, which are growing crystals from a melt, sublimation and chemical vapor deposition.

Reference list
  1. Kablov E.N., Echin A.B., Bondarenko Yu.A. History of development of directional crystallization technology and equipment for casting blades of gas turbine engines. Trudy VIAM, 2020, no. 3 (87), paper no. 01. Available at: http://www.viam-works.ru (accessed: December 18, 2023). DOI: 10.18577/2307-6046-2020-0-3-3-12.
  2. Kablov E.N., Semenova S.N., Suleymanov R.R., Chaykun A.М. Prospects for the use of ethylene-propylene-diene rubber as part of cold resistant rubber. Trudy VIAM, 2019, no. 12 (84), paper no. 04. Available at: http://www.viam-works.ru (accessed: December 18, 2023). DOI: 10.18577/2307-6046-2019-0-12-29-36.
  3. Kablov E.N., Valueva M.I., Zelenina I.V., Khmelnitskiy V.V., Aleksashin V.M. Carbon plastics based on benzoxazine oligomers – perspective materials. Trudy VIAM, 2020, no. 1 (85), paper no. 07. Available at: http://www.viam-works.ru (accessed: December 18, 2023). DOI: 10.18577/2307-6046-2020-0-1-68-77.
  4. She X., Huang A., Lucia O. et al. Review of silicon carbide power devices and their applications. IEEE Transactions on Industrial Electronics, 2017, vol. 64, pp. 8193–8205.
  5. Maddi H., Yu S., Zhu S. et al. The road to a robust and affordable SiC power MOSFET technology. Energies, 2021, vol. 14, p. 8283.
  6. Harris G. Properties of silicon carbide. INSPEC. Institution of Electrical Engineers, 1995, p. 118.
  7. Davis R., Kelner G., Shur M. et al. Thin film deposition and microelectronic and optoelectronic device fabrication and characterization in monocrystalline alpha and beta silicon carbide. Proceedings of the IEEE, 1991, vol. 79, pp. 677–701.
  8. Kimoto T. Material science and device physics in SiC technology for high-voltage power devices. Japanese Journal of Applied Physics, 2015, vol. 54, p. 040103.
  9. Cooper J., Agarwal A. SiC Power-Switching Devices – The Second Electronics Revolution? Proceedings of the IEEE, 2002, vol. 90, pp. 956–968.
  10. Pensl G., Clobanu F., Frank T. et al. SiC material properties. International Journal of High Speed Electronics and Systems, 2005, vol. 4, pp. 705–745.
  11. Bechstedt F., Käckell P., Zywietz A. et al. Polytypism and Properties of Silicon Carbide. Physica Status Solidi, 1997, vol. 202, pp. 35–62.
  12. Powell A., Rowland L. SiC Materials – progress, status, and potential roadblocks. Proceedings of the IEEE, 2002, vol. 90, pp. 942–955.
  13. Elasser A., Chow T. Silicon carbide benefits and advantages for power electronics circuits and systems. Proceedings of the IEEE, 2002, vol. 90, pp. 969–986.
  14. Friedrichs P. Silicon carbide power-device products – Status and upcoming challenges with a special attention to traditional, nonmilitary industrial applications. Physica Status Solidi, 2008, vol. 245, pp. 1232–1238.
  15. Liu L., Wu J., Ren N. 1200-V 4H–SiC merged p-i-n Schottky diodes with high avalanche capability. IEEE Transactions on Electron, 2020, vol. 67, pp. 3679–3684.
  16. Li P., Guo J., Lin Z. A Power MOSFET with P-base Schottky diode and built-in channel diode for fast reverse recovery. IEEE Journal of the Electron Devices Society, 2021, vol. 9, pp. 300–305.
  17. Rodriguez G.A., Gill L., Mueller J.A. Cascaded SiC JFET topology for high-voltage solid-state circuit breaker applications. IEEE Transactions on Industry Applications, 2022, vol. 59, pp. 2326–2339.
  18. Agamy M., Tao F., Elasser A. High speed medium voltage SiC thyristors for pulse power applications. IEEE Transactions on Industry Applications, 2021, vol. 57, pp. 3812–3821.
  19. Hofmann D., Muller M. Prospects of the use of liquid phase techniques for the growth of bulk silicon carbide crystals. Materials Science and Engineering, 1999, vol. 61, рр. 29–39.
  20. Syväyärvi M., Yakimova R., Radamson H.H. et al. Liquid phase epitaxial growth of SiC. Journal of Crystal Growth, 1999, vol. 197, pp. 147–154.
  21. Kamei K., Kusunoki K., Yashiro N. et al. Solution growth of single crystalline 6H, 4H–SiC using Si–Ti–C melt. Journal of Crystal Growth, 2009, vol. 311, pp. 855–858.
  22. Yamamoto Y., Harada S., Seki K. et al. High-efficiency conversion of threading screw dislocations in 4H–SiC by solution growth. Applied Physics Express, 2012, vol. 5, pp. 5501–5504.
  23. Danno K., Shirai T., Seki A. et al. Solution growth on 4H–SiC (1100) for lowering density of threading dislocations. Presented at 15th International Conference on Defects Recognition, Imaging and Physics in Semiconductors. Warsaw, 2013, p. 235.
  24. Lely J. Darstellung voneinkristallen von silicium carbide und beherrschung von art und menge der eingebauten verunreinigungen. Berichte der deuchen keramischen gesellschaft, 1955, vol. 32, pp. 229–236.
  25. Tairov Y., Tsvetkov V. General principles of growing large-size single crystals of various silicon carbide polytypes. Journal of Crystal Growth, 1981, vol. 52, pp. 146–150.
  26. Jokubavicius V., Sun J., Liu X. et al. Growth optimization and applicability of thick on-axis SiC layers using sublimation epitaxy in vacuum. Journal of Crystal Growth, 2016, vol. 478, pp. 159–162.
  27. Burk A., Rowland L. Homoepitaxial VPE growth of SiC active layers. Physica Status Solidi, 1997, vol. 202, pp. 263–279.
  28. Kimoto T., Itoh A., Matsunami H. Step-controlled epitaxial growth of high-quality SiC layers. Physica Status Solidi, 1997, vol. 202, pp. 247–262.
  29. Rupp R., Makarov Y., Behner H., Wiedenhofer A. Silicon carbide epitaxy in a vertical CVD reactor: experimental results and numerical process simulation. Physica Status Solidi, 2005, vol. 202, pp. 281–304.
  30. Landini B.E., Brandes G.R. Characteristics of homoepitaxial 4H–SiC films grown on c-axis substrates offcut towards 1100> or 1120>. Applied Physics Letters, 1999, vol. 74, pp. 2632–2634.
  31. Kordina O., Hallin C., Henry A. et al. Growth of SiC by «Hot-Wall» CVD and HTCVD. Physica Status Solidi, 1997, vol. 202, pp. 321–334.
  32. Henry A., Hassan J., Bergman J.P. et al. Thick silicon carbide homoepitaxial layers grown by CVD techniques. Chemical Vapor Deposition, 2006, vol. 12, pp. 475–482.
  33. La Via F., Izzo G., Mauceri M. et al. 4H–SiC epitaxial layer growth by trichlorosilane (TCS). Journal of Crystal Growth, 2008, vol. 311, pp. 107–113.
  34. Hagasawa H., Yagi K., Kawahara T. et al. Hetero- and homo-epitaxial growth of 3C–SiC for MOS-FETs. Microelectronic Engineering, 2006, vol. 83, pp. 185–188.
  35. Ellison A., Zhang J., Henry A., Janzén E. Epitaxial growth of SiC in a chimney CVD reactor. Journal of Crystal Growth, 2002, vol. 236, pp. 225–238.
  36. Latha H., Udayakumar A., Prasad V. Microstructure and electrical properties of nitrogen doped 3C–SiC thin films deposited using methyltrichlorosilane. Materials Science in Semiconductor Processing, 2015, vol. 29, pp. 117–123.
  37. Ellison A., Zhang J., Peterson J. et al. High temperature CVD growth of SiC. Materials Science and Engineering, 1999, vol. 62, pp. 113–120.
  38. Kito Y., Makino E., Ikeda K. et al. SiC HTCVD simulation modified by sublimation etching. Materials Science Forum, 2006, vol. 527–529, pp. 107–110.
  39. Fanton M., Snyder D., Weiland B. et al. Growth of nitrogen-doped SiC boules by halide chemical vapor deposition. Journal of Crystal Growth, 2006, vol. 287, pp. 359–362.
  40. Sidorov D.V., Shavnev A.A., Melentev A.A. Formation of silicon carbide coatings by chemical vapor deposition (review). Part 2. Trudy VIAM, 2022, no. 2 (108), paper no. 07. Available at: http://www.viam-works.ru (accessed: December 18, 2023). DOI: 10.18577/2307-6046-2022-0-2-88-89.