Magnesium ion batteries: prospects and challenges in the field of energy

Leonov A.A., Trofimov N.V.
Leonov A.A., Trofimov N.V. Magnesium ion batteries: prospects and challenges in the field of energy // Proceedings of VIAM. 2024. No. 3. DOI: 10.18577/2307-6046-2024-0-3-41-51. URL: https://www.viam-works.ru/en/journal/2024/3/4
Keywords
magnesium alloys, battery, anode, electrolyte, cathode
Abstract

New type of the energy carrier include magnesium-ion batteries, which represents potentially more effective and ecologically safe alternative to existing storage technologies. The main types of anode, cathode and electrolyte materials for magnesium-ion batteries, ensuring efficient transfer of Mg2+ cations and possible cyclic durability, are considered. In the article advantages and disadvantages of this technology, its potential for application in different areas also are analyzed.

Reference list
  1. Zhang J., Roumeliotis I., Zhang X., Zolotas A. Techno-economic-environmental evaluation of aircraft propulsion electrification: Surrogate-based multi-mission optimal design approach. Renewable and Sustainable Energy Reviews, 2023, vol. 175, pp. 442–464.
  2. Emmanouil K. Reliability in the era of electrification in aviation: A systems approach. Microelectronics Reliability, 2020, vol. 114, pp. 77–82.
  3. Kablov E.N. Aviation materials science in the 21st century. Prospects and objectives. Aviation materials. Selected works of VIAM 1932–2002. Moscow: MISIS – VIAM, 2002, pp. 23–47.
  4. Kablov E.N. Modern materials – the basis of innovative modernization of Russia. Metally Evrazii, 2012, no. 3, pp. 10–15.
  5. Salem K.A., Polaia G., Quarta A.A. Review of hybrid-electric aircraft technologies and designs: Critical analysis and novel solutions. Progress in Aerospace Sciences, 2023, vol. 141, pp. 89–113.
  6. Liu Yu., Song Yu., Gao Z., Li L. Analysis of the immersion cooling of electric motors for hybrid aircraft. Progress Safety and Environmental Protection, 2023, vol. 178, pp. 404–416.
  7. Gimenez F.R., Keutenedjian Mady C.E., Henriques I.B. Assessment of different more-electric and hybrid-electric configurations for long-range multi-engine aircraft. Journal of Cleaner Production, 2023, vol. 392, pp. 321–338.
  8. Sziroczak D., Jankovics I., Gal I., Rohacs D. Conceptual design of small aircraft with hybrid-electric propulsion system. Energy, 2020, vol. 204, pp. 289–329.
  9. Park J., Lee D., Lim D., Yee K. A refined sizing method of fuel cell-battery hybrid system for eVTOL aircraft. Applied Energy, 2022, vol. 328, pp. 232–249.
  10. Xu R., Gao X., Chen Ya et al. Research advances of the electrolytes for rechargeable magnesium ion batteries. Materials Today Physics, 2023, no. 36, pp. 116–133.
  11. Li R., Zhang R., Liu Q. et al. Bifunctional non-nucleophilic electrolyte enables long-life magnesium batteries via elimination of passive film on Mg anode. Chemical Engineering Journal, 2023, no. 462, pp. 67–81.
  12. Moselhy M.A., Farrag M., Zhu Y., Sheha E. Probing the effect of ethylene carbonate on optimizing the halogen-free electrolyte performance for Mg sulfur batteries. Royal Society of Chemistry, 2023, no. 13, pp. 228–232.
  13. Rashad M., Asif M., Ahmed I. et al. Quest for carbon and vanadium oxide based rechargeable magnesium-ion batteries. Journal of Magnesium and Alloys, 2020, vol. 8, pp. 364–373.
  14. Dominko R., Bitenc J., Berthelot R. et al. Magnesium batteries: Current picture and missing pieces of the puzzle. Journal of Power Sources, 2020, no. 478, pp. 321–339.
  15. Kablov E.N. Chemistry in aviation materials science. Rossiyskiy khimicheskiy zhurnal, 2010, vol. LIV, no. 1, pp. 3–4.
  16. Bagotsky V.S. Basics of electrochemistry. Moscow: Khimiya, 1988, 400 p.
  17. Fomina M.A., Volkov I.A., Vdovin A.I., Yamshchikov E.I. Study of protective capacity anodic oxide coating with environmental friendly improved filling technology. Aviation materials and technologies, 2023, no. 4 (73), paper no. 10. Available at: http://www.journal.viam.ru (accessed: January 16, 2024). DOI: 10.18577/2713-0193-2023-0-4-101-110.
  18. Shi M., Li T., Shang H. et al. A critical review of inorganic cathode materials for rechargeable magnesium ion batteries. Journal of Energy Storage, 2023, no. 68, pp. 216–228.
  19. Deivanayagam R., Ingram B.J., Shahbazian-Yassar R. Progress in development of electrolytes for magnesium batteries. Energy Storage Materials, 2019, no. 21, pp. 136–153.
  20. Ma B., Ouyang L., Zheng J. Magnesium-rare earth intermetallic compounds for high performance high power aqueous Magnesium-Air batteries. Journal of Magnesium and Alloys, 2023, no. 4, рр. 76–90. DOI: 10.1016/j.jma.2023.06.010.
  21. Lia Q., Xiong W., Yu M. et al. Effect of Ce content on performance of AZ31 magnesium alloy anode in air battery. Journal of Alloys and Compounds, 2021, vol. 891 (4), pp. 132–141. DOI:10.1016/j.jallcom.2021.161914.
  22. Kablov E.N., Akinina M.V., Volkova E.F., Mostyaev I.V., Leonov A.A. The research of aspects of phase composition and fine structure of magnesium alloy ML9 in the as-cast and heat-treated conditions. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 17–24. DOI: 10.18577/2071-9140-2020-0-2-17-24.
  23. Miao X., Yang J., Pan W. et al. Graphite fluoride as a cathode material for primary magnesium batteries with high energy density. Electrochimica Acta, 2016, vol. 210, pp. 704–711.
  24. Giraudet J., Claves D., Guerin K. et al. Magnesium batteries: towards a first use of graphite fluorides. Journal of Power Sources, 2007, vol. 173, is. 8, pp. 595–598.
  25. Lee M., Jeong M., Nam Y.S. et al. Nitrogen-doped graphitic mesoporous carbon materials as effective sulfur imbibition hosts for magnesium-sulfur batteries. Journal of Power Sources, 2022, vol. 535, pp. 444–462.
  26. Mana Y., Jaumaux P., Xu Y. et al. Research development on electrolytes for magnesium-ion batteries. Science Bulletin, 2023, no. 68, pp. 1819–1842.
  27. Das A., Balakrishnan N.T.M., Sreeram P. et al. Prospects for magnesium ion batteries: A compreshensive materials review. Coordination Chemistry Reviews, 2024, vol. 502, pp. 118–129.
  28. Higashi S., Miwa K., Aoki M., Takechi K. A novel inorganic solid-state ion conductor for rechargeable Mg batteries. ChemCommun, 2014, no. 50, pp. 1320–1322. DOI: 10.1039/c3cc47097k.
  29. Yamanaka T., Hayashi A., Yamauchi A., Tatsumisago M. Preparation of magnesium ion conducting MgS–P2S5–MgI2 glasses by a mechanochemical technique. Solid State Ionics, 2014, no. 262, pp. 601–603. DOI: 10.1016/j.ssi.2013.10.037.
  30. Halim Z.A., Adnan S.B.R.S., Mohamed N.S. Effect of sintering temperature on the structural, electrical and electrochemical properties of novel Mg0,5Si2(PO4)3 ceramic electrolytes. Ceramics International, 2016, no. 42, pp. 4452–4461.
  31. Ikeda S., Takahashi M., Ishikawa J., Ito K. Solid electrolytes with multivalent cation conduction: 1. Conducting species in Mg–Zr–PO4 system. Solid State Ionics, 1987, no. 23, pp. 125–129.
  32. Canepa P., Bo S.H., Sai Gautam G. et al. High magnesium mobility in ternary spinel chalcogenides. Nature Communications, 2017, no. 8, pp. 1759. DOI: 10.1038/s41467-017-01772-1.
  33. Kotobuki M., Yan B., Lu L. Recent progress on cathode materials for rechargeable magnesium batteries. Energy Storage Materials, 2023, vol. 54, pp. 227–253.
  34. Voronov V.A., Chaynikova A.S., Tkalenko D.M. Aspects of usage of organic or aqueous binders based on III or IV group elements oxides in the production of ceramic molds for chemically active alloys casting (review). Aviation materials and technologies, 2021, no. 2 (63), paper no. 08. Available at: http://www.journal.viam.ru (accessed: January 22, 2024). DOI: 10.18577/2713-0193-2021-0-2-73-84.
  35. Zhang X., Li D., Ruan Q. et al. Vanadium-based cathode materials for rechargeable magnesium batteries. Materials Today Energy, 2023, no. 32, pp. 169–199.
  36. Kozlov I.A., Vinogradov S.S., Tarasova K.G., Kulyushina N.V., Manchenko V.A. Plasma electrolytic oxidation of magnesium alloys (review). Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 23–36. DOI: 10.18577/2071-9140-2019-0-1-23-36.
  37. Chen S., Fan S., Li H. et al. Recent advances in kinetic optimizations of cathode materials for rechargeable magnesium batteries. Coordination Chemistry Reviews, 2022, no. 466, pp. 4–15.