Standard measurements of dielectric properties of solid composite materials at low frequencies by contact and non-contact methods

Akzigitov V.A., Beljaev А.А., Kurnosov A.O., Payarel S.M.
Akzigitov V.A., Beljaev А.А., Kurnosov A.O., Payarel S.M. Standard measurements of dielectric properties of solid composite materials at low frequencies by contact and non-contact methods // Proceedings of VIAM. 2024. No. 2. DOI: 10.18577/2307-6046-2024-0-2-116-128. URL: https://www.viam-works.ru/en/journal/2024/2/12
Keywords
dielectric properties, permittivity, dielectric loss angle tangent, capacitor
Abstract

The article is devoted to the issues in the field of measuring the dielectric properties (permittivity and the tangent of the dielectric loss angle) of solid non-metallic materials using parallel plates (capacitor) at low frequencies. Two main methods (contact and non-contact), devices, equipment and software for measuring the permittivity and the tangent of the dielectric loss angle of solid non-metallic materials are described. The corresponding frequency ranges in which it is possible to measure the dielectric properties of solid non-metallic materials by the capacitor method are given.

Reference list
  1. Getman A.A. Main directions of development of materials science for the creation of new technology. Armaturostroenie, 2021, no. 4 (133), pp. 48–51.
  2. Tarasov F.I., Orlova N.Yu. Polymer materials. Current state, application and development prospects. Scientific session of NRNU MEPhI-2020 in the direction of «Innovative nuclear technologies»: reports All-Russian Conf. Moscow: NRNU MEPhI, 2020, pp. 75–77.
  3. Kablov E.N. The role of fundamental research in the creation of new generation materials. Report XXI Mendeleev Congress on General and Applied Chemistry: in 6 vol. St. Petersburg, 2019, vol. 4, р. 24.
  4. Kablov E.N. Composites: today and tomorrow. Metally Evrazii, 2015, no. 1, pp. 36–39.
  5. Kablov E.N. Main results and directions of development of materials for advanced aviation technology. 75 years. Aviation materials. Moscow: VIAM, 2007, pp. 20–26.
  6. Landau L.D., Lifshits E.M. Theoretical physics: textbook for univ.: in 10 vols. Moscow: Fizmatlit, 2005, vol. VIII: Electrodynamics of continuous media, 370 p.
  7. Nikolsky V.V., Nikolskaya T.I. Electrodynamics and propagation of radio waves: textbook for univ. 3rd. ed. Moscow: Nauka, 1989, 544 p.
  8. Dyakonov V. Keysight PNA circuit analyzers – a breakthrough in the field of microwaves and microwaves. Komponenty i tekhnologii, 2015, no. 2 (163), pp. 103–112.
  9. Korenev A.V., Goshin G.G. Measurement of the effective dielectric constant of support washers of coaxial connectors. SVCH-tekhnika i telekommunikatsionnyye tekhnologii, 2021, no. 3, pp. 332–333.
  10. Korenev A.V., Goshin G.G. Taking into account parasitic effects when measuring the effective dielectric constant using the quarter-wave resonator method. Ural Radio Engineering Journal, 2021, vol. 5, no. 3, pp. 272–283. DOI: 10.15826/urej.2021.5.3.005.
  11. Bezhko M. Changing the parameters of materials in the microwave range using software for analyzing the parameters of materials Keysight N1500A. Tekhnologii v elektronnoy promyshlennosti, 2015, no. 8 (84), pp. 64–68.
  12. Bezhko M. Measuring parameters of materials in the microwave range using Keysight N1500A. Problems of microwave electronics: reports II All-Rus. United Scientific. conf. Moscow, 2015, pp. 6–8.
  13. Inozemtsev M.A. Review of methods for measuring the dielectric constant of rocks. Electronic means and control systems: reports Intl. scientific-practical conf. Moscow, 2020, no. 1–1, pp. 279–281.
  14. Donchenko A.V., Zargano G.F., Zemlyakov V.V., Kleshchenkov A.B. Measurement of the complex dielectric constant of materials based on a ridge waveguide. Radiotekhnika i elektronika, 2020, vol. 65, no. 5, pp. 427–433. DOI: 10.31857/S0033849420050022.
  15. Ivanov V.A., Sherimov D., Tokarev I.A., Repin V.A. Methodology for measuring the dielectric properties of materials at a frequency of 2.45 GHz. Elektronika i mikroelektronika SVCH, 2021, vol. 1, pp. 595–599.
  16. Klepikova A.S., Charikova T.B., Popov M.R. et al. Anisotropy of magnetic properties and dielectric constant of Nd1.9Ce0.1CuO4+δ single crystal. Fizika metallov i metallovedenie, 2021, vol. 122, no. 5, pp. 520–526. DOI: 10.31857/S0015323021050065.
  17. Parkhomenko M.P., Kalenov D.S., Eremin I.S. et al. Improving the accuracy of measurements of complex dielectric and magnetic permeabilities in the microwave range using the waveguide method. Radiotekhnika i elektronika, 2020, vol. 65, no. 8, pp. 764–768. DOI: 10.31857/S0033849420080112.
  18. Pevneva N.A., Kondrashov D.A., Gursky A.L., Gusinsky A.V. Determination of S-parameters and dielectric constant of quartz ceramic samples in the millimeter wavelength range. Doklady Belorusskogo gosudarstvennogo universiteta informatiki i radioelektroniki, 2021, vol. 19, no. 7, pp. 65–71. DOI: 10.35596/1729-7648-2021-19-7-65-71.
  19. Pevneva N.A., Gursky A.L. Uncertainty of the results of measurements of the dielectric constant of materials using the Nicholson–Ross–Weir method. Metrologiya i priborostroyenie, 2021, no. 4 (95), pp. 25–29.
  20. Sonnov N.V., Leukhin S.A. Study of dielectric properties of structural radio-absorbing materials. Elektronika i mikroelektronika SVCH, 2021, vol. 1, pp. 347–350.
  21. Usanov D.A., Nikitov S.A., Skripal A.V. et al. Using a microwave coaxial Bragg structure to measure the parameters of dielectrics. Radiotekhnika i elektronika, 2020, vol. 65, no. 5, pp. 495–503. DOI: 10.31857/S0033849420040099.
  22. Kharalgin S.V., Voitovich M.I. Study of dielectric characteristics of materials manufactured using additive technologies. Rossiyskiy tekhnologicheskiy zhurnal, 2021, vol. 9, no. 2 (40), pp. 57–65. DOI: 10.32362/2500-316X-2021-9-2-57-65.
  23. Chukhlanov V.Yu., Smirnova N.N., Smirnov K.V. Dielectric characteristics of epoxy resin modified with tetraethoxysilane in the millimeter range. Butlerovskiye soobshcheniya, 2020, vol. 62, no. 4, pp. 77–80. DOI: 10.37952/ROI-jbc-01/20-62-4-77.
  24. Panferov S.Yu. On the issue of measuring the humidity of thin layers of material using the reflective microwave method. APK Russii, 2017, vol. 24, no. 2, pp. 498–502.
  25. Atamasov V.V., Malenkov G.I. Measuring the dielectric constant of materials by the capacitor method using the Ni ELVIS II+ and Labview hardware and software complex. Sbornik izbrannykh statey nauchnoy sessii TUSUR. Tomsk: TUSUR, 2019, no. 1–1, pp. 96–98.
  26. Zhukov A.A., Zhuravlev V.A., Atamasov V.V., Malenko G.I. Hardware and software complex on the Agilent E4285A-LabVIEW platform for measuring the dielectric constant of materials using the capacitor method. Current problems of radiophysics APR-2021: reports IX Int. scientific-practical conf. Tomsk: NI TSU, 2021, pp. 254–256.
  27. Ivanitsa M.G., Testov I.O. Development and creation of measuring cells for studying dielectric constant. Nauka nastoyashchego i budushchego, 2019, vol. 3, pp. 87–90.
  28. Korotkova T.N., Korotkov L.N., Pankova M.A. Dielectric properties of fullerites c60–c70 and the possibility of using materials in radio-electronic components. Vestnik Voronezhskogo instituta MVD Rossii, 2021, no. 1, pp. 169–174.
  29. Shakirzyanov R.I., Kostishin V.G., Morchenko A.T. et al. Synthesis and study of the properties of radio-absorbing composite films consisting of Mn0.5792Zn0.2597Fe2.1612O4 inclusions and a polymer matrix –[(CH2–CH2)m–(CF2–CF2)n]k–. Zhurnal neorganicheskoy khimii, 2020, vol. 65, no, 6, pp. 758–763. DOI: 10.31857/S0044457X20060197.
  30. Semenova S.N., Chaykun A.M., Suleymanov R.R. Ethylene-propylene-diene rubber and its use in rubber materials for special purposes (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 23–30. DOI: 10.18577/2071-9140-2019-0-3-23-30.
  31. Mishurov K.S., Kurnosov A.O., Payarel S.M. Сalculation and experimental determination of dielectric characteristics of fiberglass based on a phthalonitrile matrix. Aviation materials and technologies, 2023, no. 2 (71), paper no. 07. Available at: http://www.journal.viam.ru (accessed: June 01, 2023). DOI: 10.18577/2713-0193-2023-0-2-85-93.
  32. Tkachuk A.I., Terekhov I.V., Gurevich Ya.M., Kudryavtseva A.N. Application of bismaleimide VST-57 binder for obtaining heat-resistant dimensionally stable molds from polymer composite materials. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 32–40. DOI: 10.18577/2071-9140-2020-0-2-32-40.
  33. Serdtselyubova A.S., Merkulova Yu.I., Zagora A.G., Kurshev E.V. Research of film-forming parameters and protective properties of basecoat/clearcoat system. Aviation materials and technologies, 2023, no. 1 (70), paper no. 07. Available at: http://www.journal.viam.ru (accessed: August 18, 2023). DOI: 10.18577/2713-0193-2022-0-1-93-104.