High-temperature carbon fiber reinforced plastics based on polyimide binders

Valueva M.I., Zelenina I.V., Nacharkina A.V., Sidorina A.I., Slavin A.V.
Valueva M.I., Zelenina I.V., Nacharkina A.V., Sidorina A.I., Slavin A.V. High-temperature carbon fiber reinforced plastics based on polyimide binders // Proceedings of VIAM. 2024. No. 11. DOI: 10.18577/2307-6046-2024-0-11-71-88. URL: https://www.viam-works.ru/en/journal/2024/11/6
Keywords
high-temperature polymer composite materials, high-temperature carbon fiber reinforced plastics, polyimide binders, market, technologies, trends
Abstract

The article presents an up-to-date review of scientific and technical information in the field of development and research of high-temperature carbon fiber reinforced plastics based on thermosetting polyimide binders and their manufacturing technology. The article considers the world market of polyimide binders and carbon fiber reinforced plastics based on them, the features of the production of carbon fiber reinforced plastics based on polyimide binders, their properties and application, studies publication activity, global development trends and the main areas of research in this area.

Reference list
  1. Kablov E.N., Antipov V.V. The Role of New Generation Materials in Ensuring the Technological Sovereignty of the Russian Federation. Vestnik Rossiyskoy akademii nauk, 2023, vol. 93, no. 10, pp. 907–916.
  2. Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), paper no. 10. Available at: http://www.journal.viam.ru (accessed: August 31, 2024). DOI: 10.18577/2713-0193-2023-0-2-122-144.
  3. Mikhailin Yu.A. Heat-resistant polymers and polymeric materials. St. Petersburg: Profession, 2006, 624 p.
  4. Hergenrother P. The use, design, synthesis, and properties of high performance/high temperature polymers: an overview. High Performance Polymers, 2003, vol. 15, pp. 3–45.
  5. Mangalgiri P.D. Polymer-matrix composites for high-temperature applications. Defense Science Journal, 2005, vol. 55, pp. 175–193.
  6. High Temperature Composite Resin Market Size and Forecast. Available at: https://www.verifiedmarketresearch.com/product/high-temperature-composite-resin-market/#:~:text=High%20Temperature%20Composite%20Resin%20Market,aerospace%2C%20transportation%2C%20and%20defense%20globally (accessed: December 09, 2023).
  7. Xinwei F., Jiafu W., Yiru R. Research on high-temperature resistant resin matrix composites of hypersonic aircraft structure. ICMTAE-2021. Journal of Physics: Conference Series. Ser. 2228012014, 2022, pp. 1–6.
  8. Global Polyimide Resins Market Study 2016–2032. Available at: https://www.marketresearch.com/Prismane-Consulting-Private-Limited-v4215/Global-Polyimide-Resins-Study-32057574/ (accessed: December 10, 2023).
  9. Global Polyimide Plastic Market Insights, Forecast to 2028. Available at: https://www.marketresearch.com/QYResearch-Group-v3531/Global-Polyimide-Plastic-Insights-
  10. Forecast-32021561/ (accessed: December 10, 2023).
  11. Global Polyimide Resin Matrix Composite Laminate SuPly, Demand and Key Producers, 2023–2029. Available at: https://www.marketresearch.com/GlobalInfoResearch-v4117/Global-Polyimide-Resin-Matrix-Composite-35273331/ (accessed: December 10, 2023).
  12. Global polyimides market. Available at: https://marketlitmus.com/report-store/chemicals-and-materials/resins-and-polymers/global-polyimides-market/ (accessed: November 17, 2019).
  13. Valueva M.I., Zelenina I.V., Zharinov M.A., Akhmadieva K.R. World market of high temperature polyimide carbon plastic (review). Trudy VIAM, 2019, no. 12 (84), paper no. 08. Available at: http://www.viam-works.ru (accessed: August 31, 2024). DOI: 10.18577/2307-6046-2019-0-12-67-79.
  14. Zharinov M.A., Shimkin A.A., Akhmadiyeva K.R., Zelenina I.V. Features and properties of solvent-free PMR-type polyimide resin. Trudy VIAM, 2018, no. 12 (72), paper no. 05. Available at: http://www.viam-works.ru (accessed: August 31, 2024). DOI: 10.18577/2307-6046-2018-0-12-46-53.
  15. Valueva M.I., Zelenina I.V., Zharinov M.A., Khaskov M.A. High-Temperature Carbon Fiber Reinforced Plastics Based on a Thermoreactive Polyimide Binder. Inorganic Materials: Applied Research, 2021, vol. 12, no. 6, pp. 1581–1589.
  16. PROOF Research Advanced composites division. Available at: https://www.proofresearch.com/advanced-composites-division/ (accessed: November 17, 2023).
  17. AVIC Composit. Available at: https://www.avic.com/en (accessed: November 17, 2023).
  18. Hong W., Yuan L., Ma Y. et al. Resin Transfer Moldable Fluorinated Phenylethynyl-Terminated Imide Oligomers with High Tg: Structure–Melt Stability Relationship. Polymers, 2021, vol. 13, no. 903, pp. 1–9.
  19. Zhang H.-Y., Yuan L.-L., Hong W.-J., Yang S.-Y. Improved Melt Processabilities of Thermosetting Polyimide Matrix Resins for High Temperature Carbon Fiber Composite Applications. Polymers, 2022, vol. 14, no. 965, pp. 1–16.
  20. Imide oligomers, varnishes, otverzhdenny products from them, prepregs and fibrous composites with their use: pat. JP 7418737B2; appl. 24.12.19; publ. 22.01.24.
  21. Method for manufacturing a wholly aromatic polyimide resin having improved heat resistance and elongation properties in a high temperature range: pat. ЕР 2520606В1; appl. 30.12.09; publ. 09.09.15.
  22. Gao S.Z., Huang Z.Q., Wang X.L. et al. Research on Properties of 450 °С Resistant Polyimide Composites. Journal of Physics: Conference Series (ISALT 2022), 2023, vol. 2460, no. 012091, рр. 1–8.
  23. Ghose S., Cano R.J., Watson K.A. et al. High temperature VARTM of phenilethynyl terminated imides. Available at: https://www.iccm-cen-tral.org/Proceedings/ ICCM17proceedings/Themes/Industry/AEROSPACE%20APPLICATIONS/A2.8%20Ghose.pdf (accessed: December 04, 2023).
  24. Fernberg P., Gong G., Mannberg P., Tsampas S. Development of novel high Tg polyimide-based composites. Part I: RTM processing properties. Journal of Composite Materials, 2018, vol. 2, no. 2, pp. 253–260.
  25. Bain S., Ozawa S., Jim M., Criss Jr. Development of a Cure/Postcure Cycle for PETI-330 Laminates Fabricated by Resin Transfer Molding. High Performance Polymers, 2006. Available at: https://www.academia.edu/5559484/Development _of a_Cure_Postcure_Cycle_for_PETI-330_Laminates_Fabricated_by_Resin_Transfer_Molding (accessed: December 04, 2021).
  26. Varna J., Zrida H. Analysis of Microdamage in Thermally Aged CF/Polyimide Laminates. Mechanics of Composite Materials, 2017, vol. 53, no. 1, pp. 45–58.
  27. Proof research ACD. Data sheet product: P2SI® 900HT. Available at: https://proofresearch.com/wp-content/uploads/2020/11/PROOF-CD_data_sheet_900HT_update_ 10-16-15v2-correct.pdf (accessed: August 31, 2023).
  28. Kablov E.N., Laptev A.B., Prokopenko A.N., Gulyaev A.I. Relaxation of polymeric composite materials under the prolonged action of static load and climate (review). Part 1. Binders. Aviation materials and technologies, 2021, no. 4 (65), paper no. 08. Available at: http://www.journal.viam.ru (accessed: August 31, 2023). DOI: 10.18577/2713-0193-2021-0-4-70-80.
  29. Kablov E.N., Startsev V.O. Measurement and forecasting of materials samples’ temperature during weathering in different climatic zones. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 47–58. DOI: 10.18577/2071-9140-2020-0-4-47-58.
  30. Abramova M.G., Lutsenko A.N., Varchenko E.A. Concerning the aspects of validation of climate resistance of airborne materials at all life cycle stages (review). Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 86–94. DOI: 10.18577/2071-9140-2020-0-1-86-94.
  31. Proof research ACD. Data sheet product: P2 SI® 635LM. Available at: https://proofresearch.com/wp-content/uploads/2020/11/PROOF-ACD_data_sheet_635LM_RESIN-Correct.pdf (accessed: August 31, 2023).
  32. Valueva M.I., Zelenina I.V., Nacharkina A.V., Ahmadieva K.R. Technological features of obtaining high temperature polyimide carbons. Foreign experience (review). Trudy VIAM, 2022, no. 6 (112), paper no. 08. Available at: http://www.viam-works.ru (accessed: August 31, 2023). DOI: 10.18577/2307-6046-2022-0-6-80-95.
  33. Valueva M.I., Zelenina I.V., Nacharkina A.V., Boychuk A.S. Determination of the guaranteed shelf life of high-temperature polyimide carbon fiber reinforced plastic prepreg. Trudy VIAM, 2023, no. 10 (128), paper no. 07. Available at: http://www.viam-works.ru (accessed: August 31, 2023). DOI: 10.18577/2307-6046-2023-0-10-64-81.
  34. Semipreg, prepreg, resine composite material, and production methods thereof: pat. US 11492446B2; appl. 22.03.2018; publ. 08.11.2022.
  35. Uncured laminate, reinforcing fiber composite material, method for producing uncured laminate, and method for producing reinforcing fiber composite material: pat. US 2021/0221113A1; appl. 02.04.2021; publ. 22.07.2021.
  36. A novel amide acid oligomer process for molding polyimide composites: pat. WO 2020072639A1; appl. 02.10.19; publ. 09.04.20.
  37. Method for impregnating layered blanks based on woven fillers and epoxy, organosilicon and polyimide binders and a device for implementing this method: pat. 2743422C1 Rus. Federation; appl. 27.03.20; publ. 18.02.21.
  38. Aleksandrova D., Komarova M., Egorov A. Topology and structure analysis of carbon fiber-reinforced polyimide composites. International Scientific and Practical Conference «Environmental Risks and Safety in Mechanical Engineering» (ERSME-2023), 2023, vol. 376, no. 01023, pp. 1–8.
  39. Autoclave cure cycle design process and curing method: pat. WO2010087918A1; appl. 21.12.09; publ. 05.08.10.
  40. Improved processing of polymer matrix composites: pat. EP 2337672B1; appl. 22.10.08; publ. 28.02.18.
  41. Magato J., Klosterman D. Development of a methodology for characterizing reaction kinatics, rheology, and in situ compaction of polyimide prepregs during cure. Journal of composite materials, 2019, no. 8, pp. 1–9.
  42. Products Nexam Chemical AB. Available at: http://www.nexamchemical.com/products/ (accessed: November 17, 2023).
  43. Low-viscosity high-temperature-resistant thermosetting polyimide resin and preparation method and application thereof: pat. CN 112961347B; appl. 20.02.21; publ. 12.04.22.
  44. Polyimide resin composition and method for producing the same: pat. JP2016216720A; appl. 22.12.16; publ. 18.11.20.
  45. Antioxidant polyimide prepreg and preparation method thereof: pat. CN 111154260В; appl. 19.01.20; publ. 23.09.22.
  46. Yang S.Y. Advance polyimide materials: synthesis, characterization, and applications. Elsevier, 2018, 498 p.
  47. Fiber-reinforced laminated body and method for manufacturing same: pat. ЕР 3718765А1; appl. 28.11.17; publ. 06.06.19.
  48. Liu Y., Li J., Chen X. Interlaminar properties of carbon nanotubes modified carbon fiber fabric reinforced polyimide composites. Journal of Composite Materials, 2023, vol. 57, no. 7, pp. 1277–1288.
  49. Method for preparing carbon fiber-polyimide composite material: pat. CN 104629365A; appl. 17.02.15; publ. 01.02.17.
  50. Composite material with a polyimide resin matrix, reinforced with carbon fiber, with super-strong characteristics of interfacial interaction at a high temperature of 300 °C and a method for producing it: pat. CN 116694075A; appl. 29.06.23; publ. 05.09.23.
  51. Method for producing a polyimide composite material reinforced with modified carbon fiber: pat. CN 116278224A; appl. 24.03.23; publ. 23.06.23.