Effect of mutual strengthening in polymer composites based on polyethereketone and thermotropic liquid crystal polymers obtained by 3D-printing
Gurov D.A., Tsapenko A.N., Pavlukovich N.G. Effect of mutual strengthening in polymer composites based on polyethereketone and thermotropic liquid crystal polymers obtained by 3D-printing // Proceedings of VIAM. 2024. No. 10. DOI: 10.18577/2307-6046-2024-0-10-45-62. URL: https://www.viam-works.ru/en/journal/2024/10/5
Keywords
additive technologies, fused deposition modeling, polyetheretherketone, semi-crystalline polymer, thermotropic liquid crystal polymers, Z-axis strengthening
Abstract
The dependences of the mechanical and thermophysical characteristics in samples with different ratios of polyetheretherketone (PEEK) and liquid crystalline polymers (LCP), synthesized by layer-by-layer filament deposition, are shown. It has been shown for certain concentrations, adding LCP to PEEK can increase the mechanical characteristics compared to the material synthesized by FDM from unfilled PEEK. The presence of fibrils and coaxial shells between the layers of 3D-synthesized organic composite plastic and inside the threads themselves is shown. A relationship has been proposed between the microstructure of samples synthesized by FDM and their mechanical properties.
Reference list
- Kablov E.N., Kondrashov S.V., Melnikov A.A., Pavlenko S.A., Guseva M.A., Pykhtin A.A., Larionov S.A. Investigation of the influence of the thermal regime of FDM printing on the structuring and warping of polyethylene samples. Trudy VIAM, 2021, no. 7 (101), paper no. 06. Available at: http://www.viam-works.ru (accessed: August 18, 2023). DOI: 10.18577/2307-6046-2021-0-7-48-58.
- Pykhtin A.A., Sorokin A.E., Larionov S.A., Lonskii S.L. Study of the influence of non-covalent modifiers on the structure and properties of polymer filaments for FDM-printing based on ABS-plastic and carbon nanoparticles. Trudy VIAM, 2021, no. 10 (104), paper no. 04. Available at: http://www.viam-works.ru (accessed: August 18, 2023). DOI: 10.18577/2307-6046-2021-0-10-36-44.
- Kirin B.S., Lonskii S.L., Petrova G.N., Sorokin A.E. Materials for the 3D-printing on the basis of polyetheretherketones. Trudy VIAM, 2019, no. 4 (76), paper no. 03. Available at: http://viam-works.ru (accessed: August 18, 2023). DOI: 10.18577/2307-6046-2019-0-4-21-29.
- Kirin B.S., Kuznetsova K.R., Petrova G.N., Sorokin A.E. Comparative analysis of properties of polyetheretherketones of domestic and foreign production. Trudy VIAM, 2018, no. 5 (65), paper no. 05. Available at: http://www.viam-works.ru (accessed: August 18, 2023). DOI: 10.18577/2307-6046-2018-0-5-34-43.
- Sikder P., Challa B.T., Gummadi S.K. A comprehensive analysis on the processing-structure-property relationships of FDM-based 3-D printed polyetheretherketone (PEEK) structures. Materialia. 2022, vol. 22, р. 101427.
- Dua R., Rashad Z., Spears J., Dunn G., Maxwell M. Applications of 3D-Printed PEEK via Fused Filament Fabrication: A Systematic Review. Polymers, 2021, vol. 13, р. 4046.
- Rinaldi M., Cecchini F., Pigliaru L., Ghidini T., Lumaca F., Nanni F. Additive Manufacturing of Polyether Ether Ketone (PEEK) for Space Applications: A Nanosat Polymeric Structure. Polymers, 2021, vol. 13, р. 11
- Rinaldi M., Ghidini T., Cecchini F., Brandao A., Nanni F. Additive layer manufacturing of poly (ether ether ketone) via FDM. Composites Part B. 2018, vol. 145, рр. 162–172.
- Li Y., Lou Y. Tensile and Bending Strength Improvements in PEEK Parts Using Fused Deposition Modelling 3D Printing Considering Multi-Factor Coupling. Polymers, 2020, vol. 12 (11), р. 2497
- Gonçalves J., Lima P., Krause B. et al. Electrically conductive polyetheretherketone nanocomposite filaments: From production to fused deposition modeling. Polymers, 2018, vol. 10, р. 925.
- Aysha M. A futuristic reality: 3D printed SpaceX helmets. 3DNatives. Available at: https://www.3dnatives.com/en/3d-printed-spacex-helmets-090620206/ (accessed: August 18, 2023).
- Steers S. 3D printing: The future of space construction? Construction Digital. Available at: https://constructiondigital.com/epc/3d-printing-future-space-construction (accessed: August 18, 2023).
- Reuters T. Boeing's new spacecraft to use more than 600 3D-printed parts. CBC News. Available at: https://www.cbc.ca/news/science/boeing-new-spacecraft-3d-parts-1.3966358 (accessed: August 18, 2023).
- Pearson A. Stratasys additive manufacturing chosen by Airbus to produce 3D printed flight parts. Stratasys Blog. Available at: https://www.stratasys.com/en/resources/blog/airbus-3d-printing/ (accessed: August 18, 2023).
- Tyrer-Jones A. Finnair upgrades its Airbus A320 fleet with new 3D printed components. 3D printing industry. Available at: https://3dprintingindustry.com/news/finnair-upgrades-its-airbus-a320-fleet-with-new-3d-printed-components-230516/ (accessed: August 18, 2023).
- Materialise. Why Airbus Qualified A New 3D Printing Material In 2021: Flame-Retardant PA. Aviation Week. Available at: https://aviationweek.com/mro/why-airbus-qualified-new-3d-printing-material-2021-flame-retardant-pa (accessed: August 18, 2023).
- Case study. Airbus Gets on Board with 3D Printing. Materialise. Available at: https://www.materialise.com/en/inspiration/cases/airbus-3d-printing (accessed: August 18, 2023).
- Davies S. Boeing qualifies Stratasys Antero 800NA 3D printing thermoplastic material. TCT Magazine. Available at: https://www.tctmagazine.com/additive-manufacturing-3d-printing-news/boeing-qualifies-stratasys-antero-800na-3d-printing-material/ (accessed: August 18, 2023).
- Autonomous Manufacturing. Application Spotlight: 3D Printing for Aircraft Cabins. AMFG. Available at: https://amfg.ai/2020/07/27/application-spotlight-3d-printing-for-aircraft-cabins/ (accessed: August 18, 2023).
- Torke N. Materialise to Deliver 3D-Printed, Flight-Ready Plastic Parts for Airbus. Materialise. Available at: https://www.materialise.com/en/news/press-releases/3d-printed-flight-ready-plastic-parts-for-airbus (accessed: August 18, 2023).
- Gardner J.M., Stelter C.J., Yashin E.A., Siochi E.J. High Temperature Thermoplastic Additive Manufacturing Using Low-Cost, OpenSource Hardware. NASA Report № NASA-TM-2016-219344. Available at: https://ntrs.nasa.gov/api/citations/20170000214/downloads/20170000214.pdf (accessed: August 18, 2023).
- Prater T.J., Bean Q.A., Beshears R.D. et al. Summary Report on Phase I Results From the 3D Printing in Zero-G Technology Demonstration Mission, Volume I // NASA Report № NASA/TP—2016–219101. Available at: https://ntrs.nasa.gov/api/citations/20160008972/downloads/20160008972.pdf (accessed: August 18, 2023).
- Gaskill M. Solving the Challenges of Long Duration Space Flight with 3D Printing. NASA website. Available at: https://www.nasa.gov/missions/station/solving-the-challenges-of-long-duration-space-flight-with-3d-printing/ (accessed: August 18, 2023).
- Caliendo H. Mercedes-Benz Turns to 3D Printing for Plastic Spare Parts. Additive Manufacturing. Available at: https://www.additivemanufacturing.media/articles/mercedes-benz-turns-to-3d-printing-for-plastic-spare-parts-(2) (accessed: August 18, 2023).
- Griffiths L. Audi Sport reduces design time by 90% with automation of 3D printed jigs and fixtures. TCT Magazine. Available at: https://www.tctmagazine.com/additive-manufacturing-3d-printing-news/software-and-simulation-news/audi-sport-reduces-design-time-by-90-with-automated-design-o/ (accessed: August 18, 2023).
- Camillo J. Bentley Motors Drives its Future Car Design With 3D Printing. Assembly Magazine. Available at: https://www.assemblymag.com/articles/95439-bentley-motors-drives-its-future-car-design-with-3d-printing (accessed: August 18, 2023).
- Farish M. Bentley increases use of additive manufacturing. AMS magazines. Available at: https://www.automotivemanufacturingsolutions.com/oems/bentley-increases-use-of-additive-manufacturing/43137.article (accessed: August 18, 2023).
- Lamborghini и Stratasys: история любви на высокой скорости. Новости 3D Today. Available at: https://3dtoday.ru/blogs/news3dtoday/lamborghini-and-stratasys-a-love-story-at-high-speed (accessed: August 18, 2023).
- Five Ways 3D Printing Is Transforming the Automotive Industry. Stratasys. Available at: https://www.stratasys.com/contentassets/e85c0f5f58be4be1a4e12ceac237e026/wp_fdm_fivewaysauto_a4_0516-web.pdf?v=48fd7e (accessed: August 18, 2023).
- Lamborghini Accelerates and Perfects Automotive Engineering with Stratasys 3D Printed Prototypes and Track-Ready Parts. Statasys corporate blog. Available at: http://blog.stratasys.com/ (accessed: August 18, 2023).
- 3D Printed Lamborghini: Next-Gen Innovations In Automotive Design. Petropoulos G. Available at: https://www.inorigin.eu/3d-printed-lamborghini/ (accessed: August 18, 2023).
- Stratasys. UPSA spurs pharmaceutical manufacturing innovation with 3D printing. Stratasys Case Study. Available at: https://www.stratasys.com/en/resources/case-studies/upsa/ (accessed: August 18, 2023).
- How UPSA realizes its return on investment by integrating 3D printing. 3D Adept Media. Available at: https://3dadept.com/stratasys-upsa-3d-printing/ (accessed: August 18, 2023).
- Stratasys to test 3D printed materials on the moon. The Engineer. Available at: https://www.theengineer.co.uk/content/news/stratasys-to-test-3d-printed-materials-on-the-moon/ (accessed: August 18, 2023).
- Boissonneault T. Marshall Aerospace and Defence using FDM 3D printing for flight-ready parts. Voxel Matters. Available at: https://www.voxelmatters.com/marshall-aerospace-defence-fdm-3d-printing/ (accessed: August 18, 2023).
- Sevcik S. The Install Ready (FORM 1) Approach - AM Part Qual in Aviation, Part 1. Aerospace & Defense | Technology, Strategy, Additive Manufacturing. Available at: https://www.linkedin.
- com/pulse/install-ready-form-1-approach-am-part-qual-aviation-scott-sevcik-k6pmc (accessed: August 18, 2023).
- De Zeeuw E. Breaking the certification barrier in aerospace AM. Aerospace Manufacturing and Design. Available at: https://www.aerospacemanufacturinganddesign.com/article/breaking-the-certification-barrier-in-aerospace-am/ (accessed: August 18, 2023).
- Stratasys. A Path to Certification. White paper, 2019, рр. 1–9. Available at: https://www.padtinc.com/blog2/wp-content/uploads/2019/12/Path-to-Certification-EN-A4-FDM-White-Paper.pdf (accessed: August 18, 2023).
- Banerjee S., Kar K.K. Introduction to Liquid Crystalline Polymers. Polymers and Polymeric Composites: A Reference Series, 2020, рр. 1–26.
- Wang X.-J., Zhou Q.-F. Liquid Crystalline Polymers. World Scientific Publishing Company, 2004, 388 р.
- Thakur V.K., Kessler M.R. Liquid Crystalline Polymers. Springer, 2016, vol. 1: Structure and Chemistry, 626 р.
- Deberdeev T.R., Akhmetshina A.I., Karimova L.K. et al. Heat-resistant polymer materials based on liquid crystalline compounds. Vysokomolekulyarnyye soyedineniya. Ser.: С, 2020, vol. 62, no. 2, pp. 145–165. DOI: 10.31857/S230811472002003X.