Investigation of the fatigue strength of VT41 titanium alloy sheet material at room temperature under uniaxial stretching conditions in the low- and high-cycle region

Kashapov O.S., Ryzhkov P.V., Chuchman O.V., Naprienko S.A.
Kashapov O.S., Ryzhkov P.V., Chuchman O.V., Naprienko S.A. Investigation of the fatigue strength of VT41 titanium alloy sheet material at room temperature under uniaxial stretching conditions in the low- and high-cycle region // Proceedings of VIAM. 2024. No. 10. DOI: 10.18577/2307-6046-2024-0-10-34-44. URL: https://www.viam-works.ru/en/journal/2024/10/4
Keywords
titanium alloys, mechanical properties, fatigue strength, titanium sheets, phase composition
Abstract

The article presents and summarizes the test results of the mechanical properties of material of industrial sheets with a thickness of 2,0 mm made of heat-resistant titanium alloy VT41. The results of tensile tests, low- and high-cycle fatigue tests of flat samples are presented as well as the results of tensile testing of samples with a corset shape of the working part at different loading speeds. On the base of tests results a stress-cycles to failure curve is  constructed in the areas of static, re-static, low-cycle and classical high-cycle destruction.

Reference list
  1. Shanyavskiy A.A., Soldatenkov A.P. Large-scale levels of the fatigue limit of metals. Fizicheskaya mezomekhanika, 2019, no. 1, pp. 44–53. DOI: 10.24411/1683-805X-2019-11005.
  2. Burago N.G., Nikitin I.S., Shanyavski A.A., Zhuravlev A.B. Durability estimations for in-service titanium compressor disks subjected to multiaxial cyclic loads in low- and very-high-cycle fatigue regimes. Proceedings of 19th European Conference on Fracture (Kazan, Russia, 26–31 Aug. 2012). Available at: https://www.grouppofrattura.it (accessed: February 11, 2024).
  3. Belousov G.G., Nikitin A.D., Shanyavskiy A.A. Model of fatigue failure in operation of a titanium fan disk of the TA12-60 engine. Nauchnyy vestnik MGTUGA, 2013, no. 187, pp. 103–107.
  4. Ravikovich Yu.A., Kholobtsev D.P., Arkhipov A.N., Shakhov A.S. Calculation and experimental study of the dynamics and strength of the main parts of a gas turbine engine taking into account geometric deviations. Vestnik UGATU, 2023, vol. 27, no. 1 (99), pp. 47–59.
  5. Soloviev B.A., Kulandin A.A., Makarov N.V. Design and flight operation of power plants. Moscow: Transport, 1991, 256 p.
  6. Pakhomenkov A.V. Calculation and experimental forecasting of low-cycle durability and service life of gas turbine engine disks taking into account the influence of analytical and operational factors: thesis, Cand. Sc, (Tech.). Rybinsk, 2020, 154 p.
  7. Makarov P.V., Kolotnikov M.E., Vedeneev V.V., Abdukhakimov F.A. Comprehensive analysis of the dynamic behavior of compressor blades at the design stage. Aviatsionnye dvigateli, 2023, no. 3 (20), рр. 20–27.
  8. Petukhov A.N. Problems of high-cycle fatigue of structural materials and gas turbine engine parts. Vestnik Samarskogo gosudarstvennogo aerokosmicheskogo universiteta, 2012, no. 3 (34), pp. 17–25. DOI: 10.18287/2541-7533-2012-0-3-1(34)-17-25.
  9. Inozemtsev A.A., Sandratsky V.L. Gas turbine engines. Perm: Aviadvigatel, 2006, 1204 p.
  10. De Monicault J.-M., Guedou J.-Y., Soniak F. Issues and progress in manufacturing of aero titanium parts. 24th ITA: Titanium Conference Proceedings. Las Vegas, 2008, р. 7.
  11. Geary B., Bolam V.J., Jenkins S.L., Davies D.P. High temperature titanium sheet for helicopter exhaust applications. 8th Titanium World Conference. London: Cambridge University Press, 1996, рр. 1638–1645.
  12. Pavlova T.V., Kashapov O.S., Kalashnikov V.S., Kondrateva A.R. Industrial development of manufacturing large-size forgings from heat-resistant titanium alloy VT41 for welded assemblies of aircraft products. Trudy VIAM, 2022, no. 9 (115), paper no. 04. Available at: http://www.viam-works.ru (accessed: February 16, 2024). DOI: 10.18577/2307-6046-2022-0-9-39-57.
  13. Makhutov N.A., Gdenini M.M. Study of generalized curves of static and cyclic deformation, damage and destruction. Zavodskaya laboratoriya. Diagnostika materialov, 2023, vol. 89, no. 5, pp. 46–54. DOI: 10.26896/1028-6861-2023-89-5-46-55.
  14. Kapustin V.I., Zakharchenko K.V., Cherepanova V.K., Shayapov V.R. Investigation of dissipative processes of VT6 alloy under fatigue. Aviation materials and technologies, 2022, no. 4 (69), paper no. 09. Available at: http://www.journal.viam.ru (accessed: February 01, 2024). DOI: 10.18577/2713-0193-2022-0-4-96-111.
  15. Gorbovets M.A., Khodinev I.A., Monin S.A. Influence of average cycle stress on characteristics of low-cycle fatigue of high-temperature nickel alloy VZh175. Aviation materials and technologies, 2023, no. 1 (70), paper no. 10. Available at: http://www.journal.viam.ru (accessed: February 16, 2024). DOI: 10.18577/2713-0193-2023-0-1-126-136.
  16. Gorbovets M.A., Khodinev I.A., Karanov V.A., Yushin V.D. Influence of the type of loading on high-cycle fatigue of heat-resistant alloys. Trudy VIAM, 2019, no. 3 (75), paper no. 11. Available at: http://www.viam-works.ru (accessed: February 12, 2024). DOI: 10.18577/2307-6046-2019-0-3-96-104.
  17. Duyunova V.A., Putyrskiy S.V., Arislanov A.A., Krokhina V.A., Shiryaev A.A. Analysis of the effect of heat treatment on the structure and mechanical properties of bars made of VT47 titanium alloy. Aviation materials and technologies, 2021, no. 4 (65), paper no. 03. Available at: http://www.journal.viam.ru (accessed: February 17, 2024). DOI: 10.18577/2713-0193-2021-0-4-26-34.
  18. Kablov D.E., Panin P.V., Shiryaev A.A., Nochovnaya N.A. The use of ADL VAR L200 vacuum-arc furnace for ingots fabrication of high-temperature titanium aluminides base alloys. Aviacionnye materialy i tehnologii, 2014, no. 2, pp. 27–33. DOI: 10.18577/2071-9140-2014-0-2-27-33.
  19. Nochovnaya N.A., Shiryaev A.A. Features of the structural and phase composition, mechanical properties of metastable β-titanium alloy VT47 alloyed with silicon. Aviation materials and technologies, 2023, no. 1 (70), paper no. 04. Available at: http://www.journal.viam.ru (accessed: February 15, 2024). DOI: 10.18577/2713-0193-2023-0-1-51-60.
  20. Dzunovich D.A., Lukina E.A., Yakovlev A.L. Influence of heat treatment parameters on producibility and mechanical properties of sheets made from high-strength titanium alloy VT23. Aviacionnye materialy i tehnologii, 2018, no. 3 (52), pp. 3–10. DOI: 10.18577/2071-9140-2018-0-3-3-10.
  21. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  22. Antipov V.V. Prospects for development of aluminium, magnesium and titanium alloys for aerospace engineering. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 186–194. DOI: 10.18577/2107-9140-2017-0-S-186-194.
  23. Kablov E.N., Kashapov O.S., Pavlova T.V., Nochovnaya N.A. Development of a pilot industrial technology for the production of semi-finished products from pseudo-α titanium alloy VT41. Titan, 2016, no. 2 (52), pp. 33–42.
  24. Shrestha R., Simsiriwong J., Shamsaei N. Fatigue behavior of additive manufactured 316L stainless steel under axial versus rotating-bending loading: Synergistic effects of stress gradient, surface roughness, and volumetric defects. International Journal of Fatigue, 2021, vol. 144, p. 106063. DOI: 10.1016/j.ijfatigue.2020.106063.
  25. Medvedev P.N., Kashapov O.S., Reshetilo L.P. Study of surface layers of titanium alloy VT41 after mechanical treatment. Voprosy materialovedeniya, 2022, no. 1 (109), pp. 54–63.
  26. Derimow N., Benzing J., Newton D., Beamer C. Microstructural effects on the rotating bending fatigue behavior of Ti–6Al–4V produced via laser powder bed fusion with novel heat treatments. International Journal of Fatigue, 2024, vol. 185, p. 108362. DOI: 10.1016/j.ijfatigue.2024.108362.