Methodological issues of studying the effectiveness of anticorrosion protection used in aviation equipment products

Kutyrev A.E., Vdovin A.I., Antipov V.V., Duyunova V.A.
Kutyrev A.E., Vdovin A.I., Antipov V.V., Duyunova V.A. Methodological issues of studying the effectiveness of anticorrosion protection used in aviation equipment products // Proceedings of VIAM. 2024. No. 1. DOI: 10.18577/2307-6046-2024-0-1-78-91. URL: https://www.viam-works.ru/en/journal/2024/1/8
Keywords
corrosion, corrosion protection tests, contact corrosion of aluminum alloys, corrosion state analysis, full-scale tests, design-like specimens
Abstract

The question of development of methodology for testing, allowing to choose the most highly effective complex system of anticorrosion protection, is considered. The principles of testing of corrosion protection systems are noted/ Structurally similar specimens representing the connection of aluminum alloy 1163-AT and carbon plastic of mark VKU-25 with the help of fasteners from titanium alloy BT6 as with application of protective coatings on the basis of primers, enamels, varnishes, sealants and pastes, and without their application are made. The algorithm of evaluation of corrosion lesions on structural-like samples for selection of complex protection system is proposed.

Reference list
  1. Sagitov I.F. Composite materials in modern aircraft construction. Aktualnye problemy aviatsii i kosmonavtiki, 2017, vol. 2, pр. 480–490.
  2. Kablov E.N., Karimova S.A., Semenova L.V. Corrosion activity of carbon fiber reinforced plastics and protection of metal load-bearing structures in contact with carbon fiber reinforced plastics. Korroziya: materialy, zashchita, 2011, no. 12, pp. 1–7.
  3. Rosenfeld I.L. Corrosion and protection of metals. Moscow: Metallurgy, 1969, 448 p.
  4. Sinyavsky V.S., Valkov V.D., Kalinin V.D. Corrosion and protection of aluminum alloys. Moscow: Metallurgy, 1986, 76 p.
  5. Zhang W., Frankel G.S. Transition between pitting and intergranular corrosion in AA2024. Electrochimica Acta, 2003, vol. 48, pp. 1193–1210.
  6. Findlay S.J., Harrison N.D. Why aircraft fail. Materials Today: Materials feature, 2002, vol. 5, no. 11, pp. 18–25.
  7. Gromov M.S., Shapkin V.S. Features of maintaining the airworthiness of an aircraft in conditions of maintenance-free operation. Nauchnyy vestnik MGTU GA. Seriya Aeromekhanika i prochnost, podderzhaniye letnoy godnosti VS, 2006, no. 103, p. 713.
  8. Kinzie R.C. USAF Cost of Corrosion Maintenance. Sixth Joint FAA/DoD/NASA Conference on Aging Aircraft. San Francisco CA, 2002, p. 35.
  9. Feigenbaum Yu.M., Dubinsky S.V. The influence of accidental operational damage on the strength and service life of aircraft structures. Scientific Bulletin of MSTU GA, 2013, no. 187, pp. 83–91.
  10. Kutyrev A.E., Chesnokov D.V., Antipov V.V., Vdovin A.I. The development of a solution for promotion of corrosion attack on aluminium alloys in a galvanostatic mode. Trudy VIAM, 2018, no. 9 (69), paper no. 11. Available at: http://www.viam-works.ru (accessed: June 15, 2023). DOI: 10.18577/2307-6046-2018-0-9-105-118.
  11. Kuzyakina V.A., Toleukhanov A.D. The problem of transition to an aircraft repair system based on the actual technical condition. Advanced technologies in transport systems. Orenburg: Orenburg State Univ., 2019, pp. 332–336.
  12. Vinogradov S.S., Nikiforov A.A., Zakirova L.I. Cadmium replacement. Stage 2 – final. Galvanic thermal coating of zinc–tin system – real alternative to cadmium plating. Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 59–66. DOI: 10.18577/2071-9140-2019-0-3-59-66.
  13. Chaykun A.M., Venediktova M.A., Smirnov D.N., Gerasimov D.M. Features of the influence of atmospheric factors on the main technical characteristics of sealing materials of various types of aviation purposes. Trudy VIAM, 2019, no. 2 (74), paper no. 06. Available at: http://viam-works.ru (accessed: August 07, 2023). DOI: 10.18577/2307-6046-2019-0-2-58-67.
  14. Merkulova Yu.I., Kuznetsova V.A., Novikova T.A. Investigation of properties of coating system based on fluorine polyurethane enamel and primer with low toxical pigment content. Trudy VIAM, 2019, no. 5 (77), paper no. 08. Available at: http://www.viam-works.ru (accessed: July 15, 2023). DOI: 10.18577/2307-6046-2019-0-5-68-75.
  15. Fomina M.A., Volkov I.A., Vdovin A.I., Yamshchikov E.I. Study of protective capacity anodic oxide coating with environmental friendly improved filling technology. Aviation materials and technologies, 2023, no. 4 (73), paper no. 10. Available at: http://www.journal.viam.ru (accessed: November 20, 2023). DOI: 10.18577/2713-0193-2023-0-4-101-110.
  16. Sadkov V.V., Mirkin I.I. Ensuring corrosion resistance of aluminum structures in Tu aircraft. Non-ferrous metals, 2006, no. 11, pp. 73–76.
  17. Kurs M.G., Karimova S.A. Salt-accelerated outdoor corrosion testing: methodology and evaluation of corrosion susceptibility of aluminum alloy. Aviacionnye materialy i tehnologii, 2014, no. 1, pp. 51–57. DOI: 10.18577/2071-9140-2014-0-1-51-57.
  18. Simpson C.H., Ray C.J., Skerry B.S. Accelerated Corrosion Testing of lndustrial Maintenance Paints Using a Cyclic Corrosion Weathering Method. Journal of Protective Coatings and Linings, 1991, vol. 8, no. 5, p. 2836.
  19. Kutyrev A.E., Fomina M.A., Chesnokov D.V. Development of a method of cyclic corrosion tests simulating natural exposure of aluminum alloys in a coastal atmosphere. Part 1. Basic principles. Korroziya: materialy, zashchita, 2019, no. 10, pp. 35–42.
  20. Zhuk N.P. Course on the theory of corrosion and protection of metals. Moscow: Metallurgy, 1976, 472 p.
  21. DuQuesnay D.L., Underhill P.R., Britt H.J. Fatigue crack growth from corrosion damage in 7075-T6511 aluminium alloy under aircraft loading. International Journal of Fatigue, 2003, vol. 25, no. 5, рр. 371–377.
  22. Mills T., Sharp P.K., Loader C. The incorporation of pitting corrosion damage into F-111 fatigue life modeling. Canberra (Australia): Defense science and technology organization, 2002, 138 p.
  23. Sprowls D.O. Evaluation of pitting corrosion. ASM Handbook. ASM International, 1987, vol. 13: Corrosion, pр. 516–521.