Prescription techniques for creating elastomeric compositions with reduced flammability
Potapova A.I., Bobrova I.I., Evdokimov A.A., Venediktova M.A. Prescription techniques for creating elastomeric compositions with reduced flammability // Proceedings of VIAM. 2024. No. 1. DOI: 10.18577/2307-6046-2024-0-1-60-77. URL: https://www.viam-works.ru/en/journal/2024/1/7
Keywords
flame retardant, elastomeric material, rubber, combustion, fire resistance, oxygen index
Abstract
This article is devoted to the analysis of existing methods of increasing the fire resistance of elastomers. The stages and mechanism of the combustion process are considered. Methods for assessing flammability, flammability classes, and prescription methods for increasing the fire resistance of rubbers are described. Rubbers that are of interest for the creation of materials with reduced flammability are listed, and energy characteristics, by which their resistance to open flame is assessed, are given. Traditional flame-retardants used to increase the fire resistance of elastomers and the new ones are presented. The areas of application of low-flammable rubbers are shown.
Reference list
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N. The role of chemistry in the creation of new generation materials for complex technical systems. XX Mendeleev Congress on General and Applied Chemistry: abstracts of reports: in 5 vols. Ekaterinburg: Ural Branch of the Russian Academy of Sciences, 2016, vol. 1, pp. 25–26.
- History of aviation materials science. VIAM – 80 years: years and people. Ed. E.N. Kablov. Moscow: VIAM, 2012, pp. 346–348.
- Kablov E.N. The sixth technological structure. Nauka i zhizn, 2010, no. 4, pp. 2–7.
- Venediktova M.A., Evdokimov A.A., Krasnov L.L., Petrova A.P. Research of possibility of application of fireproof paste for increase of fire safety of designs from polymeric composite materials. Trudy VIAM, 2021, no. 9 (103), paper no. 07. Available at: http://www.viam-works.ru (accessed: November 27, 2023). DOI: 10.18577/2307-6046-2021-0-9-67-75.
- Kan A.Ch., Zhelezina G.F., Kulagina G.S., Ayupov T.R. Fire safety of structural organic plastics reinforced with aramid fabrics. Aviation materials and technologies, 2022, no. 4 (69), paper no. 05. Available at: http://www.journal.viam.ru (accessed: October 17, 2023). DOI: 10.18577/2713-0193-2022-0-4-51-60.
- Garashchenko A.N., Vinogradov A.V., Kobylkov N.V., Nikolchenkin A.A., Antipov E.A. Experimental and computational modeling of fire and thermal protection composite materials under high-temperature exposure. Aviation materials and technologies, 2022, no. 3 (68), paper no. 03. Available at: http://www.journal.viam.ru (accessed: October 09, 2023). DOI: 10.18577/2713-0193-2022-0-3-84-97.
- Garashchenko A.N., Kulkov A.A., Strakhov V.L. The effect of the service life on the flame-retardant efficiency of the bulging coatings and the fire resistance of structures. Aviation materials and technologies, 2022, no. 2 (67), paper no. 09. Available at: http://www.journal.viam.ru (accessed: October 09, 2023). DOI: 10.18577/2713-0193-2022-0-2-97-110.
- Nacharkina A.V., Zelenina I.V., Valueva M.I., Barbotko S.L. Fire safety of high-temperature carbon fiber reinforced plastics for aviation purposes (review). Trudy VIAM, 2022, no. 7 (113), paper no. 12. Available at: http://www.viam-works.ru (accessed: November 27, 2023). DOI: 10.18577/2307-6046-2022-0-7-134-150.
- Khomich V.A., Smirnova T.B. Assessment of the influence of flame retardant additives on the flammability of rubber. Education. Transport. Innovation. Construction: Materials of III National Scientific and Practical Conference. Omsk: SibADI, 2020, pp. 472–477.
- Shashok Zh.S. Fundamentals of formulation development of elastomeric compositions: educational allowance. Minsk: BSTU, 2013, 98 p.
- Rubber technology. Recipe development and testing: trans. from Engl. Ed. J.S. Dick. St. Petersburg: Scientific principles and technologies, 2010, 620 p.
- Kodolov V.I. Flammability and fire resistance of polymer materials. Moscow: Khimiya, 1976, 157 p.
- Kryzhanovsky V.K., Burlov V.V., Panimatchenko A.D., Kryzhanovskaya Yu.V. Technical pro-perties of polymer materials: allowance, 2nd. ed. St. Petersburg: Profession, 2005, 249 p.
- Berlin Al.Al. Combustion of polymers and polymer materials of reduced flammability. Sorosovskiy obrazovatel'nyy zhurnal, 1996, no. 9, vol. 2, pp. 57–63.
- Venediktova M.A. Fire and heat-protective coatings with improved operational, technological and environmental characteristics: thesis, Cand. Sc. (Tech.). Moscow: VIAM, 2021, 114 p.
- Koshelev F.F., Kornev A.E., Bukanov A.M. General rubber technology. 4th ed. Moscow: Khimiya, 1978, 528 p.
- Zhirikova Z.M., Aloev V.Z., Tarchokova M.A. Fire resistance of polymer materials and methods for increasing it. Izvestiya Kabardino-Balkarskogo gosudarstvennogo agrarnogo universiteta im. V.M. Kokova, 2019, no. 3 (25), pp. 43–48.
- Chaikun A.M., Venediktova M.A., Bryk Ya.A. Development of the compounding of rubber extremely high heat resistance with temperature range of exploitation from the –60 to +500 °С. Trudy VIAM, 2019, no. 1 (73), paper no. 03. Available at: http://viam-works.ru (accessed: November 27, 2023). DOI: 10.18577/2307-6046-2019-0-1-21-30.
- Fire-resistant hose reinforced with fiberglass cord fabric: pat. 2589589 Rus. Federation; appl. 16.04.13; publ. 10.07.16.
- Petrova N.P. Development of fire-resistant rubbers based on nitrile butadiene rubbers and general purpose rubbers using combinations of fire retardants: thesis abstract, Cand. Sc. (Tech.). Cheboksary: Printing House of Chuvash State Univ., 2015, 24 p.
- Kodolov V.I. Flame retardants for polymer materials. Moscow: Khimiya, 1980, 274 p.
- Kablov V.F., Novopoltseva O.M., Kochetkov V.G., Lapina A.G. Basic methods and mechanisms for increasing the fire and heat resistance of materials. Izvestiya Volgogradskogo gosudarstvennogo tekhnicheskogo universiteta, 2016, no. 4, pp. 46–60.
- Fire-resistant rubber mixture: pat. 2522627 Rus. Federation; appl. 21.11.12; publ. 20.07.14.
- Petrova N.M., Tarasov N.A., Ushmarin N.F. et al. The influence of fire retardants on the combustion kinetics of rubber based on SKI-3 and SKD rubbers. Vestnik Kazanskogo tekhnologicheskogo universiteta, 2015, vol. 18, no. 2, pp. 104–107.
- Composition of flame retardant epdm rubber compound and its preparing method: pat. 100637655 KR; appl. 09.08.2005; publ. 24.10.06.
- Naumov I.S., Petrova A.P., Barbotko S.L., Guliaev A.I. Rubbers with the lowered combustibility on basis of ethylenepropylene-diene rubber. Trudy VIAM, 2016, no. 2 (38), paper no. 09. Available at: http://www.viam-works.ru (accessed: November 27, 2023). DOI: 10.18577/2307-6046-2016-0-2-9-9.
- Fire-retardant material for coatings and method of its production: pat. 2105029 Rus. Federation; appl. 05.09.95; publ. 20.02.98.
- Kablov V.F., Novopoltseva O.M., Kochetkov V.G., Lapina A.G., Zvada S.S., Gaidukova A.A. Study of the influence of highly dispersed intumescent fire retardant systems on the fire and heat resistance of elastomeric compositions. Vestnik Kazanskogo tekhnologicheskogo universiteta, 2015, vol. 18, no. 14, pp. 48–49.
- Petrova N.P., Ushmarin N.F., Koltsov N.I. Increasing the fire resistance of NBR-based rubber using combinations of trichlorethyl phosphate with various flame retardants. Vestnik Kazanskogo tekhnologicheskogo universiteta, 2012, vol. 15, no. 19, pp. 94–97.
- Hamdani S., Longuet C., Perrin D. et al. Flame retardancy of silicone-based materials. Polymer Degradation and Stability, 2009, no. 4, pp. 465–495. DOI: 10.1016/j.polymdegradstab.2008.11.019.
- Naumov I.S., Petrova A.P., Eliseev O.A., Barbotko S.L. Experimental research in the field of development of organic silicon rubbers with low flammability. Trudy VIAM, 2015, no. 10, paper no. 09. Available at: http://www.viam-works.ru (accessed: November 27, 2023). DOI: 10.18577/2307-6046-2015-0-10-9-9.
- Eliseev O.A., Naumov I.S., Smirnov D.N., Bryk Ya.A. Rubbers, sealants, fireproof and heat-shielding materials. Aviacionnye materialy i tehnologii, 2017, no. S, рр. 437–451. DOI: 10.18577/2071-9140-2017-0-S-437-451.
- Zimina A.S., Khakimullin Yu.N. The influence of aluminum hydroxide and magnesium hydroxide on the heat resistance of siloxane rubbers. Promyshlennoe proizvodstvo i ispol'zovaniye elastomerov, 2022, no. 3–4, pp. 22–26. DOI: 10.24412/2071-8268-2022-3-4-22-26.
- Ryutkyanen E.A., Sirotinkin N.V., Belshina Yu.N. Composite heat-insulating polyurethane foam of reduced flammability. Vestnik Sankt-Peterburgskogo universiteta Gosudarstvennoy protivopozharnoy sluzhby MCHS Rossii, 2012, no. 1, pp. 42–46.
- Platonov M.M., Nesterova T.A., Nazarov I.A., Bejder E.Ya. Fabric-based fireproof material with polyurethane coating for inflatable shell of rescue ladder. Aviacionnye materialy i tehnologii, 2013, no. 2, pp. 50–54.
- Kablov V.F., Novopoltseva O.M., Kochetkov V.G., Lapina A.G., Tsybulko N.O. Study of the influence of a modified dispersed aluminosilicate filler on the fire resistance of elastomeric compositions. Vestnik Kazanskogo tekhnologicheskogo universiteta, 2015, vol. 18 , no. 14, pp. 54–55.
- Kablov V.F., Novopoltseva O.M., Kochetkov V.G., Lapina A.V. Study of the influence of transition metal compounds on the fire and heat resistance of elastomeric compositions. Izvestiya Volgogradskogo gosudarstvennogo tekhnicheskogo universiteta, 2014, no. 22, pp. 68–71.
- Ushmarin N.F., Petrova N.N., Sandalov S.I., Petrova N.P., Koltsov N.I. Development of fire-resistant rubbers based on nitrile butadiene rubbers using a combination of fire retardants. Kauchuk i rezina, 2012, no. 1, pp. 28–31.
- Lomakin S.M., Zaikov G.E. Flame retardants for polymers. Kauchuk i rezina, 2010, no. 4, pp. 34–42.
- Murzaev R.K., Abdumavlyanova M.K., Sodikova M.R., Tadzhikhodzhaev Z.A. Problems of classification of chemical products – fire retardant additives («fire retardants») for customs purposes. Universum: tekhnicheskiye nauki, 2021, no. 10–3 (91), pp. 73–79.