The influence of carbon filler type on the physical, mechanical and electrically conductive properties of polyamide-based injection molded thermoplastic materials
Solovyanchik L.V., Minaeva L.A., Gurov D.A. The influence of carbon filler type on the physical, mechanical and electrically conductive properties of polyamide-based injection molded thermoplastic materials // Proceedings of VIAM. 2024. No. 1. DOI: 10.18577/2307-6046-2024-0-1-35-43. URL: https://www.viam-works.ru/en/journal/2024/1/4
Keywords
carbon nanotubes, polyamide, injection molded thermoplastic materials, electrical conductivity, antistatic properties
Abstract
The low level of electrically conductive properties is one of the limiting factors for their use of thermoplastic materials for the production of instrument housings, radio-controlled equipment, structural elements of aircraft and ground equipment operating in conditions of dry air and interaction with other dielectrics. It is shown that by changing the type of the carbon filler, extra adding a modifier with carbon nanotubes and a plasticizer, it is possible to influence the electro-physical and mechanical characteristics of injection molded polymer compositions to achieve the required level of properties.
Reference list
- Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), paper no. 10. Available at: http://www.journal.viam.ru (accessed: November 10, 2023). DOI: 10.18577/2713-0193-2023-0-2-122-144.
- Sorokin A.E., Ivanov M.S., Sagomonova V.A. Thermoplastic polymer composite materials based on polyetheretherketones of various manufacturers. Aviation materials and technologies, 2022, no. 1 (66), paper no. 04. Available at: http://www.journal.viam.ru (accessed: November 10, 2023). DOI: 10.18577/2071-9140-2022-0-1-41-50.
- Zhelezina G.F., Solovyeva N.A., Makrushin K.V., Rysin L.S. Polymer composite materials for manufacturing engine air particle separation of advanced helicopter engine. Aviacionnye materialy i tehnologii, 2018, no. 1 (50), pp. 58–63. DOI: 10.18577/2071-9140-2018-0-1-58-63.
- Postnov V.I., Veshkin E.A., Makrushin K.V., Sudin Yu.I. Technological features of manufacturing polymer composite materials of main rotor blades for a light helicopter. Aviation materials and technologies, 2023, no. 1 (70), paper no. 06. Available at: http://www.journal.viam.ru (accessed: November 10, 2023). DOI: 10.18577/2713-0193-2023-0-1-30-50.
- Meincke O., Kaempfer D., Weickmann H. et al. Mechanical properties and electrical conductivity of carbon-nanotube filled polyamide-6 and its blends with acrylonitrile/butadiene/styrene. Polymer, 2004, vol. 45, pp. 739–748.
- Kanbur Y., Küçükyavuz Z. Electrical and mechanical properties of polypropylene/carbon black composites. Journal of Reinforced Plastics and Composites, 2009, vol. 28, no. 18, pp. 2251–2260.
- Bauhofer W., Kovacs J.Z. A review and analysis of electrical percolation in carbon nanotube polymer composites. Composites science and technology, 2009, vol. 69, no. 10, pp. 1486–1498.
- Kondrashov S.V., Solovyanchik L.V., Minaeva L.A., Shorstov S.Yu. Thermoplastic polyamide composition with electrically conductive properties. Trudy VIAM, 2023, no. 4 (122), paper no. 03. Available at: http://www.viam-works.ru (accessed: November 08, 2023). DOI: 10.18577/2307-6046-2023-0-4-40-48.
- Deng H., Lin L., Ji M. et al. Progress on the morphological control of conductive network in conductive polymer composites and the use as electroactive multifunctional materials. Progress in Polymer Science, 2014, vol. 39, no. 4, pp. 627–655.
- Carbon nanotubes in multiphase polymer blends. Polymer–Carbon Nanotube Composites: Preparation, properties and applications. Eds. T. McNally, P. Pötschke. Woodhead Publishing, 2011, pp. 587–620.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N. New generation materials – the basis of innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
- Kablov E.N. Chemistry in aviation materials science. Rossiyskiy khimicheskiy zhurnal, 2010, vol. LIV, no. 1, pp. 3–4.
- Kablov E.N. What is innovation. Nauka i zhizn, 2011, no. 5, pp. 2–6.
- Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.