Epoxybismaleimide resins: features and advantages

Mukhametov R.R., Mosiyuk V.N., Shosheva A.L., Bukharov S.V.
Mukhametov R.R., Mosiyuk V.N., Shosheva A.L., Bukharov S.V. Epoxybismaleimide resins: features and advantages // Proceedings of VIAM. 2023. No. 8. DOI: 10.18577/2307-6046-2023-0-8-64-73. URL: https://www.viam-works.ru/en/journal/2023/8/6
Keywords
4, epoxy resins, bismaleimide resins, 4'-bismaleimidodiphenylmethane, polymer composite materials, adhesive
Abstract

The review of the released epoxybismaleimide materials of various scopes is provided in the real work on the basis of the analysis of domestic and foreign patent and scientific and technical literature: binding, adhesives. The physical and thermomechanical properties of polymer matrices of epoxybismaleimide resins and adhesives are presented. Modification of the epoxy polymer matrix with bismaleimides increases the heat resistance, strength, and crack resistance of polymer composite materials (PCMs) based on them.

Reference list
  1. Zagora A.G., Tkachuk A.I., Terekhov I.V., Mukhametov R.R. Methods of chemical modification of epoxy oligomers (review). Trudy VIAM, 2021, no. 7 (101), paper no. 08. Available at: http://www.viam-works.ru (accessed: June 06, 2023). DOI: 10.18577/2307-6046-2021-0-7-73-85.
  2. Bao L.-R., Yee A.F. Effect of temperature on moisture absorption in a bismaleimide resin and its carbon fiber composites. Polymer, 2002, vol. 43, pp. 3987–3997.
  3. Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composites (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 48–58. DOI: 10.18577/2071-9140-2019-0-3-48-58.
  4. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  5. Shosheva A.L. Bismaleimide resins (review). Part 1. Trudy VIAM, 2022, no. 10 (116), paper no. 03. Available at: http://www.viam-works.ru (accessed: December 15, 2022). DOI: 10.18577/2307-6046-2022-0-10-23-41.
  6. Radue M.S., Varshney V., Baur J.W. et al. Molecular Modeling of Cross-Linked Polymers with Complex Cure Pathways: A Case Study of Bismaleimide Resins. Macromolecules, 2018, vol. 51, pp. 1830–1840.
  7. Yi X.-S., Du S., Zhang L. Composite materials engineering. Chemical Industry Press, 2006, vol. 1. Fundamentals of Composite Materials, 765 p.
  8. Bismaleimide-epoxy compositions and prepregs: pat. 4510272 USA 475836; appl. 16.03.83, publ. 09.04.85.
  9. Iredale R.J., Ward C., Hameron I. Modern Advances in Bismaleimide Resin Technology: a 21st Century Perspective on the Chemistry of Addition Polyimides. Progress in Polymer Science, 2017, vol. 6, pp. 1–21.
  10. Musto P., Martuscelli E., Ragosta G., Russo P., Scarinzi G., Villano P. FTIR spectroscopy and physical properties of an epoxy/Bismaleimide IPN system. Journal of Materials Science, 1998, vol. 33, p. 4595.
  11. Musto P. Two-Dimensional FTIR Spectrodcopt Dtudies on the Thermal-Oxidative Degradation of Epoxy-Bis(maleimide) Networks. Macromolecules, 2003, vol. 36, p. 3210.
  12. Woo E.M., Chen L.B., Seferis J.C. Characterization of epoxy-bismaleimide network matrices. Journal of Materials Science, 1987, vol. 22, p. 3665.
  13. Kim D.S., Han M.J., Lee J.R. Cure behavior and Properties of an Epoxy resin Modified With a Bismaleimide Resin. Polymer engineering and science, 1995, vol. 35, no. 17, pp. 1353–1358.
  14. Patel K.D. Novel Bismaleimide-epoxy resin system. Oriental Journal of Chemistry, 1999, vol. 15(3), pp. 457–462.
  15. Wu C.-S., Liu Y.-L., Hsu K.-Y. Maleimide-epoxy resins: preparation, thermal properties, and flame retardance. Polymer, 2003, no. 44, pp. 565–573.
  16. Heat resistant resin compositions, articles and method: pat. US 531498A; appl. 05.02.93; publ. 24.05.94.
  17. Thermo-appropriate composition: pat. 2201947 Rus. Federation; appl. 17.05.01; publ. 10.04.03.
  18. Jena R.K., Yue C.Y., Sk M.M., Ghosh K. A novel high performance bismaleimide/diallyl bisphenol A (BMI/DBA) – epoxy interpenetrating network resin for rigid riser application. RSC Advances, 2015, vol. 5, pp. 79888–79897.
  19. Zhang Q., Wang J., Yang S. et al. Facile construction of one-component intrinsic flame-retardant epoxy resin system with fast curing ability using imidazole-blocked bismaleimide. Composite Part B, 2019, vol. 177, p. 107380.
  20. Mahesh K.P.O., Alagar M. Preparation and Characterization of Chain-Extended Bismaleimide Modified Polyurethane–Epoxy Matrices. Journal of Applied Polymer Science, 2002, vol. 87, pp. 1562–1568.
  21. Tkachuk A.I., Donetsky K.I., Terekhov I.V., Karavaev R.Yu. The use of thermosetting matrices for the manufacture of polymer composite materials by the non-autoclave molding methods. Aviation materials and technology, 2021, no. 1 (62), paper no. 03. Available at: https://journal.viam.ru (accessed: June 07, 2023). DOI: 10.18577/2713-0193-2021-0-1-22-33.
  22. Kablov E.N., Erofeev V.T., Zotkina M.M. et al. Plasticized epoxy composites for manufacturing of composite reinforcement. Journal of Physics. Conference Series: International Conference on Engineering Systems 2020, 2020, p. 012031.
  23. Modified epoxy resin film for RFI molding process and preparation method thereof: pat. 101735573 CN; appl. 12.03.09; publ. 30.05.12.
  24. Heat-resistant epoxy binder for the manufacture of products by pressure impregnation: pat. 2590563 Rus. Federation; appl. 23.04.15; publ. 10.07.16.
  25. Kablov E.N., Chursova L.V., Babin A.N., Mukhametov R.R., Panina N.N. Developments of FSUE "VIAM" in the field of melt binders for polymer composite materials. Polimernye materialy i tekhnologii, 2016, vol. 2, no. 2, pp. 37–42.
  26. Composition of epoxybismaleimide binder for prepregs (options), method for producing epoxybismaleimide binder (options), prepreg and product: pat. 2335514 Rus. Federation; appl. 27.12.06; publ. 10.10.08.
  27. Composition of epoxybismaleimide binder for prepregs, prepreg and product: pat. 2427598 Rus. Federation; appl. 29.10.09; publ. 10.05.11.
  28. Composition of epoxybismaleimide resin and method for its production: pat. 2587169 Rus. Federation; appl. 15.12.14; publ. 20.06.16.
  29. Mosiyuk V.N., Vorvul S.V., Tomchani O.V. Differential vacuum molding as an advanced technology of vacuum molding. Aviacionnye materialy i tehnologii, 2017, no. 4 (49), pp. 37–41. DOI: 10.18577/2071-9140-2017-0-4-37-41.
  30. azhenov S.L., Berlin A.A., Kulkov A.A., Oshmyan V.G. Polymer composite materials. Strength and technology. Dolgoprudny: Intelligence, 2010, 352 p.
  31. Method for manufacturing composite shaping equipment for molding products from polymer composite materials: pat. 2720312 Rus. Federation; appl. 10.07.19; publ. 28.04.20.
  32. Kotukhova A.M., Ivanitsky A.S., Boyko L.I., Tomchani O.V., Dolmatov S.A. Heat-resistant epoxyimide binder for composite materials. Plasticheskie massy, 2006, no. 8, pp. 9–12.
  33. Ragjasekaran R., Alagar M. Mechanical Properties of Bismaleimides Modified Polysulfone Epoxy Matrices. International Journal of Polymeric Materials, 2007, vol. 56, pp. 911–927.
  34. Method for Preparing Modified Bismaleimide Resin Adhesive Film: pat. 104177828A CN; appl. 30.07.14; publ. 03.12.14.
  35. Epoxy adhesive: pat. 25202479 Rus. Federation; appl. 10.12.12; publ. 27.06.14.
  36. Hysol EA 9673 Modified BMI Film Adhesive. Available at: https://www.lookpolymers.com (accessed: May 18, 2023).
  37. LOCTITE EA 9673 AERO Epoxy Film Adhesive (known as Hysol EA 9673). Available at: http://aero-consultants.co.uk/uploads/article2398/LOCTITE%20EA%209673%20AERO.PDF (accessed: May 18, 2023).
  38. Adhesive Composition, Laminate, and Adhesive Sheet: pat. 2020-012026 A; appl. 13.07.18; publ. 23.01.20.