Investigation of the influence of heat treatment modes in the β-region on the structure and mechanical properties of semi-finished products from the VT22M alloy

Krokhinа V.A., Arislanov A.A., Putyrskiy S.V., Naprienko S.A.
Krokhinа V.A., Arislanov A.A., Putyrskiy S.V., Naprienko S.A. Investigation of the influence of heat treatment modes in the β-region on the structure and mechanical properties of semi-finished products from the VT22M alloy // Proceedings of VIAM. 2023. No. 8. DOI: 10.18577/2307-6046-2023-0-8-25-34. URL: https://www.viam-works.ru/en/journal/2023/8/3
Keywords
titanium alloy VT22M, microstructure, mechanical properties, fractographic analysis of fractures
Abstract

. Presents the results of a study of the structure and mechanical properties of semi-finished products from the VT22M alloy after various modes of heat treatment with heating in the β-region. The regimes differed in the rate of cooling from the β-region and the presence of intermediate exposures. The study of mechanical properties in tension, impact strength and fracture toughness was carried out, the analysis of macrostructure and microstructure was carried out. After testing for fracture toughness, fractographic studies were performed to assess the nature of the fracture of the samples. The effect of heat treatment modes in the β-region on the structure and mechanical properties of semi-finished products from the VT22M alloy is shown.

Reference list
  1. Kablov E.N. Trends and guidelines for Russia's innovative development. 3rd ed., rev. and add. Moscow: VIAM, 2015, 720 p.
  2. Kablov E.N. What is the future to be made of? Materials of a new generation, technologies for their creation and processing – the basis of innovation. Krylya Rodiny, 2016, no. 5, рр. 8–18.
  3. Kablov E.N. What is innovation. Nauka i zhizn, 2011, no. 5, pp. 2–6.
  4. Demakov S.T., Gadeev D.V., Illarionov A.G., Ivasishin O.M. Effect of heat treatment in the structure and fracture behavior of titanium alloy VST5553. Metal Science and Heat Treatment, 2015, vol. 57, no. 7–8, pp. 473–479.
  5. Kablov E.N., Putyrsky S.V., Yakovlev A.L., Krokhina V.A., Naprienko S.A. Investigation of resistance to fatigue failure of forgings from high-strength titanium alloy VT22M, manufactured with final deformation in (α + β)- and β-regions. Titan, 2021, no. 1 (70), pp. 473–479. DOI: 10.1007/s11041-015-9907-1.
  6. Glazunov S.G., Moiseev V.N. Structural titanium alloys. Moscow: Metallurgiya, 1974, 368 p.
  7. Horev A.I. Fundamental and applied works on structural titanium alloys and perspective directions of their development. Trudy VIAM, 2013, no. 2, paper no. 04. Available at: http://www.viam-works.ru (accessed: December 15, 2022).
  8. Anoshkin N.F., Bochvar G.A., Livanov V.A. Titanium alloys. Metallography of titanium alloys. Moscow: Metallurgiya, 1980, 464 p
  9. Peters M., Kumpfert J., Ward C.H., Leyens C. Titanium Alloys for Aerospace Applications. Advanced Engineering Materials, 2003, vol. 5, pp. 419–427.
  10. Tetyukhin V.V., Levin I.V., Leder M.O., Shibanov A.S. Development of a new high-strength alloy: Ti 5Al–5Mo–5V–3Cr. Sovremennye nauchnyye problemy i tekhnologii v grazhdanskoy aviatsii, Moscow: Nauka, 2013, pp.. 240–251.
  11. Krokhina V.A., Putyrsky S.V., Yakovlev A.L., Nochovnaya N.A. Prospects for the use of β-deformation for a high-strength titanium alloy of the transition class VT22M. Titan, 2019, no. 3 (65), pp. 42–47.
  12. Inagaki I., Shirai Y., Takechi T., Ariyasu N. Application and Features of Titanium for the Aerospace Industry. Osaka: Nippon Steel & Sumitomo Metal, 2014, pp. 22–27.
  13. Kablov E.N., Nochovnaya N.A., Shiryaev A.A., Davydova E.A. Investigation of structural and phase transformations in metastable β-titanium alloys and effect of cooling rate from homogenization temperature on structure and properties of VT47 alloy. Part 2. Trudy VIAM, 2020, no. 8 (90), paper no. 02. Available at: http://www.viam-works.ru (accessed: December 08, 2022). 10.18577/2307-6046-2020-0-8-11-19.
  14. Dzunovich D.A., Panin P.V., Lukina E.A., Shiryaev A.A. Heat treatment effect on structure and properties of welded large-dimensioned semi-finished products from VT23 titanium alloy. Trudy VIAM, 2018, no. 1 (61), paper no. 07. Available at: http://www.viam-works.ru (accessed: June 20, 2022). DOI: 10.18577/2307-6046-2018-0-1-7-7.
  15. Kalashnikov V.S., Reshetilo L.P., Chuchman O.V., Naprienko S.A. Strength and reliability of rods and rotor blade stamps made of heat-resistant industrial titanium alloys and modern pseudo-α-titanium alloy. Trudy VIAM, 2022, no. 2 (108), paper no. 02. Available at: http://www.viam-works.ru (accessed: December 08, 2022). DOI: 10.18577/2307-6046-2022-0-2-13-31.
  16. Nochovnaya N.A., Shiryaev A.A. Effect of heat treatment on mechanical properties and structure of high-strength metastable β-titanium alloy with experimental composition. Trudy VIAM, 2018, no. 6 (66), paper no. 03. Available at: http://www.viam-works.ru (accessed: December 13, 2022). DOI: 10.18577/2307-6046-2018-0-6-22-29.
  17. Panin P.V., Nochovnaya N.A., Kablov D.E., Alekseev E.B., Shiryaev A.A., Novak A.V. A practical guide to the metallography of alloys based on titanium and its intermetallic compounds: textbook. allowance. Ed. E.N. Kablov. Moscow: VIAM, 2020, 200 p.
  18. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  19. Kablov E.N. VIAM: continuation of the path. Nauka v Rossii, 2012, no. 4, pp. 7–11.