High temperature oxide corrosion of ceramic materials in turbine engines

Tolmachev Y.V., Zavarzin S.V., Loshchinina A.O., Knyazev A.V.
Tolmachev Y.V., Zavarzin S.V., Loshchinina A.O., Knyazev A.V. High temperature oxide corrosion of ceramic materials in turbine engines // Proceedings of VIAM. 2023. No. 7. DOI: 10.18577/2307-6046-2023-0-7-69-83. URL: https://www.viam-works.ru/en/journal/2023/7/6
Keywords
thermal barrier coatings, ceramics, ceramic coatings, zirconia, CMAS-corrosion, high temperature corrosion
Abstract

Рresents the issues of corrosion of ceramic thermal barrier coatings caused by the molten mixture of calcium, magnesium, aluminium and silicon oxides (CMAS). The influence of structure of the thermal barrier coatings on CMAS-corrosion is examined. The faliure mechanisms of thermal-barrier coatings are discussed in detail. It has been determined that the primary cause of faliure is the difference in the coefficients of thermal expansion between the CMAS-penetrated layers and the rest of the thermal barrier system. Different methods of testing the effects of CMAS-corrosion on thermal barrier coatings are reviewed.

Reference list
  1. Miller R.A. Thermal barrier coatings for aircraft engines: history and directions. Journal of thermal spraying, 1997, vol. 6, pp. 35–43.
  2. Zhang W.W., Li G.R., Zhang Q., Yang G.J. Epitaxial growth and cracking of highly tough 7YSZ splats by thermal spray technology. Journal of Advanced Ceramics, 2017, vol. 6, pp. 230–239.
  3. Li G.R. Strain-induced stiffness-dependent structural changes and the associated failure mechanism in TBCs. Journal of Advanced Ceramics, 2017, vol. 37, pp. 3609–3621.
  4. Wright P.K., Evans A.G. Mechanisms governing the performance of thermal barrier coatings. Current opinion in solid state and material science, 1999, vol. 4, pp. 255–265.
  5. Evans A.G., Mumm D.R., Hutchinson J.W. et al. Mechanisms controlling the durability of thermal barrier coatings. Progress in material science, 2001, vol. 5, pp. 505–553.
  6. Padture N.P. Thermal barrier coatings for gas-turbine engine applications. Science, 2002, vol. 6, pp. 280–284.
  7. Levi C.G. Emerging materials and processes for thermal barrier systems. Opinion in Solid State and Materials Science, 2004, vol. 8, pp. 77–91.
  8. Schafrik R., Sprague R. Saga of gas turbine materials Part I. Advanced Materials and Processes, 2004, vol. 5, pp. 29–33.
  9. Kablov E.N., Muboyadzhyan S.A. Heat-shielding coatings for high-pressure turbine blades of promising gas turbine engines. Metally, 2012, no. 1, pp. 5–13. DOI: 10.18577/2307-6046-2016-0-1-17-24.
  10. Kablov E.N., Muboyadzhyan S.A. Heat resisting and heat-protective coverings for turbine blades of high pressure of perspective GTE. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 60–70.
  11. Zhou Y.C., Liu Q.X., Yang L. Failure mechanisms and life predictions of thermal barrier coating. Acta Mechanica Solida Sinica, 2010, vol. 31, pp. 504–531.
  12. Clarke D.R., Oechsner M., Padture N.P. Thermal-barrier coatings for more efficient gas-turbine engines. Materials research society, 2012, vol. 37, pp. 891–898.
  13. Darolia R. Thermal barrier coatings technology: critical review, progress update, remaining challenges and prospects. International Materials Reviews, 2013, vol. 58, pp. 315–348.
  14. Peng H., Wang L., Guo L. et al. Degradation of EB-PVD thermal barrier coatings caused by CMAS deposits. Progress in Natural Science: Materials International, 2012, vol. 22, pp. 461–464.
  15. Meier S., Gupta D., Sheffler K. Ceramic thermal barrier coatings for commercial gas turbine engines. The Journal of the Minerals, 1991, vol. 43, pp. 50–53.
  16. Kablov E.N., Muboyadzhyan S.A. Heat-shielding coatings with a ceramic layer of low thermal conductivity based on zirconium oxide for high-pressure turbine blades of promising gas turbine engines. Modern achievements in the field of creating promising non-metallic composite materials and coatings for aviation and space technology. Moscow: VIAM, 2015, p. 3.
  17. Kablov E.N., Doronin O.N., Artemenko N.I., Stekhov P.A., Marakhovsky P.S., Stolyarova V.L. Study of the physicochemical properties of ceramics based on the Sm2O3–Y2O3–HfO2 system for the development of advanced heat-shielding coatings. Zhurnal neorganicheskoy khimii, 2020, vol. 65, no. 6, pp. 846–855. DOI: 10.31857/S0044457X20060070.
  18. Loshchinin Yu.V., Budinovskiy S.A., Razmakhov M.G. Heat conductivity of heat-protective coatings ZrO2–Y2O3 alloyed by REM oxides obtained by magnetronny application. Aviaсionnye materialy i tehnologii, 2018, no. 3, pp. 42–49. DOI: 10.18577/2071-9140-2018-0-3-42-49.
  19. Sokolov A.V., Deynega G.I., Kuzmina N.A. Influence of Sc2O3 additive on sintering temperature and properties of ZrO2–Y2O3 system oxide ceramics. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 64–69. DOI: 10.18577/2071-9140-2020-0-1-64-69.
  20. Stiger M.J., Yanar N.M., Topping M.G. et al. Thermal Barrier Coatings for the 21st Century. Zeitschrift fur Metallkunde, 1999, vol. 90, pp. 1–37.
  21. Jadhav A.D., Padture N.P., Jordan E.H. et al. Low-thermal-conductivity plasma-sprayed thermal barrier coatings with engineered microstructures. Acta Materialia, 2006, vol. 6, pp. 3343–3349.
  22. Schulz U., Fritscher K., Peters M. EB-PVD Y2O3- and CeO2Y2O3-stabilized zirconia thermal barrier coatings – crystal habit and phase composition. Surface and Coatings Technology, 1996, vol. 82, pp. 259–269.
  23. Doronin O.N., Artemenko N.I., Stekhov P.A., Voronov V.A. Deposition of ceramic layers of heat protection coatings based on the system Gd2O3–ZrO2–HfO2 and Sm2O3–Y2O3–HfO2. Aviation materials and technologies, 2022, no. 1 (66), paper no. 10. Available at: http://www.journal.viam.ru (accessed: April 24, 2023). DOI: 10.18577/2713-0193-2022-0-1-129-142.
  24. Sampath S., Schulz U., Jarligo M.O., Kuroda S. Processing science of advanced thermal-barrier systems. MRS Bulletin, 2012, vol. 37, pp. 903–910.
  25. Lugscheider E., Bobzin K., Bärwulf S., Etzkorn A. Mechanical properties of EB-PVD-thermal barrier coatings by nanoindentation. Surface and Coatings Technology, 2001, vol. 138, pp. 9–13.
  26. Drexler J.M., Chen C.H., Gledhill A.D. et al. Plasma sprayed gadolinium zirconate thermal barrier coatings that are resistant to damage by molten Ca–Mg–Al-silicate glass. Surface and Coatings Technology, 2012, vol. 206, pp. 3911–3916.
  27. Wu J., Guo H., Gao Y., Gong S. Microstructure and thermo-physical properties of yttria stabilized zirconia coatings with CMAS deposits. Journal of the European Ceramic Society, 2011, vol. 31, pp. 1881–1888.
  28. Niranatlumpong P., Ponton C.B., Evans H.E. The Failure of Protective Oxides on Plasma-Sprayed NiCrAlY Overlay Coatings. Oxidation of Metals, 2000, vol. 53, pp. 241–258.
  29. Koomparkping T., Damrongrat S., Niranatlumpong P. Al-rich precipitation in CoNiCrAlY bondcoat at high temperature. Journal of Thermal Spray Technology, 2005, vol. 14, pp. 264–267.
  30. Mumm D.R., Evans A.G., Spitsberg I.T. Characterization of a cyclic displacement instability for a thermally grown oxide in a thermal barrier system. Acta Materialia, 2001, vol. 49, pp. 2329–2340.
  31. Chen W.R. The growth and influence of thermally grown oxide in a thermal barrier coating. Surface and Coatings Technology, 2006, vol. 201, pp. 1074–1079.
  32. Karlsson A.M., Hutchinson J.W., Evans A.G. The displacement of the thermally grown oxide in thermal barrier systems upon temperature cycling. Materials Science and Engineering, 2003, vol. 351, pp. 244–257.
  33. Wiesner V.L., Bansal N.P. Mechanical and thermal properties of calcium–magnesium aluminosilicate (CMAS) glass. Journal of the European Ceramic Society, 2005, vol. 35, pp. 2907–2914.
  34. Kramer S., Faulhaber S., Chambers M. et al. Mechanisms of cracking and delamination within thick thermal barrier systems in aero-engines subject to calcium-magnesium-alumino-silicate (CMAS) penetration. Materials Science and Engineering: A, 2008, vol. 490, pp. 26–35.
  35. Kim J., Dunn M., Baran A. et al. Deposition of volcanic materials in the hot sections of two gas turbine engines. The Journal of Engineering for Gas Turbines and Power, 1993, vol. 155, pp. 641–651.
  36. Borom M., Johnson C., Peluso L. Role of environmental deposits and operating surface temperature in spallation of air plasma sprayed thermal barrier coatings. Surface and Coatings Technology, 1996, vol. 86, pp. 116–126.
  37. Stott F., Wet D., Taylor R. The effects of molten silicate deposits in the stability of the thermal barrier coatings for turbine applications at very high temperatures. 3rd International SAMPE Metal Conference, 1992, vol. 3, pp. M92–M101.
  38. Strangman T., Raybould D., Jamell A., Baker W. Damage mechanisms, life prediction and development of EB-PVD thermal barrier coatings for turbine airfoils. Surface and Coatings Technology, 2007, vol. 202, pp. 658–664.
  39. Mackenzie J., Canil D. Volatile heavy metal mobility in silicate liquids: implications for volcanic degassing and eruption prediction. Earth and Planetary Science Letters, 2008, vol. 269, pp. 488–496.
  40. Leyen P., Schulz U., Pint B., Wright I. Influence of EB-PVD TBC microstructure on thermal barrier coating system performance under cyclic oxidation conditions. Surface and Coatings Technology, 1999, vol. 6, pp. 280–284.
  41. Kramer S., Yang J., Levi C. Thermochemical interaction of thermal barrier coatings with CMAS deposits. Journal of the American Ceramic Society, 2006, vol. 89, pp. 3167–3175.
  42. Grant K., Kramer S., Lofvander J., Levi C. CMAS degradation of environmental barrier coatings. Surface and Coatings Technology, 2007, vol. 202, pp. 653–657.
  43. Kramer S., Yang J., Levi C. Infiltration-inhibiting reaction of gadolinium zirconate thermal barrier coatings with CMAS melts. Journal of the American ceramics society, 2008, vol. 91, pp. 576–583.
  44. Mercer C., Faulhaber S., Evans A., Darolia R. A delamination mechanism for the thermal barrier coatings subject to CMAS infiltration. Acta Materialia, 2005, vol. 53, pp. 1029–1039.
  45. Guo L., Li G., Gan L. Effects of surface roughness on CMAS corrosion behavior for thermal barrier coating applications. Journal of Advanced Ceramics Society, 2020, vol. 10, pp. 472–481.
  46. Watanabe M., Mercer C., Levi C.G., Evans A.G. On a Ferroelastic Mechanism Governing The Toughness of Metastable Tetragonal-Prime Yttria-Stabilized Zirconia. Acta Materialis, 2004, vol. 52, pp. 1479–1487.
  47. Zhao L.G., Lu T.J., Fleck N.A. Crack channeling and spalling in a plate due to thermal shock loading. Journal of the Mechanics and Physics of Solids, 2000, vol. 48, pp. 867–897.
  48. Suo Z., Hutchinson J.W. Steady-state cracking in brittle. substrates beneath adherent films. International Journal of Solids and Structures, 1989, vol. 25, pp. 1337–1487.
  49. Drory M.D., Thouless M.D., Evans A.G. On the decohesion of residually stressed thin films. Acta Metallurgica, 1988, vol. 36, pp. 2019–2028.
  50. Chen X., Wang R., Yao N. et al. Foreign object damage in a thermal barrier system: mechanisms and simulations // Materials Science and Engineering. 2002, vol. 352, no. 1–2, рр. 221–231.
  51. Zavarzin S.V., Oglodkov M.S., Chesnokov D.V., Kozlov I.A. Hot corrosion and protection of materials of gas turbine engines (review). Trudy VIAM, 2018, no. 3 (109), paper no. 11. Available at: http://www.viam-works.ru (accessed: April 24, 2023). DOI: 10.18577/2307-6046-2022-0-3-121-134.
  52. Liu S., Liu Q., Hu X. et al. CMAS corrosion resistance behavior and mechanism of Hf6Ta2O17 ceramic as potential material for thermal barrier coatings. Coatings, 2023, vol. 13, art. 404.
  53. Li D., Jiang P., Gao R. et al. Experimental and numerical investigation on the thermal and mechanical behaviours of thermal barrier coatings exposed to CMAS corrosion. Journal of Advanced Ceramics, 2021, vol. 10, pp. 551–564.
  54. DeWet D.J., Taylor R., Stott F.H. Corrosion mechanisms of ZrO2–Y2O3 thermal barrier coatings in the presence of molten middle-east sand. Journal de physique. IV, Colloque, 1993, vol. 3, pp. 655–663.
  55. Zhao H., Levi C.G., Haydn N.G.W. Molten silicate interactions with thermal barrier coatings. Surface and coatings Technology, 2014, vol. 251, pp. 74–86.
  56. Zhang Q., Zhang X., Ma Zh. et al. Water vapor and CMAS corrosion tests of Y2SiO5/Si thermal and environmental barrier coating. Heliyon, 2022, vol. 8, art. e10262. DOI: 10.1016/j.heliyon.2022.e10262.
  57. Guo L., Xin H., Hu Ch. Comparison of NaVO3+CMAS mixture and CMAS corrosion to thermal barrier coatings. Corrosion Science, 2020, vol. 177, art. 108968. DOI: 10.1016/j.corsci.2020.108968.
  58. Shifler D.A., Choi S.R. CMAS effects on ship gas-turbine components/materials. Proceedings of ASME Turbo Expo: Turbomachinery Technical Conference and Exposition, 2018, art. GT2018-75865. DOI: 10.1115/GT2018-75865.
  59. Budinovsky S.A., Stekhov P.A., Doronin O.N., Artemenko N.I. Main mechanisms of destruction of the ceramic layer of thermal barrier coatings (review). Trudy VIAM, 2019, no. 2 (74), paper no. 11. Available at: http://www.viam-works.ru (accessed: April 24, 2023). DOI: 10.18577 / 2307-6046-2019-0-2-105-112.