Some causes of voids formation in polymer composite materials (review)

Khrulkov A.V., Karavaev R.Y., Gorodilova N.A., Donetskiy K.I.
Khrulkov A.V., Karavaev R.Y., Gorodilova N.A., Donetskiy K.I. Some causes of voids formation in polymer composite materials (review) // Proceedings of VIAM. 2023. No. 6. DOI: 10.18577/2307-6046-2023-0-6-72-86. URL: https://www.viam-works.ru/en/journal/2023/6/7
Keywords
polymer composite material, pores, autoclave molding, vacuum molding
Abstract

In the manufacture of structures from polymer composite materials (PCM), defects in the form of pores are very often formed. The study of the causes of pore formation in composites began about half a century ago and is still relevant. This is due to the difficulty of preventing their formation with modern PCM manufacturing technologies, such as non-autoclave molding and the manufacture of parts of increased complexity, as well as due to the increased viscosity of the modified resins. To eliminate defects in the form of the time arising by production, it is necessary to carry out search of way of right choice of parameters of processing.

Reference list
  1. Composites Market – Global Industry Analysis and Forecast (2022–2029). Available at: https://www.maximizemarketresearch.com/market-report/global-composites-market/34243/ (accessed: January 10, 2023).
  2. Kablov E.N. New Generation Materials and Technologies for Their Digital Processing. Herald of the Russian Academy of Sciences. 2020, vol. 90, no. 2, pp. 225–228.
  3. Kablov E.N. The role of fundamental research in the creation of new generation materials. Report XXI Mendeleev Congress on General and Applied Chemistry: in 6 vols. St. Petersburg, 2019, vol. 4, p. 24.
  4. Kablov E.N. Aviation materials science in the XXI century. Prospects and tasks. Aviation materials. Selected works of VIAM 1932–2002. Moscow: MISIS; VIAM, 2002, pp. 23–47.
  5. Timoshkov P.N., Khrulkov A.V., Yazvenko L.N., Composite materials for non-autoclave technology (review). Trudy VIAM, 2018, no. 3 (63), paper no. 05. Available at: http://www.viam-works.ru (accessed: February 01, 2023). DOI: 10.18577/2307-6046-2018-0-3-37-48.
  6. Tkachuk A.I., Donetsky K.I., Terekhov I.V., Karavaev R.Yu. The use of thermosetting matrices for the manufacture of polymer composite materials by the non-autoclave molding methods. Aviation materials and technology, 2021, no. 1 (62), paper no. 03. Available at: https://journal.viam.ru (accessed: February 01, 2023). DOI: 10.18577/2713-0193-2021-0-1-22-33.
  7. Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composites (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), рр. 48–58. DOI: 10.18577/2071-9140-2019-0-3-48-58.
  8. Veshkin E.A., Postnov V.I., Postnova M.V., Barannikov A.A. Experience in the use of vacuum infusion technologies in the production of PCM structures. Izvestiya Samarskogo nauchnogo tsentra Rossiyskoy akademii nauk, 2018, vol. 20, no. 4-3, pp. 344–350.
  9. Goncharov V.A., Raskutin A.E. Computer modeling of the infusion process in the manufacture of composite arched element. Trudy VIAM, 2015, no. 7, paper no. 11. Available at: http://www.viam-works.ru (accessed: February 02, 2023). DOI: 10.18577/2307-6046-2015-0-7-11-11.
  10. Kolobkov A.S. Polymer composite materials for various aircraft structures (review). Trudy VIAM, 2020, no. 6–7 (89), paper no. 05. Available at: http://www.viam-works.ru (accessed: January 10, 2023). DOI: 10.18577/2307-6046-2020-0-67-38-44.
  11. Timoshkov P.N., Goncharov V.A., Usacheva M.N., Khrulkov A.V. The development of automated laying: from the beginning to our days (review). Part 1. Automated Tape Laying (ATL). Aviation materials and technologies, 2021, no. 2 (63), paper no. 06. Available at: http://www.journal.viam.ru (accessed: January 18, 2023). DOI: 10.18577/2713-0193-2021-0-2-51-61.
  12. Kablov E.N., Valueva M.I., I.V. Zelenina, Khmelnitskiy V.V., Aleksashin V.M. Carbon plastics based on benzoxazine oligomers – perspective materials. Trudy VIAM, 2020, no. 1, paper no. 07. Available at: http://www.viam-works.ru (accessed: January 20, 2023). DOI: 10.18577/2307-6046-2020-0-1-68-77.
  13. Valueva M.I., Zelenina I.V., Zharinov M.A., Akhmadieva K.R. World market of high temperature polyimide carbon plastic (review). Trudy VIAM, 2019, no. 12 (84), paper no. 08. Available at: http://www.viam-works.ru (accessed: January 10, 2023). DOI: 10.18577/2307-6046-2019-0-12-67-79.
  14. Zhelezina G.F., Tikhonov I.V., Chernykh T.E., Bova V.G., Voynov S.I. Aramid fibers of the third generation Rusar NT for reinforcing organotextolites for aviation purposes. Plasticheskie massy, 2019, no. 3–4, pp. 43–46.
  15. Popov Yu.O., Koloкoltseva T.V., Gromova A.A., Gusev Yu.A. Influence of operational factors on the main physical and mechanical properties of a fiberglass product VPS-31. Trudy VIAM, 2021, no. 11 (105), paper no. 08. Available at: http://www.viam-works.ru (accessed: January 10, 2023). DOI: 10.18577/2307-6046-2021-0-11-82-90.
  16. Sorokin A.E., Ivanov M.S., Sagomonova V.A. Thermoplastic polymer composite materials based on polyetheretherketones of various manufacturers. Aviation materials and technologies, 2022, no. 1 (66), paper no. 04. Available at: http://www.journal.viam.ru (accessed: February 01, 2023). DOI: 10.18577/2071-9140-2022-0-1-41-50.
  17. Mahoor M., Gorbatikh L., Verpoest I., Lomov S. Voids in fiber-reinforced polymer composites: A review on their formation, characteristics, and effects on mechanical performance. Journal of Composite Materials, 2018, no. 35, pp. 25–69.
  18. Centea T., Grunenfelder L., Nutt S. A review of out-of-autoclave prepregs – Material properties, process phenomena, and manufacturing considerations. Composites. Part A: Applied Science and Manufacturing, 2014, no. 70, pp. 132–154.
  19. Tereshkova I. Creation of heat-resistant polymer composites is one of the priority areas of national materials science. Available at: https://viam.ru/news/2734 (accessed: January 13, 2023).
  20. Patel N., Rohatgi V., Lee LJ. Micro-scale flow behavior, fiber wetting and void formation in liquid composite molding. Materials Science, 1995, no. 35, рр. 837–851.
  21. Park C.H., Lebel A., Saouab A. Modeling and simulation of voids and saturation in liquid composite molding processes. Composites. Part A: Applied Science and Manufacturing, 2011, no. 42, pp. 658–668.
  22. Hubert P., Centea T., Grunefelder L. Out-of-Autoclave Prepreg Processing. Reference Module in Materials Science and Materials Engineering, 2017, no. 9, pp. 36–60.
  23. Boey F., Lye S. Void reduction in autoclave processing of thermoset composites. I – High pressure effects on void reduction. II – Void reduction in a microwave curing process. Composites, 1992, no. 26, pp. 126–150.
  24. James K., Göran F. Processing conditions and voids in out of autoclave prepregs. Department of Materials Engineering, 2012, no. 6, pp. 1–12.
  25. Edwards W., Martínez P., Nutt S. Process robustness and defect formation mechanisms in unidirectional semipreg. Advanced Manufacturing: Polymer & Composites Science, 2020, no. 13, pp. 26–39.
  26. Kobina E. VIAM will expand the production of composite materials in Ulyanovsk. Available at: https://uldelo.ru/2019/08/28/b-viam-rasshirit-proizvodstvo-b-kompozitnykh-materialov-v-ulyanovske(accessed: January 31, 2023).
  27. Kay J., Fahrang L. Effect of process conditions on porosity in out-of-autoclave prepreg laminates. Engineering, 2011, no. 10, pp. 1–27.
  28. Grunenfelder L., Dills A. Effect of prepreg format on defect control in out-of-autoclave processing. Composites. Part A: Applied Science and Manufacturing, 2017, no. 4, pp. 37–60.