Research of influence of thermal aging on properties high-temperature polyimide carbon fiber reinforced plastic
Valueva M.I., Zelenina I.V., Nacharkina A.V., Gulyaev A.I. Research of influence of thermal aging on properties high-temperature polyimide carbon fiber reinforced plastic // Proceedings of VIAM. 2023. No. 6. DOI: 10.18577/2307-6046-2023-0-6-46-62. URL: https://www.viam-works.ru/en/journal/2023/6/5
Keywords
polymer composite materials, high-temperature carbon fiber reinforced plastics, polyimide binders, influencing factors, thermal aging
Abstract
The results of studies of the effect of laboratory-simulated exposure to elevated temperatures (of 250, 280 and 320 °С) on the structure and properties of high-temperature carbon fiber reinforced plastic (CFRP) based on a thermosetting polyimide binder are presented. The mass loss of CFRP under prolonged exposure to elevated temperatures has been determined, and the activation energy of the thermal aging process has been calculated. For comparison, the data of scientific and technical literature on the thermal-oxidative effect of elevated temperatures on CFRP of foreign manufacturers based on polyimide binders of the PMR-type are presented.
Reference list
- Kablov E.N., Startsev V.O. The influence of internal stresses on the aging of polymer composite materials: a review. Mechanics of Composite Materials, 2021, vol. 57, no. 5, pp. 565–576.
- Kablov E.N., Startsev V.O. Climatic aging of aviation polymer composite materials: I. Influence of significant factors. Russian metallurgy (Metally), 2020, vol. 2020, no. 4, pp. 364–372.
- Kablov E.N., Startsev V.O. Climatic aging of aviation polymer composite materials: II. Development of methods for studying the early stages of aging. Russian metallurgy (Metally), 2020, vol. 2020, no. 10, pp. 1088–1094.
- Kablov E.N., Startsev V.O. Measurement and forecasting of materials samples’ temperature during weathering in different climatic zones. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 47–58. DOI: 10.18577/2071-9140-2020-0-4-47-58.
- Abramova M.G., Lutsenko A.N., Varchenko E.A. Concerning the aspects of validation of climate resistance of airborne materials at all life cycle stages (review). Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 86–94. DOI: 10.18577/2071-9140-2020-0-1-86-94.
- Kurs M.G., Nikolayev E.V., Abramov D.V. Full-scale and accelerated tests of metallic and nonmetallic materials: key factors and specialized stands. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 66–73. DOI: 10.18577/2071-9140-2019-0-1-66-73.
- Laptev A.B., Nikolayev E.V., Kolpachkov E.D. Thermodynamic characteristics of aging of polymeric composite materials under conditions of real exploitation. Aviaсionnye materialy i tehnologii, 2018, no. 3, pp. 80–88. DOI: 10.18577/2071-9140-2018-0-3-80-88.
- Perov NS, Gulyaev A.I. About the importance of structure evolution control of polymer composite materials with the microheterogeneous matrix for service life forecasting. Aviacionnye materialy i tehnologii, 2017, no. 1 (46), pp. 75–85. DOI: 10.18577 / 2071-9140-2017-0-1-75-85.
- Gulyaev A.I., Medvedev P.N., Sbitneva S.V., Petrov A.A. Experimental research of «fiber–matrix» adhesion strength in carbon fiber epoxy/polysulphone composite. Aviacionnye materialy i tehnologii, 2019, no. 4 (57), pp. 80–86. DOI: 10.18577/2071-9140-2019-0-4-80-86.
- Grigorenko V.B., Morozova L.V. Application of the scanning electron microscopy for studying of initial destruction stages. Aviacionnye materialy i tehnologii, 2018, no. 1 (50), pp. 77–87. DOI: 10.18577/2071-9140-2018-0-1-77-87.
- Raskutin A.E. Heat-resistant carbon plastics for aircraft structures operating at temperatures up to 400 °C: thesis, Cand.Sc. … cand. tech. Sciences. Moscow, 2007, 166 p.
- Mikhailin Yu.A. Heat-resistant polymers and polymeric materials. St. Petersburg: Professiya, 2006, 624 p.
- Mikhailin Yu.A. Heat, thermal and fire resistance of polymeric materials. St. Petersburg: Nauchnye osnovy i tekhnologii, 2011, 416 p.
- Zharinov M.A., Shimkin A.A., Akhmadiyeva K.R., Zelenina I.V. Features and properties of solvent-free PMR-type polyimide resin. Trudy VIAM, 2018, no. 12 (72), paper no. 05. Available at: http://www.viam-works.ru (accessed: September 01, 2022). DOI: 10.18577/2307-6046-2018-0-12-46-53.
- Wilson D. PMR-15 Processing, Properties and Problems – a Review. British Polymer Journal, 1988, no. 20, рр. 405–416.
- Sheppard C.H., Hoggatt J.T., Symonds W.A. Quality control developments for graphite/PMR-15 polyimide composites materials. NASA, 1979, 181 p.
- Avimid®R Polyimide Composite. Technical Data Sheet. Available at: https://matweb.com/search/datasheettext.aspx?matguid= 3dcb6c37bd39469c8e92b27045a13ea4 (accessed: December 01, 2022).
- CYCOM®2237 Polyimide Resin System. Technical Data Sheet. Available at: https://www.solvay.com/en/product/cycom-2237 (accessed: December 01, 2022).
- MVK-10. RTM Polyimide. Product description. Available at: http://www.maverickcorp.com/_CE/pagecontent/Documents/MVK-10.pdf (accessed: December 01, 2022).
- MVK-14 FREEFORM®. High temperature polyimide. Available at: http://www.maverickcorp.com/high-temperature-resins/material-options-high/mvk-14-freeform/
- (accessed: December 01, 2022).
- Tsampas S., Fernberg P., Joffe R. Development of novel high Tg polyimide-based composites. Part II: Mechanical characterization. Journal of Composite Materials. 2018, vol. 52, no. 2, pp. 261–274.
- High tempereture composite materials. Available at: https://pdf4pro.com/amp/view/high-tempereture-composite-materials-upilex-5a5302.html (accessed: December 01, 2022).
- Aerospace. Advance Composite Materials Selector Guide. Available at: https://www.toraytac.com/media/ca3eea73-6961-4ea8-adc7-5d1b861684f6/Bxgrfg/TAC/Documents/Selector%20Guides/Toray_Advanced_Composite_Material_Portfolio_Selector_Guide.pdf (accessed: December 01, 2022).
- Bowles K.J., Roberts G.D., Kamvouris J.E. Long-therm isothermal aging effects on carbon fabric-reinforced PMR-15 composites: compression strength. Washington: NASA, 1996, 17 p.
- Bowles K.J. Thermo-Oxidative Stability Studies of Celion 6000/PMR-15 Unidirectional Composites, PMR-15, and Celion 6000 Fiber. Journal of Composite Materials, 1988, vol. 22, no. 10, pp. 966–985.
- Back C.A. Effects of prior aging on the creep response of carbon fiber reinforced PMR-15 neat resin at 288 °C in an air environment: Thesis. Air Force Institute of Technology, USA, 2007, 124 p.
- Bowles K.J., Tsuji L., Kamvouris J., Roberts G.D. Long-Term Isothermal Aging Effects on Weight Loss, Compression Properties, and Dimensions of T650-35 Fabric-Reinforced PMR-15 Composites-Data. Washington: NASA, Glenn Research Center Cleveland, 2003, 65 р.
- Chuang K.С., Bowles K.J., Papadoulos D. et al. A high Tg PMR polyimide composites (DMBZ-15). Journal of Advanced Materials, 2001, vol. 33, no. 4, pp. 33–38.
- Chuang K. Development of DMBZ-15 high-glass-transition-temperature polyimides as PMR-15 replacements given R&D 100 awards. Research and technology. Washington: NASA, 2003, pp. 27–28.
- Connell J.W., Smith J.G. (Jr.), Hergenrother P.M., Criss J.M. High Temperature Transfer Molding Resins: Status of PETI-298 and PETI-330. Available at: https://www.cs.odu.edu/~mln/ltrs-pdfs/NASA-2003-35sampe-jwc.pdf (accessed: December 01, 2022).
- Avimid®RB Polyimide Composite. Technical Data Sheet. Cytec engineered materials. 2012. AECM-00052. Available at: https://www.matweb.com/search/datasheettext.aspx?matguid=d3d9f6997a2145d087bfc9342a8ee61b (accessed: December 01, 2022).
- Shoeppner G.A., Tandon G.P., Ripberger E.R. Anistropic oxidation and weight loss in PMR-15 composites. Composites: Part A, 2007, vol. 38, pp. 890–904.
- Ripberger E.R., Tandon G.P., Shoeppner G.A. Experimental techniques for characterizing thermo-oxidative behavior in high-temperature polyimide composite. Available at: https://www.researchgate.net/publication/267819653 (accessed: December 01, 2022).
- Tandon G.P., Pochiraju K.V., Shoeppner G.A. Thermo-oxidative behavior of high-temperature PMR-15 resin and composites. Materials Science and Engineering A, 2008, vol. 498, pp. 150–161.
- Tandon G.P., Ragland W.R., Shoeppner G.A. Using Optical Microscopy to Monitor Anisotropic Oxidation Growth in High-Temperature Polymer Matrix Composites. Journal of composite materials, 2009, vol. 43, no. 05, pp. 583–603.
- Korshak V.V. Heat resistant polymers. Moscow: Nauka, 1969, 381 p.
- Valevin E.O., Startsev V.O., Zelenina I.V. Thermal aging, surface degradation and water transfer in carbon fiber reinforced plastic VKU-38TR. Trudy VIAM, 2020, no. 6–7 (89), paper no. 12. Available at: http://www.viam-works.ru (accessed: December 01, 2022). DOI: 10.18577/2307-6046-2020-0-67-118-128.
- Valevin E.O. Influence of heat and moisture exposure on the properties of heat-resistant polymer composite materials based on a phthalonitrile matrix: thesis, Cand. tech. Sciences. Moscow: MAI, 2018, 130 p.
- Cavano P.J., Winters W.E. Fiber reinforced PMR polyimide composites. Washington: NASA Lewis Researcher Center, 1978, 105 p.