Heat-resistant polyimide adhesive of constructive purposes

Akhmadieva K.R., Petrova A.P., Shosheva A.L., Bokov V.V.
Akhmadieva K.R., Petrova A.P., Shosheva A.L., Bokov V.V. Heat-resistant polyimide adhesive of constructive purposes // Proceedings of VIAM. 2023. No. 6. DOI: 10.18577/2307-6046-2023-0-6-15-24. URL: https://www.viam-works.ru/en/journal/2023/6/2
Keywords
polyimides, polyimide adhesive, heat-resistant adhesives, shear strength of adhesive bonds, high-temperature polymer composite materials (PCM)
Abstract

The main physical and mechanical properties of polyimide adhesive VK-103 are discussed. The film adhesive VK-103 is a mixture of imide-forming components reinforced with non-woven glass veil. The effect of reinforcing filler on the shear strength of adhesive bonds are investigated. The properties of the adhesive VK-103 after exposure to various operational factors and in comparison with existing foreign analogues are given. The adhesive VK-103 is specialized for bonding metals and multilayer structures of PCM with an operating temperature of up to 320 °C.

Reference list
  1. Rusanov A.L. Ladder polyheteroarylenes – progress and problems. Uspekhi khimii, 1979, vol. XLVIII, is. 1, pp. 115–147.
  2. Hergenrother P.M. The use, design, synthesis, and properties of high performance/high temperature polymers: an overview. High Performance Polymers, 2003, vol. 15, no. 1, pp. 3–45.
  3. Ebnesajjad S. Handbook of adhesives and surface preparation: technology, applications and manufacturing. William Andrew, 2010, 450 р.
  4. Kurnosov A.O., Raskutin A.E., Mukhametov R.R., Melnikov D.A. Polymer composite materials based on thermosetting polyimide binders for aerospace engineering. Review. Voprosy materialovedeniya, 2016, no. 4, pр. 50–62.
  5. Gunyaeva A.G., Kurnosov A.O., Gulyaev I.N. High-temperature polymer composite materials developed FSUE «VIAM» for aerospace engineering: past, present and future (review). Trudy VIAM, 2021, no. 1 (95), paper no. 05. Available at: http://www.viam-works.ru (accessed: November 10, 2022). DOI: 10.18577/2307-6046-2021-0-1-43-53.
  6. Kablov E.N. Materials for aerospace engineering. Vse materialy. Entsiklopedicheskiy spravochnik, 2007, no. 5, pp. 7–27.
  7. Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composites (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 48–58. DOI: 10.18577/2071-9140-2019-0-3-48-58.
  8. Kablov E.N., Chursova L.V., Babin A.N., Mukhametov R.R., Panina N.N. Developments of FSUE "VIAM" in the field of melt binders for polymer composite materials. Polimernye materialy i tekhnologii, 2016, vol. 2, no. 2, pp. 37–42.
  9. Kablov E.N., Valueva M.I., Zelenina I.V., Khmelnitskiy V.V., Aleksashin V.M. Carbon plastics based on benzoxazine oligomers – perspective materials. Trudy VIAM, 2020, no. 1, paper no. 07. Available at: http://www.viam-works.ru (accessed: October 31, 2022). DOI: 10.18577/2307-6046-2020-0-1-68-77.
  10. Valueva M.I., Zelenina I.V., Zharinov M.A., Khaskov M.A. High-temperature carbon plastics based on thermosetting polyimide binder. Voprosy materialovedeniya, 2020, no. 3 (103), pp. 89–102.
  11. Kolpachkov E.D., Kurnosov A.O., Papina S.N., Petrova A.P. Specificity of the formation of fiberglass based on PMR-polyimides. Trudy VIAM, 2022, no. 6 (112), paper no. 04. Available at: http://www.viam-works.ru (accessed: November 14, 2022) DOI: 10.18577/2307-6046-2022-0-7-37-49.
  12. Mikhailin Yu.A. Heat-resistant polymers and polymeric materials. St. Petersburg: Professiya, 2006, 624 p.
  13. Subrahmanian K.P. High-Temperature Polymers and Adhesives. Structural Adhesives: Chemistry and Technology. Ed. S.R. Hartshorn. Boston: Springer, 1986, pp. 309–345.
  14. Rabilloud G. Heat-Resistant Adhesives. Handbook of Adhesives and Surface Preparation. William Andrew Publishing, 2011, pp. 185–220.
  15. Potsius A. Adhesives, adhesion, bonding technology. Trans. from Engl. St. Petersburg: Profession, 2016, 384 p.
  16. Scola D.A., Vontell J.H. High temperature polyimides, chemistry and properties. Polymer Composites, 1988, vol. 9, no. 6, pp. 443–452.
  17. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.