Analysis of the chemical composition of intermetallic titanium ortho-alloys by inductively coupled plasma atomic emission spectrometry

Part 1
Dvoretskov R.M., Alexeev E.B., Karachevtsev F.N., Zagvozdkina T.N.
Dvoretskov R.M., Alexeev E.B., Karachevtsev F.N., Zagvozdkina T.N. Analysis of the chemical composition of intermetallic titanium ortho-alloys by inductively coupled plasma atomic emission spectrometry. Part 1 // Proceedings of VIAM. 2023. No. 6. DOI: 10.18577/2307-6046-2023-0-6-115-129. URL: https://www.viam-works.ru/en/journal/2023/6/10
Keywords
analytical control, chemical analysis, titanium alloys, titanium intermetallics, ortho-alloys, atomic emission spectrometry, inductively coupled plasma
Abstract

A technique is proposed for determining the base elements Ti, Nb, Al and alloying elements Mo, V, Zr, W, Ta in ortho-titanium alloys by inductively coupled plasma atomic emission spectrometry. Analytical lines of elements free from significant spectral overlaps are chosen. The spectral lines of the internal standard were selected. The limits of detection of elements are estimated. The metrological characteristics of the technique were evaluated using model solutions. The correctness of the developed methodology was assessed using standard samples.

Reference list
  1. Kablov E.N. Materials and chemical technologies for aviation equipment. Vestnik Rossiyskoy akademii nauk, 2012, vol. 82, no. 6, pp. 520–530.
  2. Kolobov Yu.R., Kablov E.N., Kozlov E.V. et al. Structure and properties of intermetallic materials with nanophase hardening. Moscow: MISiS, 2008, 328 p.
  3. Kablov E.N., Kashapov O.S., Medvedev P.N., Pavlova T.V. Study of a α + β-titanium alloy based on a system of Ti–Al–Sn–Zr–Si–β-stabilizing alloying elements. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 30–37. DOI: 10.18577/2071-9140-2020-0-1-30-37.
  4. Abraimov N.V., Petukhov I.G., Zarypov M.S., Lukina V.V. On the issue of heat resistance of titanium alloys operating at temperatures above 650 °C. Elektrometallurgiya, 2021, no. 12, pp. 10–20.
  5. Nochovnaya N.A., Panin P.V., Alekseev E.B., Novak A.V. Patterns of the formation of the structural-phase state of alloys based on ortho- and gamma-titanium aluminides in the process of thermomechanical treatment. Vestnik RFFI, 2015, no. 1, pp. 18–26.
  6. Novak A.V. Regularities of the effect of microadditives of rare earth elements on the structural-phase state and mechanical characteristics of an intermetallic alloy based on orthorhombic titanium aluminide: thesis, Cand. Sc. (Tech.). Moscow, 2019, 128 p.
  7. Skvortsova S.V., Umarova O.Z., Anishchuk D.S., Smirnov V.G. Formation of the structure, phase composition and mechanical properties of an alloy based on titanium aluminide Ti2AlNb during heat treatment. Titan, 2015, no. 3 (49), pp. 29–33.
  8. Skvortsova S.V., Umarova O.Z., Agarkova E.O., Chernyshova A.A. Influence of heat treatment on the structure and mechanical properties of the plate from the VTI-4 intermetallic alloy. Titan, 2015, no. 4 (50), pp. 17–21.
  9. Makushina M.A., Kochetkov A.S., Nochovnaya N.A. Cast titanium alloys for aviation equipment (review). Trudy VIAM, 2021, no. 7 (101), paper no. 05. Available at: http://www.viam-works.ru (accessed: January 09, 2023). DOI: 10.18577/2307-6046-2021-0-7-39-47.
  10. Nochovnaya N.A., Bazyleva O.A., Kablov D.E., Panin P.V. Intermetallic alloys based on titanium and nickel. Ed. E.N. Kablov. Moscow: VIAM, 2018, 308 p.
  11. Antipov V.V. Prospects for development of aluminium, magnesium and titanium alloys for aerospace engineering. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 186–194. DOI: 10.18577/2107-9140-2017-0-S-186-194.
  12. Alekseev I.E., Pilipenko A.A., Varfolomeev M.S. The possibility of replacing nickel heat-resistant alloys with alloys based on the Ti–Al intermetallic compound. Rapidly quenched materials and coatings: Proceedings of the XIX Intern. sci.-tech. conf. Moscow, 2022, pp. 311–315.
  13. Dzunovich D.A., Alekseyev E.B., Panin P.V., Lukina E.A., Novak A.V. Structure and properties of sheet semi-finished products from various wrought intermetallic titanium alloys. Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 17–25. DOI: 10.18577/2071-9140-2018-0-2-17-25.
  14. Podkopalov I.A. Review of alloys based on titanium intermetallic compounds. Mavlyutovskie readings: materials of XV All-Rus. youth scientific conference: in 7 vols. Ufa, 2021, vol. 2, pp. 311–315.
  15. Polkin I.S., Egorova Yu.B., Davydenko L.V. Alloying, phase composition and mechanical properties of titanium alloys. Technology of light alloys, 2022, no. 2, pp. 4–13.
  16. Shubin I.Yu., Nikitin Ya.Yu., Puchkov Yu.A. et al. Investigation of resistance to high-temperature gas and salt corrosion of heat-resistant intermetallic titanium alloy VTI-4. Vestnik Moskovskogo gosudarstvennogo tekhnicheskogo universiteta im. N.E. Baumana. Ser.: Mechanical engineering, 2020, no. 6 (135), pp. 83–105.
  17. Bykov Yu.G., Nochovnaya N.A., Timokhin V.M., Alekseev E.B., Novak A.V., Zakharova E.S. Application of intermetallic titanium ortho-alloy in the bling design of the high-pressure compressor guide vane. Electrometallurgiya, 2019, no. 11, pp. 19–26.
  18. Duyunova V.A., Oglodkov M.S., Putyrskiy S.V., Kochetkov A.S., Zueva O.V. Modern technologies for melting titanium alloy ingots (review). Aviation materials and technologies, 2022, no. 1 (66), paper no. 03. Available at: http://www.journal.viam.ru (accessed: January 11, 2023). DOI: 10.18577/2071-9140-2022-0-1-30-40.
  19. Nadezhdina M.E., Shinkevich A.I., Shinkevich M.V. Monitoring system for digital production of an enterprise of the petrochemical industry. Kompetentnost, 2021, no. 7, pp. 36–39.
  20. Karpov Yu.A., Baranovskaya V.B. Analytical control is an integral part of material diagnostics. Zavodskaya laboratoriya. Diagnostika materialov, 2017, vol. 83, no. 1-I, pp. 5–12.
  21. Arkhipenko A.A., Koshel E.S., Baranovskaya V.B. Development of a technique for arc atomic emission spectral analysis of cerium oxide. Zavodskaya laboratoriya. Diagnostika materialov, 2021, vol. 87, no. 11, pp. 19–25.
  22. Nochovnaya N.A., Kochetkov A.S., Bokov K.A., Ivanov V.I. Research the characteristics of casting titanium superalloy VTI-4. Trudy VIAM, 2017, no. 5 (53), paper no. 02. Available at: http://www.viam-works.ru (accessed: January 10, 2023). DOI: 10.18577/2307-6046-2017-0-5-2-2.
  23. Umarova O.Z. Patterns of formation of phase composition and structure in a heat-resistant alloy based on titanium intermetallic compound VTI-4 during thermal and thermohydrogen treatments: thesis, Cand. Sc. (Tech.). Moscow, 2017, 179 p.
  24. Oglodkov M.S., Duyunova V.A., Nochovnaya N.A., Ivanov V.I., Avilochev L.Yu. Features of the technology manufacturing of deformed blanks from intermetallic alloys VIT1 for parts of the gas turbine engine. Trudy VIAM, 2021, no. 12 (106), paper no. 01. Available at: http://www.viam-works.ru (accessed: January 11, 2023). DOI: 10.18577/2307-6046-2021-0-12-3-13.
  25. Vyacheslavov A.V., Malinkina Yu.Yu., Bichaev V.B., Titova A.D., Ermolaeva T.N. Analysis of corrosion-resistant titanium alloys alloyed with ruthenium by inductively coupled plasma atomic emission spectrometry. Zavodskaya laboratoriya. Diagnostika materialov, 2018, vol. 84, no. 5, pp. 14–19.
  26. Baranovskaya V.B., Medvedevskikh M.Yu., Karpov Yu.A. Actual problems of the quality of chemical analysis. Analitika i kontrol, 2021, vol. 25, no. 4, pp. 273–279.
  27. Otto M. Modern methods of analytical chemistry: in 2 vols. Moscow: Technosfera, 2003, vol. I, 416 p.
  28. Karpov Yu.A., Baranovskaya V.B. The role and possibilities of analytical control in metallurgy. Tsvetnye metally, 2016, no. 8 (884), pp. 63–67. DOI: 10.17580/tsm.2016.08.09.
  29. Karpov Yu.A., Baranovskaya V.B. Problems of standardization of methods of chemical analysis in metallurgy. Zavodskaya laboratoriya. Diagnostika materialov, 2019, vol. 85, no. 1–2, pp. 5–14.
  30. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.