Solubility of rhenium and ruthenium in the γʹ-phase and physicochemical properties of nickel alloys of the Ni–Al‒Re‒Ru system

Elyutin E.S., Petrushin N.V., Karachevtsev F.N., Chabina E.B.
Elyutin E.S., Petrushin N.V., Karachevtsev F.N., Chabina E.B. Solubility of rhenium and ruthenium in the γʹ-phase and physicochemical properties of nickel alloys of the Ni–Al‒Re‒Ru system // Proceedings of VIAM. 2023. No. 6. DOI: 10.18577/2307-6046-2023-0-6-3-14. URL: https://www.viam-works.ru/en/journal/2023/6/1
Keywords
Ni–Al–Re–Ru system, directional solidification, flat growth front, segregation of alloying element, temperature solidus, temperature liquidus
Abstract

Directional solidification with a flat front of a nickel alloy of the Ni‒Al‒Re‒Ru system was performed. As a result, a casting with a variable length content of the elements Al, Re and Ru (gradient casting) was obtained. It is established that during solidification in a gradient casting, nickel alloys with the structures γ + γʹ, γʹ, γʹ + β are successively formed. The solubility’s of Re and Ru in the γʹ and β phases of the γ + γʹ, γʹ, γʹ + β alloys were determined. For the same alloys, the temperatures γʹ-solvus, solidus and liquidus are determined. It was found that in the Ni–Al–Re–Ru nickel system, the γʹ phase is formed by a peritectic reaction L + γ → γ' at 1374 °C and a eutectic reaction L → γʹ + β at 1372 °C.

Reference list
  1. The work of leading aircraft engine companies in ensuring the creation of advanced aircraft engines (analytical review). Ed. V.A. Skibin, V.I. Solonin. Moscow: TsiAM, 2021, 678 p.
  2. Kablov E.N. Materials of the new generation – the basis of innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
  3. Logunov A.V. Heat-resistant nickel alloys for blades and disks of gas turbines. Rybinsk: Gas Turbine Technologies, 2017, 854 p.
  4. Reed R.C. The Superalloys. Fundamentals and Applications. Cambridge: United Kingdom at University Press, 2006, 372 p.
  5. Bondarenko Yu.A. Trends in the development of high-temperature metal materials and technologies in the production of modern aircraft gas turbine engines. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 3–11. DOI: 10.18577/2071-9140-2019-0-2-3-11.
  6. Kablov E.N. Physico-chemical and technological features of the creation of heat-resistant alloys containing rhenium. Vestnik Moskovskogo universiteta. Ser. 2: Chemistry, 2005, vol. 46, no. 3, рр. 155–167.
  7. Lu F., Antonov S., Zheng Y. et al. Effect of Re on long-term creep behavior of nickel-based single-crystal superalloys for industrial gas turbine applications. Superalloys 2020. TMS, 2020, pp. 218–227.
  8. Svetlov I.L., Petrushin N.V., Epishin A.I., Elyutin E.S. Synergistic effect of rhenium and ruthenium on the long-term strength of single crystals of nickel heat-resistant alloys III–IV generations. Fizika metallov i metallovedenie, 2022, vol. 123, no. 8, pp. 888–894.
  9. Matuszewski K., Rettig R., Matysiak H. et al. Effect of ruthenium on the precipitation of topologically close packed phases in Ni-base superalloys of 3rd and 4th generation. Acta Materialia, 2015, vol. 95, pp. 274‒283. DOI: 10.1016/j.actamat.2015.05.033.
  10. Glatzel U. Microstructure and internal strains of undeformed and creep deformed samples of a Nickel-base superalloy. Berlin: Verlag Dr. Köster, 1994, 80 p.
  11. Kablov E.N., Petrushin N.V., Morozova G.I., Svetlov I.L. Physical and chemical factors of heat resistance of nickel alloys containing rhenium. Aviacionnye materialy i tekhnologii, 2004, no. 1, pp. 37–47.
  12. Shu D., Tian S., Liu L. et al. Influence of Re/Ru on concentration in γ/γʹ phases of in nickel-base single crystal superalloys. Materials and Design, 2017, vol. 132, pp. 198–207.
  13. Saunders N. Phase diagram calculation for Ni-base superalloys. Superalloys 1996. Pennsylvania: Minerals, Metals & Materials Society, 1996, рр. 101–110.
  14. Petrushin N.V., Bronfin M.B., Chabina E.B., Dyachkova L.A. Phase transformations and structure of directionally crystallized intermetallic alloys of the Ni–Al–Re system. Metally, 1994, no. 3, pp. 85–93.
  15. Chakravorty S., West D.R.F. Constitution of Ni3Al–Ni3Mo–Ni3W section of Ni–Al–Mo–W system. Materials Science and Technology, 1986, vol. 2, no. 10, pp. 989–996.
  16. Udovskiy A.L., Oldakovskiy I.V., Moldavskiy V.G. Theoretical and experimental studies of phase equilibria of the Ni–NiAl–W system in the range of 900–1500 °С. Metally, 1991, no. 4, pp. 112–123.
  17. Tryon B., Pollock T.M. Experimental assessment of the Ru‒Al‒Ni ternary phase diagram at 1000 and 1100 °C. Materials Sciences and Engineering A, 2006, vol. 430, pp. 266–276.
  18. Van Sluytman J.S., La Fontaine A., Cairney J.M., Pollock T.M. Elemental portioning of platinum metal containing Ni-base superalloys using electron microprobe analysis and atom probe tomography. Acta Materialia, 2010, vol. 58, pp. 1952–1962.
  19. Kuznetsov V.P., Lesnikov V.P., Konakova I.P. Structural and phase transformations in a single-crystal nickel alloy alloyed with rhenium and ruthenium under conditions of long-term strength testing. Metallovedenie i termicheskaya obrabotka metallov, 2015, no. 8 (722), pp. 55–59.
  20. Wang X.G., Liu J.L., Jin T., Sun X.F. The effects of ruthenium additions on tensile deformation mechanisms of single crystal superalloys at different temperatures. Materials and Design, 2014, vol. 63, p. 286–293.
  21. Wang Y.-J., Wang C.-J. The alloying mechanisms of Re, Ru in quaternary Ni-based superalloys γ/γʹ interface: A first principle calculation. Materials Science and Engineering A, 2008, vol. 490, pp. 242–249.
  22. Kablov E.N., Gerasimov V.V., Visik E.M. Technological features of obtaining single-crystal samples and turbine blades from high-rhenium heat-resistant alloys at UVNK-9 and VIAM-1790 units. Aviacionnye materialy i tekhnologii, 2004, no. 1, pp. 91–97.
  23. Kablov E.N., Echin A.B., Bondarenko Yu.A. History of development of directional crystallization technology and equipment for casting blades of gas turbine engines. Trudy VIAM, 2020, no. 3 (87), paper no. 01. Available at: http://www.viam-works.ru (accessed: October 18, 2022). DOI: 10.18577/2307-6046-2020-0-3-3-12. (дата обращения: 18.10.2022). DOI: 10.18577/2307-6046-2020-0-3-3-12.
  24. Vigdorovich V.N., Volpyan A.E., Kurdyumov G.M. Directed crystallization and physical and chemical analysis. Moscow: Khimiya, 1976, 200 p
  25. Epishin A., Brückner U., Portella P.D., Link T. Influence of small rhenium additions on the lattice spacing of nickel solid solution. Scripta Materialia, 2003, vol. 48, pp. 455–459.
  26. Epishin A.I., Rodin A.O., Bokshtein B.S., Svetlov I.L. Mutual diffusion in binary alloys of the Ni–Re system. Fizika metallov i metallovedeniye, 2015, vol. 116, no. 2, pp. 184–190.
  27. Petrushin N.V., Elyutin E.S., Chabina E.B. Phase and structural transformations in directionally solidified with plant front intermetallic eutectic Ni-based alloys. Trudy VIAM, 2020, no. 3 (87), paper no. 02. Available at: http://www.viam-works.ru (accessed: January 16, 2023). DOI: 10.18577/2307-6046-2020-0-3-13-29.
  28. Petrushin N.V., Elyutin E.S., Nazarkin R.M. et al. Segregation of alloying elements in directionally solidified Re–Ru-containing Ni-based superalloy. Inorganic Materials: Applied Research, 2016, vol. 7, no. 6, pp. 824–831.
  29. Kurz W., Fisher D.J. Fundamentals of solidification. Fourth revised edition. Uetikon-Zuerich: Trans Tech Publications Ltd., 1998, 306 p.
  30. Bridgman P.W. Certain physical properties of single crystals of tungsten, antimony, bismuth, tellurium, cadmium, zinc, and tin. Proceedings of the American Academy of Arts and Sciences, 1925, vol. 60, pp. 305–383. DOI: 10.2307/25130058.
  31. Kurts V., Deputy P.R. Directed crystallization of eutectic materials. Moscow: Metallurgiya, 1980, 274 p.
  32. Lashko N.F., Zaslavskaya L.V., Kozlova M.N. et al. Physico-chemical phase analysis of steels and alloys. Moscow: Metallurgiya, 1978, 336 p.
  33. Superalloys II. Heat-resistant materials for aerospace and industrial power plants: in 2 books. Ed. Ch.T. Sims, N.S. Stoloff, W.K. Hagel. Trans. from Engl. Moscow: Metallurgiya, 1995, book 1, 768 p.
  34. Shalin R.E., Svetlov I.L., Kachanov E.B., Tolorayya V.N., Gavrilin O.S. Single crystals of nickel heat-resistant alloys. Moscow: Mashinostroenie, 1997, 336 p.
  35. Barabash O.M., Koval Yu.N. Crystal structure of metals and alloys: reference book. Kyiv: Naukova Dumka, 1986, 598 p.
  36. Kablov E.N., Svetlov I.L., Petrushin N.V. Nickel heat-resistant alloys for blades with directional and single-crystal structure (part I). Materialovedenie, 1997, no. 4, pp. 32–39.
  37. Feng Q., Nandy T.K., Tin S., Pollock T.M. Solidification of high-refractory ruthenium-containing superalloys. Acta Materialia, 2003, vol. 51, no. 1, pp. 269‒284. DOI: 10.1016/S1359-6454(02)00397-X.
  38. Bremer F.J., Beyss M., Karthaus E. et al. Experimental analysis of the Ni–Al phase diagram. Journal Crystal Growth, 1988, vol. 87, no. 2–3, pp. 185–192.
  39. Hilpert K., Kobertz D., Venugopal V. et al. Phase diagram studies on the Al–Ni system. Zeitschrift fur Naturforschung, 1987, vol. 42a, pp. 1327–1332.
  40. Verhoeven J.D., Lee J.H., Laabs F.C., Jones L.L. The phase equilibria of Ni3Al evaluated by directional solidification and diffusion couple experiment. Journal Phase Equilibrium, 1991, vol. 12, no. 1, pp. 15–23.
  41. Udovskiy A.L., Oldakovskiy I.V., Moldavskiy V.G. On the revision of the state diagram of the nickel-aluminum system. Doklady AN SSSR, 1991, vol. 317, no. 1, pp. 161–165.