Comparison of the effect of different release agents on the free surface energy of polymer tooling

Savitsky R.S., Sudyin Yu.I., Salakhova R.K.
Savitsky R.S., Sudyin Yu.I., Salakhova R.K. Comparison of the effect of different release agents on the free surface energy of polymer tooling // Proceedings of VIAM. 2023. No. 5. DOI: 10.18577/2307-6046-2023-0-5-85-93. URL: https://www.viam-works.ru/en/journal/2023/5/8
Keywords
free surface energy (SFE), antiadhesive, release agent, contact angle, OVRK method, polymer tooling
Abstract

Optimality of choice of an antiadhesive for a specific molding surface when molding products from polymer composite materials (PCM) is determined by many factors: absence of scratching of coating from the surface of tooling and of transfer of release agent to molded blank, ease of removal and defectlessness of the product from PCM. Offers an additional factor for evaluating the optimality of selecting an antiadhesive for polymer tooling: determination of free surface energy (FSE), which gives a characteristic of tooling surface wettability. In the framework of this work the FSEs of five different antiadhesion compositions were investigated.

Reference list
  1. Kablov E.N. Composites: today and tomorrow. Metally Evrazii, 2015, no. 1, pp. 36–39.
  2. Kablov E.N. Materials and chemical technologies for aviation equipment. Vestnik Rossiyskoy akademii nauk, 2012, vol. 82, no. 6, pp. 520–530.
  3. Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
  4. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  5. Kablov E.N., Grashchenkov D.V., Isaeva N.V., Solntsev S.S., Sevastyanov V.G. High-Temperature Structural Composite Materials Based on Glass and Ceramics for Advanced Aircraft Products. Steklo i keramika, 2012, no. 4, pp. 7–11.
  6. Tkachuk A.I., Donetsky K.I., Terekhov I.V., Karavaev R.Yu. The use of thermosetting matrices for the manufacture of polymer composite materials by the non-autoclave molding methods. Aviation materials and technology, 2021, no. 1 (62), paper no. 03. Available at: https://journal.viam.ru (accessed: November 16, 2022). DOI: 10.18577/2713-0193-2021-0-1-22-33.
  7. Tkachuk A.I., Terekhov I.V., Gurevich Ya.M., Kudryavtseva A.N. Application of bismaleimide VST-57 binder for obtaining heat-resistant dimensionally stable molds from polymer composite materials. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 32–40. DOI: 10.18577/2071-9140-2020-0-2-32-40.
  8. Mosiyuk V.N., Tomchani O.V. Evaluation of properties of glass-fibre-reinforced plastics based on epoxybisma-leimide resin, produced by different non-autoclave molding techniques. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 47–52. DOI: 10.18577/2071-9140-2019-0-2-47-52.
  9. Kolpachkov E.D., Petrova A.P., Kurnosov A.O., Sokolov I.I. Methods of molding aviation products from PCM (review). Trudy VIAM, 2019, no. 11 (83), paper no. 03. Available at: http://www.viam-works.ru (accessed: November 16, 2022). DOI: 10.18577/2307-6046-2019-0-11-22-36.
  10. Kablov E.N., Chursova L.V., Babin A.N., Mukhametov R.R., Panina N.N. Developments of FSUE "VIAM" in the field of melt binders for polymer composite materials. Polimernye materialy i tekhnologii, 2016, vol. 2, no. 2, pp. 37–42.
  11. Mukhametov R.R., Petrova A.P., Ponomarenko S.A. Anti-adhesive coatings and their properties. Trudy VIAM, 2018, no. 12 (72), paper no. 10. Available at: http://www.viam-works.ru (accessed: November 16, 2022). DOI: 10.18577/2307-6046-2018-0-12-88-96.
  12. Semenova L.V., Novikova T.A., Nefedov N.I. Study of removing ability of removers for paint systems removal. Aviacionnye materialy i tehnologii, 2017, no. 1 (46), pp. 32–37. DOI: 10.18577/2071-9140-2017-0-1-32-37.
  13. Frolov V.I., Semenov A.P., Grishina I.N., Kucherov V.G. Wetting angle and methods for its determination. Moscow: Publishing Center of the Russian State University of Oil and Gas (NRU) im. I.M. Gubkina, 2021, 53 p.
  14. Zinina I.N., Pimanov M.V. Influence of the surface energy of metal samples on the strength of adhesive joints. Izvestiya MSTU "MAMI", 2011, no. 2 (21), pp. 127–130.
  15. Yakovets N.V., Krutko N.P., Opanasenko O.N. Determination of the free surface energy of powdered resinous-asphalten substances by the Owens–Wendt–Rabel–Kaelble method. Sviridovskie chteniya, 2012, no. 8, pp. 253–260.