Analysis of aluminum by glow discharge high resolution mass spectrometry
UDC
543.51; 669.1
DOI
10.18577/2307-6046-2023-0-5-134-144
Article PDF (Russian)
(839.15 KB)
How to cite
Alekseev A.V., Yakimovitch P.V., Koshelev A.V. Analysis of aluminum by glow discharge high resolution mass spectrometry // Proceedings of VIAM. 2023. No. 5. DOI: 10.18577/2307-6046-2023-0-5-134-144. URL: https://www.viam-works.ru/en/journal/2023/5/12
Keywords
high-resolution glow discharge mass spectrometry (GDMS), aluminium, aluminum alloys, determination of harmful impurities
Abstract
In this work, the impurities of 72 elements in high purity (4N) aluminum were determined by the method of high-resolution glow discharge mass spectrometry (GDMS). The most suitable sample preparation was selected, including preliminary acid etching of the sample. To achieve the maximum analytical signals from all the required elements, the appropriate equipment settings were selected. Relative sensitivity coefficients (RCF) were calculated for all the elements being determined using a standard aluminum sample.
Reference list
- Kablov E.N. Materials for aerospace engineering. Vse materialy. Entsiklopedicheskiy spravochnik, 2007, no. 5, pp. 7–27.
- Popovich A.A., Panchenko O.V., Naumov A.A., Sviridov A.V., Skupov A.A., Sbitneva S.V. Friction stir wel-ding of aluminum-lithium alloy V-1469-T. Aviacionnye materialy i tehnologii, 2019, no. 4 (57), pp. 11–17. DOI: 10.18577/2071-9140-2019-0-4-11-17.
- Kablov E.N., Antipov V.V., Klochkova Yu.Yu. Aluminium-lithium alloys of a new generation and layered aluminum-glass plastics based on them. Tsvetnye metally, 2016, no. 8 (884), pp. 86–91. DOI: 10.17580/tsm.2016.08.13.
- Shavnev A.A., Babashov V.G., Varrik N.M. Continuous fibers based on alumina (review). Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 27–34. DOI: 10.18577/2071-9140-2020-0-4-27-34.
- Imametdinov E.S., Valueva M.I. Сomposites for piston engines (rеview). Aviacionnye materialy i tehnologii, 2020, no. 3 (60), pp. 19–28. DOI: 10.18577/2071-9140-2020-0-3-19-28.
- Oglodkov M.S., Shchetinina N.D., Rudchenko A.S., Panteleev M.D. Directions of the develop-ment of promising aluminum-lithium alloys for aero-space engineering (review). Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 19–29. DOI: 10.18577/2071-9140-2020-0-1-19-29.
- State Standard 11069–74. Aluminum primary. Marks. Moscow: Publ. house of standards, 1974, pp. 1–2.
- Kurochkin V.D., Kravchenko L.P. Analysis of impurities in high-purity aluminum oxide by glow discharge mass spectrometry. Powder Metallurgy and Metal Ceramics, 2006, vol. 45, pp. 493–499. DOI: 10.1007/s11106-006-0111-0.
- Kablov E.N., Chabina E.B., Morozov G.A., Muravskaya N.P. Conformity assessment of new materials using high-level RM and MI. Kompetentnost, 2017, no. 2, pp. 40–46.
- State Standard 11739.6–99. Alloys aluminum casting and deformable. Methods for the determination of iron. Moscow: Publ. house of standards, 1999, pp. 1–3.
- State Standard 11739.4–90. Alloys aluminum casting and deformable. Methods for the determination of bismuth. Moscow: Publ. house of standards, 1990, pp. 21–22.
- State Standard 11739.7–99. Alloys aluminum casting and deformable. Methods for the determination of silicon. Moscow: Publ. house of standards, 1999, pp. 8–9.
- Karachevtsev F.N., Alekseev A.V., Letov A.F., Dvoretskov R.M. Plasma methods of nickel alloys elemental chemical composition analysis. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 483–497. DOI: 10.18577/2071-9140-2017-0-S-483-497.
- Pupyshev A.A., Epova E.N. Spectral noise of polyatomic ions in the method of mass spectrometry with inductively coupled plasma. Analitika i kontrol, 2001, vol. 5, no. 4, pp. 335–369.
- Jakubowski N., Prohaska T., Rottmann L., Vanhaecke F. Inductively coupled plasma- and glow discharge plasma-sector field mass spectrometry. Part I. Tutorial: Fundamentals and instrumentation. Journal of Analytical Atomic Spectrometry, 2011, vol. 26, pp. 693–726.
- Ganeev A.A., Gubal A.R., Uskov K.N., Potapov S.V. Glow Discharge Analytical Mass Spectrometry. Izvestiya Akademii nauk. Seriya khimicheskaya, 2012, no. 4, pp. 1–15
- ASTM F1593–08. Standard Test Method for Trace metallic Impurities in Electronic Grade Aluminum by High Mass-Resolution Glow-Discharge Mass Spectometr. ASTM International, 2014, рр. 1–9.